公开(公告)号:US11802086B2
公开(公告)日:2023-10-31
申请号:US17275670
申请日:2019-09-05
Applicant: SUMITOMO OSAKA CEMENT CO., LTD.
Inventor: Daisaku Maeda , Keijiro Shigeru
IPC: C04B35/48 , C03C10/00 , C03C17/25 , C04B35/622 , C04B35/64
CPC classification number: C04B35/481 , C03C10/00 , C03C17/25 , C04B35/62222 , C04B35/64 , C03C2217/213 , C03C2217/22 , C03C2217/228 , C03C2217/23 , C03C2217/70 , C03C2218/112 , C03C2218/119 , C03C2218/32 , C04B2235/3227 , C04B2235/3244 , C04B2235/3409 , C04B2235/3418 , C04B2235/6567
Abstract: An anti-fouling coating film of the present invention includes a component (A): zirconium; a component (B): lanthanum; and a component (C): at least one selected from the group consisting of silicon, phosphorus, and boron, in which in a case where masses of the component (A), the component (B), and the component (C) are used by being converted into masses of oxides thereof, total mass of the component (A) and the component (B) with respect to a mass of the anti-fouling coating film is 90% or more and 95% or less, and in a case where X is defined by X=mass of component (B)/(total mass of component (A)+component (B))×100, X is 20% or more and 50% or less, and the mass of the component (C) to the mass of the anti-fouling coating film is 5% or more and [6+(X−20)/6]% or less.
-
公开(公告)号:US10480081B2
公开(公告)日:2019-11-19
申请号:US15762394
申请日:2016-09-02
Applicant: SUMITOMO OSAKA CEMENT CO., LTD.
Inventor: Keijiro Shigeru
Abstract: Disclosed is a method of manufacturing a dishwasher including: forming a first layer containing zirconium oxide and silicon oxide on a surface of the inner wall at a heat treatment of 200° C. or higher; forming a second layer containing an oxoacid on a surface of the first layer at a heat treatment temperature lower than the heat treatment temperature of the first layer; and obtaining a thin-film layer containing zirconium oxide and silicon oxide on the surface of the inner wall and having a contact angle of water of 20° or less on the surface, after removing the second layer by using a washing method, in which the first layer contains the zirconium oxide in an amount of 80 mass % or more in terms of oxide and the silicon oxide in an amount of 1-20 mass % in terms of oxide.
-
公开(公告)号:US20150210600A1
公开(公告)日:2015-07-30
申请号:US14421327
申请日:2014-02-24
Applicant: Sumitomo Osaka Cement Co., Ltd.
Inventor: Keijiro Shigeru
IPC: C04B41/00
CPC classification number: C04B41/0018 , C04B41/009 , C04B41/52 , C04B41/70 , C04B41/89 , Y10T428/249957 , C04B28/02 , C04B14/285 , C04B33/00 , C04B41/5031 , C04B41/5089 , C04B41/501
Abstract: A porous article is obtained by filling pores of at least one principal surface of a porous body which is formed of an inorganic material, with a mixture containing metal oxide particles and an alkaline silicate, in which the filled mixture is coated by a film containing a hydrated compound of zirconium and a silicate. According to this porous article, an effect of preventing surface contamination is superior, and alkali resistance and acid resistance are superior. In addition, a production treatment of the porous article can be performed at room temperature or at a relatively low temperature of 100° C. or lower. Therefore, the production cost can be significantly reduced.
Abstract translation: 通过填充由无机材料形成的多孔体的至少一个主表面的孔与含有金属氧化物颗粒和碱性硅酸盐的混合物填充多孔制品,其中填充的混合物用含有 锆和硅酸盐的水合化合物。 根据该多孔制品,防止表面污染的效果优异,耐碱性和耐酸性优异。 此外,多孔制品的制造处理可以在室温或相对低的100℃以下的温度下进行。 因此,可以显着降低生产成本。
-
-