公开(公告)号:US20120060981A1
公开(公告)日:2012-03-15
申请号:US12882538
申请日:2010-09-15
申请人: Robin M. Forbes Jones , John V. Mantione , Urban J. De Souza , Jean-Philippe Thomas , Ramesh Minisandram , Richard L. Kennedy , R. Mark Davis
发明人: Robin M. Forbes Jones , John V. Mantione , Urban J. De Souza , Jean-Philippe Thomas , Ramesh Minisandram , Richard L. Kennedy , R. Mark Davis
摘要: Methods of refining the grain size of titanium and titanium alloys include thermally managed high strain rate multi-axis forging. A high strain rate adiabatically heats an internal region of the workpiece during forging, and a thermal management system is used to heat an external surface region to the workpiece forging temperature, while the internal region is allowed to cool to the workpiece forging temperature. A further method includes multiple upset and draw forging titanium or a titanium alloy using a strain rate less than is used in conventional open die forging of titanium and titanium alloys. Incremental workpiece rotation and draw forging causes severe plastic deformation and grain refinement in the titanium or titanium alloy forging.
摘要翻译: 精炼钛和钛合金晶粒尺寸的方法包括热管理的高应变率多轴锻造。 高应变率在锻造期间绝热加热工件的内部区域,并且使用热管理系统将外表面区域加热到工件锻造温度,同时使内部区域冷却至工件锻造温度。 另外的方法包括使用小于用于钛和钛合金的常规开模锻造中的应变速率的多个镦锻和拉伸锻造钛或钛合金。 增加的工件旋转和拉伸锻造会导致钛或钛合金锻造中严重的塑性变形和晶粒细化。
-
公开(公告)号:US08613818B2
公开(公告)日:2013-12-24
申请号:US12882538
申请日:2010-09-15
申请人: Robin M. Forbes Jones , John V. Mantione , Urban J. De Souza , Jean-Philippe Thomas , Ramesh S. Minisandram , Richard L. Kennedy , R. Mark Davis
发明人: Robin M. Forbes Jones , John V. Mantione , Urban J. De Souza , Jean-Philippe Thomas , Ramesh S. Minisandram , Richard L. Kennedy , R. Mark Davis
摘要: Methods of refining the grain size of titanium and titanium alloys include thermally managed high strain rate multi-axis forging. A high strain rate adiabatically heats an internal region of the workpiece during forging, and a thermal management system is used to heat an external surface region to the workpiece forging temperature, while the internal region is allowed to cool to the workpiece forging temperature. A further method includes multiple upset and draw forging titanium or a titanium alloy using a strain rate less than is used in conventional open die forging of titanium and titanium alloys. Incremental workpiece rotation and draw forging causes severe plastic deformation and grain refinement in the titanium or titanium alloy forging.
摘要翻译: 精炼钛和钛合金晶粒尺寸的方法包括热管理的高应变率多轴锻造。 高应变率在锻造期间绝热加热工件的内部区域,并且使用热管理系统将外表面区域加热到工件锻造温度,同时使内部区域冷却至工件锻造温度。 另外的方法包括使用小于用于钛和钛合金的常规开模锻造中的应变速率的多个镦锻和拉伸锻造钛或钛合金。 增加的工件旋转和拉伸锻造会导致钛或钛合金锻造中严重的塑性变形和晶粒细化。
-
公开(公告)号:US20110302979A1
公开(公告)日:2011-12-15
申请号:US13027327
申请日:2011-02-15
申请人: Scott Oppenheimer , Robin M. Forbes Jones , John V. Mantione , Ramesh S. Minisandram , Jean-Philippe Thomas
发明人: Scott Oppenheimer , Robin M. Forbes Jones , John V. Mantione , Ramesh S. Minisandram , Jean-Philippe Thomas
IPC分类号: B21J3/00
CPC分类号: B21J3/00 , B21C23/32 , B21D37/16 , B21D37/18 , B21J1/06 , C10M103/02 , C10M103/06 , C10M2201/041 , C10M2201/0413 , C10M2201/0613 , C10M2201/0653 , C10M2201/0663 , C10N2210/04 , C10N2230/06 , C10N2240/402 , C10N2240/406 , C10N2250/08
摘要: Forge lubrication processes are disclosed. A solid lubricant sheet is placed between a workpiece and a die in a forging apparatus. Force is applied to the workpiece with the die to plastically deform the workpiece. The solid lubricant sheet decreases the shear friction factor for the forging system and reduces the incidence of die-locking.
摘要翻译: 公开了锻造润滑过程。 在锻造设备中将固体润滑剂片材放置在工件和模具之间。 用模具将力施加到工件上,使工件塑性变形。 固体润滑剂片材减少了锻造系统的剪切摩擦系数,并降低了模具锁定的发生率。
-
公开(公告)号:US09327342B2
公开(公告)日:2016-05-03
申请号:US13027327
申请日:2011-02-15
申请人: Scott Oppenheimer , Robin M. Forbes Jones , John V. Mantione , Ramesh S. Minisandram , Jean-Philippe Thomas
发明人: Scott Oppenheimer , Robin M. Forbes Jones , John V. Mantione , Ramesh S. Minisandram , Jean-Philippe Thomas
IPC分类号: B21J3/00 , C10M103/02 , C10M103/06
CPC分类号: B21J3/00 , B21C23/32 , B21D37/16 , B21D37/18 , B21J1/06 , C10M103/02 , C10M103/06 , C10M2201/041 , C10M2201/0413 , C10M2201/0613 , C10M2201/0653 , C10M2201/0663 , C10N2210/04 , C10N2230/06 , C10N2240/402 , C10N2240/406 , C10N2250/08
摘要: Forge lubrication processes are disclosed. A solid lubricant sheet is placed between a workpiece and a die in a forging apparatus. Force is applied to the workpiece with the die to plastically deform the workpiece. The solid lubricant sheet decreases the shear friction factor for the forging system and reduces the incidence of die-locking.
摘要翻译: 公开了锻造润滑过程。 在锻造设备中将固体润滑剂片材放置在工件和模具之间。 用模具将力施加到工件上,使工件塑性变形。 固体润滑剂片材减少了锻造系统的剪切摩擦系数,并降低了模具锁定的发生率。
-
公开(公告)号:US20120076686A1
公开(公告)日:2012-03-29
申请号:US13108045
申请日:2011-05-16
IPC分类号: C22C14/00
CPC分类号: C22C14/00 , A61L27/06 , B62D29/008 , C22F1/18 , C22F1/183
摘要: An alpha/beta titanium alloy comprising, in percent by weight based on total alloy weight: 3.9 to 4.5 aluminum; 2.2 to 3.0 vanadium; 1.2 to 1.8 iron; 0.24 to 0.30 oxygen; up to 0.08 carbon; up to 0.05 nitrogen; up to 0.015 hydrogen ; titanium; and up to a total of 0.30 of other elements. A non-limiting embodiment of the alpha/beta titanium alloy comprises an aluminum equivalent value in the range of 6.4 to 7.2, exhibits a yield strength in the range of 120 ksi (827.4 MPa) to 155 ksi (1,069 MPa), exhibits an ultimate tensile strength in the range of 130 ksi (896.3 MPa) to 165 ksi (1,138 MPa), and exhibits a ductility in the range of 12 to 30 percent elongation.
摘要翻译: 一种α/β钛合金,其以基于总合金重量的重量百分比:3.9至4.5铝; 2.2〜3.0钒; 1.2至1.8铁; 0.24〜0.30氧气; 高达0.08碳; 高达0.05氮; 高达0.015氢; 钛; 最多可达0.30个其他元素。 α/β钛合金的非限制性实施方案包括在6.4至7.2范围内的铝当量值,显示在120ksi(827.4MPa)至155ksi(1,069MPa)范围内的屈服强度,显示出最终 拉伸强度在130ksi(896.3MPa)至165ksi(113.8MPa)的范围内,并且展延伸率在12%至30%的范围内。
-
-
-
-