COMPOSITION COMPRISING HETEROPHASIC PROPYLENE COPOLYMER

    公开(公告)号:US20210122907A1

    公开(公告)日:2021-04-29

    申请号:US16635670

    申请日:2018-08-03

    Abstract: The invention relates to composition comprising (A) a propylene-based polymer, (B1) a first elastomer of ethylene and α-olefin comonomer having 4 to 10 carbon atoms, (B2) a second elastomer of ethylene and α-olefin comonomer having 4 to 10 carbon atoms and (C) an inorganic filler, wherein (B1) the first elastomer has a density of 0.850 to 0.890 g/cm3 and a melt flow index of 5 to 50 dg/min measured in accordance with ASTM D1238 using a 2.16 kg weight and at a temperature of 190° C., wherein (B2) the second elastomer has a density of 0.850 to 0.890 g/cm3 and a melt flow index of 0.55 to 4 dg/min measured in accordance with ASTM D1238 using a 2.16 kg weight and at a temperature of 190° C., wherein the total amount of (B1) the first elastomer and (B2) the second elastomer is 2 to 30 wt % based on the total composition, wherein the amount of (C) the inorganic filler is 0.1 to 30 wt % based on the total composition.

    COMPOSITION COMPRISING HETEROPHASIC PROPYLENE COPOLYMER

    公开(公告)号:US20210122906A1

    公开(公告)日:2021-04-29

    申请号:US16635666

    申请日:2018-08-02

    Abstract: The invention relates to a composition comprising (A) a propylene-based polymer, (B) an elastomer of ethylene and α-olefin comonomer having 4 to 10 carbon atoms and (C) an inorganic filler, wherein (A) the propylene-based polymer has a melt flow index of 60 to 150 dg/min measured according to ASTM D1238 (2.16 kg/230° C.) and wherein (B) the elastomer has a density of 0.840 to 0.865 g/cm3, wherein (B) the elastomer has a melt flow index of 3 to 13 dg/min measured in accordance with ASTM D1238 using a 2.16 kg weight and at a temperature of 190° C., wherein the amount of (B) the elastomer is 2 to 30 wt % based on the total composition, wherein the amount of (C) the inorganic filler is 0.1 to 30 wt % based on the total composition.

    POLYPROPYLENE COMPOSITION
    3.
    发明申请

    公开(公告)号:US20200224017A1

    公开(公告)日:2020-07-16

    申请号:US16641694

    申请日:2018-08-30

    Abstract: The invention relates to a composition comprising: (A) a propylene-based polymer which is a propylene homopolymer or a propylene copolymer consisting of at least 90 wt % of propylene monomer units and at most 10 wt % of ethylene monomer units and/or an α-olefin monomer units having 4 to 10 carbon atoms and (B) a copolymer of ethylene and α-olefin comonomer having 4 to 10 carbon atoms, wherein the elastomer has a density of 0.850 to 0.910 g/cm3 and a melt flow rate of 15 to 50 dg/min measured in accordance with IS01 133 using a 2.16 kg weight and at a temperature of 190° C., wherein the amount of (A) the propylene-based polymer is 60 to 99 wt % and the amount of (B) the copolymer is 1 to 40 wt %, with respect to the total composition.

    COMPOSITION COMPRISING HETEROPHASIC PROPYLENE COPOLYMER

    公开(公告)号:US20180237624A1

    公开(公告)日:2018-08-23

    申请号:US15751513

    申请日:2016-07-14

    Abstract: The invention relates to a composition comprising (A) a heterophasic propylene copolymer and (B) an elastomer of ethylene and α-olefin comonomer having 4 to 8 carbon atoms, wherein the heterophasic propylene copolymer consists of (a) a propylene-based matrix, wherein the propylene-based matrix consists of a propylene homopolymer and/or a propylene copolymer consisting of at least 70 wt % of propylene and at most 30 wt % of ethylene or an α-olefin having 4-10 carbon atoms, based on the total weight of the propylene-based matrix and wherein the propylene-based matrix is present in an amount of 60 to 95 wt % based on the total heterophasic propylene copolymer and wherein the propylene-based matrix has a melt flow index of at least 0.1 dg/min and at most 45 dg/min, measured according to ISO1133 (2.16 kg/230° C.) and (b) a dispersed ethylene-α-olefin copolymer, wherein the dispersed ethylene-α-olefin copolymer is an ethylene-propylene copolymer, wherein the ethylene-α olefin copolymer is present in an amount of 40 to 5 wt % based on the total heterophasic propylene copolymer and wherein the sum of the total amount of propylene-based matrix and total amount of dispersed ethylene-α-olefin copolymer is 100 wt %, wherein the amount of ethylene in the ethylene-α-olefin copolymer of the heterophasic propylene copolymer is from 10 up to and including 45 wt % (RCC2) (B) an elastomer of ethylene and α-olefin comonomer having 4 to 8 carbon atoms wherein the elastomer has a density in the range from 0.88 up to and including 0.907 g/cm3.

    Polypropylene composition
    5.
    发明授权

    公开(公告)号:US11091618B2

    公开(公告)日:2021-08-17

    申请号:US16641694

    申请日:2018-08-30

    Abstract: The invention relates to a composition comprising: (A) a propylene-based polymer which is a propylene homopolymer or a propylene copolymer consisting of at least 90 wt % of propylene monomer units and at most 10 wt % of ethylene monomer units and/or an α-olefin monomer units having 4 to 10 carbon atoms and (B) a copolymer of ethylene and α-olefin comonomer having 4 to 10 carbon atoms, wherein the elastomer has a density of 0.850 to 0.910 g/cm3 and a melt flow rate of 15 to 50 dg/min measured in accordance with IS01 133 using a 2.16 kg weight and at a temperature of 190° C., wherein the amount of (A) the propylene-based polymer is 60 to 99 wt % and the amount of (B) the copolymer is 1 to 40 wt %, with respect to the total composition.

    Composition comprising heterophasic propylene copolymer

    公开(公告)号:US11332604B2

    公开(公告)日:2022-05-17

    申请号:US16635670

    申请日:2018-08-03

    Abstract: The invention relates to composition comprising (A) a propylene-based polymer, (B1) a first elastomer of ethylene and α-olefin comonomer having 4 to 10 carbon atoms, (B2) a second elastomer of ethylene and α-olefin comonomer having 4 to 10 carbon atoms and (C) an inorganic filler, wherein (B1) the first elastomer has a density of 0.850 to 0.890 g/cm3 and a melt flow index of 5 to 50 dg/min measured in accordance with ASTM D1238 using a 2.16 kg weight and at a temperature of 190° C., wherein (B2) the second elastomer has a density of 0.850 to 0.890 g/cm3 and a melt flow index of 0.55 to 4 dg/min measured in accordance with ASTM D1238 using a 2.16 kg weight and at a temperature of 190° C., wherein the total amount of (B1) the first elastomer and (B2) the second elastomer is 2 to 30 wt % based on the total composition, wherein the amount of (C) the inorganic filler is 0.1 to 30 wt % based on the total composition.

    Composition comprising heterophasic propylene copolymer

    公开(公告)号:US11072698B2

    公开(公告)日:2021-07-27

    申请号:US16635666

    申请日:2018-08-02

    Abstract: The invention relates to a composition comprising (A) a propylene-based polymer, (B) an elastomer of ethylene and α-olefin comonomer having 4 to 10 carbon atoms and (C) an inorganic filler, wherein (A) the propylene-based polymer has a melt flow index of 60 to 150 dg/min measured according to ASTM D1238 (2.16 kg/230° C.) and wherein (B) the elastomer has a density of 0.840 to 0.865 g/cm3, wherein (B) the elastomer has a melt flow index of 3 to 13 dg/min measured in accordance with ASTM D1238 using a 2.16 kg weight and at a temperature of 190° C., wherein the amount of (B) the elastomer is 2 to 30 wt % based on the total composition, wherein the amount of (C) the inorganic filler is 0.1 to 30 wt % based on the total composition.

    Composition comprising heterophasic propylene copolymer

    公开(公告)号:US10995206B2

    公开(公告)日:2021-05-04

    申请号:US15751513

    申请日:2016-07-14

    Abstract: The invention relates to a composition comprising (A) a heterophasic propylene copolymer and (B) an elastomer of ethylene and α-olefin comonomer having 4 to 8 carbon atoms, wherein the heterophasic propylene copolymer consists of (a) a propylene-based matrix, wherein the propylene-based matrix consists of a propylene homopolymer and/or a propylene copolymer consisting of at least 70 wt % of propylene and at most 30 wt % of ethylene or an α-olefin having 4-10 carbon atoms, based on the total weight of the propylene-based matrix and wherein the propylene-based matrix is present in an amount of 60 to 95 wt % based on the total heterophasic propylene copolymer and wherein the propylene-based matrix has a melt flow index of at least 0.1 dg/min and at most 45 dg/min, measured according to ISO1133 (2.16 kg/230° C.) and (b) a dispersed ethylene-α-olefin copolymer, wherein the dispersed ethylene-α-olefin copolymer is an ethylene-propylene copolymer, wherein the ethylene-α olefin copolymer is present in an amount of 40 to 5 wt % based on the total heterophasic propylene copolymer and wherein the sum of the total amount of propylene-based matrix and total amount of dispersed ethylene-α-olefin copolymer is 100 wt %, wherein the amount of ethylene in the ethylene-α-olefin copolymer of the heterophasic propylene copolymer is from 10 up to and including 45 wt % (RCC2) (B) an elastomer of ethylene and α-olefin comonomer having 4 to 8 carbon atoms wherein the elastomer has a density in the range from 0.88 up to and including 0.907 g/cm3.

Patent Agency Ranking