公开(公告)号:US20240199474A1
公开(公告)日:2024-06-20
申请号:US18542367
申请日:2023-12-15
Applicant: SCHOTT AG
Inventor: Meike Schneider , Bernd Rüdinger , Uwe Martens
CPC classification number: C03C10/0009 , C03B32/02 , C03C1/004 , C03C10/0054 , C03C21/002 , C03C2204/00 , H05K5/03
Abstract: A transparent, chemically prestressable or chemically prestressed glass ceramic is provided. The glass ceramic has keatite as a main crystal phase, a transmittance greater than 80% at a thickness of 0.7 mm, a haze of less than or equal to 10, and a crystal phase content of at least 80% by weight of keatite solid solution based on all crystal phases in the glass ceramic.
-
公开(公告)号:US20240199473A1
公开(公告)日:2024-06-20
申请号:US18542213
申请日:2023-12-15
Applicant: SCHOTT AG
Inventor: Meike Schneider , Bernd Rüdinger , Uwe Martens
CPC classification number: C03C10/0009 , C03B32/02 , C03C10/0054 , C03C21/002 , H05K5/03 , C03C2204/00
Abstract: A transparent, chemically prestressable or chemically prestressed glass ceramic has a high transmittance, a low haze and a high crystal phase content of keatite solid solution. A method of making such a glass ceramic includes producing a silicate green glass with a melting process and subsequent hot shaping, temperature treating the silicate green glass with at least one nucleation step carried out in the temperature range of 690° C. to 850° C. for a period of 5 min to 72 h and at least one ceramization step carried out in the temperature range of 780° ° C. to 1100° C. for a period of 3 min to 150 h, and performing at least one ion exchange in an exchange bath at a temperature of the exchange bath between 370° C. and 500° ° C. for a period of between 2 hours and 50 hours
-
公开(公告)号:US20220332630A1
公开(公告)日:2022-10-20
申请号:US17725024
申请日:2022-04-20
Applicant: Schott AG
Inventor: Ulrich Fotheringham , Simone Monika Ritter , Bernd Rüdinger , Peter Nabe
Abstract: A glass includes a composition characterized by the following constituent phases (in mol-%): 20-80 lanthanum titanate; 10-50 lanthanum niobate; 0-60 lanthanum molybdenum borate; 2-40 lanthanum borate; 2-40 yttrium borate; 0-40 gadolinium borate; 2-40 zirconium silicate; 2-40 diboron trioxide; and 0-20 silicon dioxide. A refractive index is at least 2.00.
-
公开(公告)号:US20210344039A1
公开(公告)日:2021-11-04
申请号:US17244355
申请日:2021-04-29
Applicant: SCHOTT AG
Inventor: Sebastian Leukel , Meike Schneider , Andreas Roters , Jörg Schumacher , Wolfgang Schmidbauer , Bernd Rüdinger
IPC: H01M10/0562 , H01M10/0525 , H01M50/434
Abstract: The disclosure relates to an aluminum-doped lithium ion conductor based on a garnet structure comprising lanthanum, in particular an aluminum-doped lithium lanthanum zirconate (LLZO), in which the latter is co-doped with at least one trivalent M3+ ion on the lanthanum site, and in which the trivalent M3+ ion has an ionic radius that is smaller than that of La3+, and a higher lithium content is present in comparison to a stoichiometric garnet structure, with the provision that if M3+ is yttrium, a further trivalent M3+ ion, which is different than Y3+ and has an ionic radius that is smaller than that of La3+, is co-doped on the lanthanum site. A co-doping strategy is carried out, in which a doping on the lanthanum site with ions of the same valence, but smaller diameter brings about the change in the lattice geometry to the cubic modification. This leads to a stabilization of the cubic crystal modification that is present also with superstoichiometric quantities of lithium.
-
-
-