公开(公告)号:US20190002344A1
公开(公告)日:2019-01-03
申请号:US15749780
申请日:2017-02-14
Applicant: SOUTHWEST PETROLEUM UNIVERSITY
Inventor: Ping GUO , Shuai WU , Yijian CHEN , Huimin ZHANG , Wanbo ZHANG , Yuhong DU , Zhouhua WANG , Jianfen DU , Yisheng HU , Huang LIU , Hongmei REN
CPC classification number: C04B20/1025 , B28B7/384 , C04B14/04 , C04B14/06 , C04B28/04 , C04B40/0067 , C04B2111/00991 , C09K8/46 , G01N1/286 , G01N2001/2866 , G01N2001/2893 , C04B20/008
Abstract: A manufacturing method of a big-model low-permeability microcrack core includes: (1) determining the size of a microcrack core to be manufactured; (2) placing stones in a baking oven to bake for 24 h under 120° C., placing the stones into a mixer, mixing and spraying oil, enabling the oil to seep into the stone, evenly forming a thin oil film on stone's surface; (3) mixing the oil sprayed stone with quartz sand and cement, adding water to mix evenly to obtain cement paste; (4) spreading butter on core mould's inner surface to form a thin butter film, pouring the cement paste into the core mould to obtain a cement sample; (5) loading confining pressure outside the core according to the requirements of porosity and permeability of the mould to adjust a pore permeability value; (6) obtaining the big-model core with microcrack after the cement sample is dried and formed.
-
2.
公开(公告)号:US20180348105A1
公开(公告)日:2018-12-06
申请号:US15775391
申请日:2016-12-02
Applicant: SOUTHWEST PETROLEUM UNIVERSITY
Inventor: Ping GUO , Shuai WU , Wanbo ZHANG , Yisheng HU , Yijian CHEN , Huimin ZHANG , Zhouhua WANG , Jianfen DU , Huang LIU , Hongmei REN
CPC classification number: G01N1/36 , G01N15/082 , G01N15/088 , G01N33/241 , G01N2001/2873 , G01N2001/366
Abstract: A direct method for manufacturing a large model fractured core and maintaining original oil-water saturation, including the following steps: (1) determining the volume V, porosity φ, permeability K, oil saturation So, water saturation Sw and the like of a fractured core to be manufactured; (2) preparing simulated oil, and determining the used oil mass mo=Vo×ρo; (3) under the circumstance of no consideration of oil saturation, acquiring the mass of the used water, cement and quartz sand; (4) while establishing oil saturation, acquiring the mass mw of water for manufacturing the core as mw=a−Vo×ρw; (5) mixing oil, water and an emulsifier evenly to prepare an oil-in-water emulsion; (6) adding cement and quartz sand into the emulsion and stirring evenly to obtain cement slurry; (7) when a cement sample is in a semi-solidified state, cutting the cement sample with a steel wire; and (8) solidifying the cement sample to the end.
-