公开(公告)号:US10703891B2
公开(公告)日:2020-07-07
申请号:US16078099
申请日:2017-02-21
Applicant: SABIC GLOBAL TECHNOLOGIES B.V.
Inventor: Marc Herklots , Désirée Marie Louise Seegers , Ralf Kleppinger , Timo Olavi Latvakangas , Eddy Jozef Agnes van de Gaar
IPC: C08L23/14 , C08K3/34 , C08K5/098 , C08K5/20 , C08L23/12 , C08L23/16 , C08K5/06 , C08F210/16 , C08F110/06 , C08J3/20
Abstract: The invention relates to a composition comprising a heterophasic propylene copolymer and a C10-C30 aliphatic carboxylic acid amide, wherein the heterophasic propylene copolymer consists of a propylene-based matrix consisting of a propylene homopolymer and/or a propylene-α-olefin copolymer consisting of at least 70 wt % of propylene and at most 30 wt % of α-olefin and wherein the propylene-based matrix is present in an amount of 76 to 90 wt % based on the total heterophasic propylene copolymer and a dispersed ethylene-α-olefin copolymer, wherein the dispersed ethylene-α-olefin copolymer is present in an amount of 24 to 10 wt % based on the total heterophasic propylene copolymer and wherein the sum of the total amount of propylene-based matrix and total amount of the dispersed ethylene-α-olefin copolymer in the heterophasic propylene copolymer is 100 wt %, wherein the amount of ethylene in the ethylene-α-olefin copolymer is 30 to 38 wt %.
-
公开(公告)号:US20190062542A1
公开(公告)日:2019-02-28
申请号:US16078099
申请日:2017-02-21
Applicant: SABIC GLOBAL TECHNOLOGIES B.V.
Inventor: Marc Herklots , Désirée Marie Louise Seegers , Ralf Kleppinger , Timo Olavi Latvakangas , Eddy Jozef Agnes van de Gaar
Abstract: The invention relates to a composition comprising (A) a heterophasic propylene copolymer and (B) a C10-C30 aliphatic carboxylic acid amide, wherein the heterophasic propylene copolymer consists of (a) a propylene-based matrix, wherein the propylene-based matrix consists of a propylene homopolymer and/or a propylene-α-olefin copolymer consisting of at least 70 wt % of propylene and at most 30 wt % of α-olefin, based on the total weight of the propylene-based matrix and wherein the propylene-based matrix is present in an amount of 76 to 90 wt % based on the total heterophasic propylene copolymer and (b) a dispersed ethylene-α-olefin copolymer, wherein the dispersed ethylene-α-olefin copolymer is present in an amount of 24 to 10 wt % based on the total heterophasic propylene copolymer and wherein the sum of the total amount of propylene-based matrix and total amount of the dispersed ethylene-α-olefin copolymer in the heterophasic propylene copolymer is 100 wt %, wherein the amount of ethylene in the ethylene-α-olefin copolymer is 30 to 38 wt % and wherein the propylene-based matrix has a melt flow index MFIPP as determined according to IS01133 at 230° C. and 2.16 kg and the dispersed ethylene-a-olefin elastomer has a melt flow index MFIEPR as determined according to IS01133 at 230° C. and 2.16 kg, wherein the ratio of MFIPP/MFIEPR is 0.5-15 and wherein the composition has a MFI of 10 to 100 dg/min as determined according to IS01133 at 230° C. and 2.16 kg.
-