TRANSPARENT GLASS CERAMIC AND COVER PANE
    4.
    发明公开

    公开(公告)号:US20240199473A1

    公开(公告)日:2024-06-20

    申请号:US18542213

    申请日:2023-12-15

    Applicant: SCHOTT AG

    Abstract: A transparent, chemically prestressable or chemically prestressed glass ceramic has a high transmittance, a low haze and a high crystal phase content of keatite solid solution. A method of making such a glass ceramic includes producing a silicate green glass with a melting process and subsequent hot shaping, temperature treating the silicate green glass with at least one nucleation step carried out in the temperature range of 690° C. to 850° C. for a period of 5 min to 72 h and at least one ceramization step carried out in the temperature range of 780° ° C. to 1100° C. for a period of 3 min to 150 h, and performing at least one ion exchange in an exchange bath at a temperature of the exchange bath between 370° C. and 500° ° C. for a period of between 2 hours and 50 hours

    Glass ceramic substrate made of a transparent, colored LAS glass ceramic and method for producing it
    5.
    发明申请
    Glass ceramic substrate made of a transparent, colored LAS glass ceramic and method for producing it 审中-公开
    由透明的彩色LAS玻璃陶瓷制成的玻璃陶瓷基片及其制造方法

    公开(公告)号:US20160176752A1

    公开(公告)日:2016-06-23

    申请号:US14757392

    申请日:2015-12-23

    Applicant: SCHOTT AG

    CPC classification number: C03C10/0027 C03B32/02 C03C3/097 C03C23/007

    Abstract: A glass ceramic substrate made of a transparent, colored LAS glass ceramic is provided. The glass ceramic has a gradient layer with keatite solid solution and an underlying core with high-quartz solid solution as predominant crystal phase. The keatite solid solution in a depth of 10 μm or greater exceeds 50% of the sum of the high-quartz solid solution proportion and keatite solid solution proportion. The ceramization includes a crystal transformation step, in which the high-quartz solid solution is transformed at a maximum temperature in the range of 910° to 980° and a time period of between 1 and 25 minutes in part into the keatite solid solution.

    Abstract translation: 提供由透明的有色LAS玻璃陶瓷制成的玻璃陶瓷基片。 玻璃陶瓷具有具有酮钙石固溶体的梯度层和具有高石英固溶体作为主要晶相的下层核心。 深度为10μm以上的凯氏体固溶体超过了高石英固溶体比例和酮钙石固溶体比例之和的50%以上。 陶瓷化包括晶体转变步骤,其中将高石英固溶体在910°至980°的范围内的最高温度和1至25分钟的时间段内部分转化为酮钙石固溶体。