公开(公告)号:US20220178060A1
公开(公告)日:2022-06-09
申请号:US17539298
申请日:2021-12-01
Applicant: TAIWAN TEXTILE RESEARCH INSTITUTE
Inventor: Ying-Chi LIN , Wei-Hung CHEN , Li-Chen CHU , Rih-Sheng CHIANG
Abstract: A breathable and waterproof non-woven fabric is manufactured by a manufacturing method including the following steps. Performing a kneading process on 87 to 91 parts by weight of a polyester, 5 to 7 parts by weight of a water repellent, and 3 to 6 parts by weight of a flow promoter to form a mixture, in which the polyester has a melt index between 350 g/10 min and 1310 g/10 min at a temperature of 270° C., and the mixture has a melt index between 530 g/10 min and 1540 g/10 min at a temperature of 270° C. Performing a melt-blowing process on the mixture, such that the flow promoter is volatilized and a melt-blown fiber is formed, in which the melt-blown fiber has a fiber body and the water repellent disposed on the fiber body with a particle size (D90) between 350 nm and 450 nm.
-
公开(公告)号:US20240167204A1
公开(公告)日:2024-05-23
申请号:US18426583
申请日:2024-01-30
Applicant: TAIWAN TEXTILE RESEARCH INSTITUTE
Inventor: Ying-Chi LIN , Wei-Hung CHEN , Li-Chen CHU , Rih-Sheng CHIANG
CPC classification number: D04H3/033 , B32B5/022 , B32B5/265 , B32B7/14 , D06M11/79 , B32B2255/02 , B32B2255/20 , B32B2307/724 , B32B2307/73 , D06M2200/12
Abstract: A breathable and waterproof non-woven fabric is manufactured by a manufacturing method including the following steps. Performing a kneading process on 87 to 91 parts by weight of a polyester, 5 to 7 parts by weight of a water repellent, and 3 to 6 parts by weight of a flow promoter to form a mixture, in which the polyester has a melt index between 350 g/10 min and 1310 g/10 min at a temperature of 270° C., and the mixture has a melt index between 530 g/10 min and 1540 g/10 min at a temperature of 270° C. Performing a melt-blowing process on the mixture, such that the flow promoter is volatilized and a melt-blown fiber is formed, in which the melt-blown fiber has a fiber body and the water repellent disposed on the fiber body with a particle size (D90) between 350 nm and 450 nm.
-
公开(公告)号:US20240158968A1
公开(公告)日:2024-05-16
申请号:US18422136
申请日:2024-01-25
Applicant: TAIWAN TEXTILE RESEARCH INSTITUTE
Inventor: Ying-Chi LIN , Wei-Hung CHEN , Li-Chen CHU , Rih-Sheng CHIANG
CPC classification number: D04H3/033 , B32B5/022 , B32B5/265 , B32B7/14 , D06M11/79 , B32B2255/02 , B32B2255/20 , B32B2307/724 , B32B2307/73 , D06M2200/12
Abstract: A breathable and waterproof non-woven fabric is manufactured by a manufacturing method including the following steps. Performing a kneading process on 87 to 91 parts by weight of a polyester, 5 to 7 parts by weight of a water repellent, and 3 to 6 parts by weight of a flow promoter to form a mixture, in which the polyester has a melt index between 350 g/10 min and 1310 g/10 min at a temperature of 270° C., and the mixture has a melt index between 530 g/10 min and 1540 g/10 min at a temperature of 270° C. Performing a melt-blowing process on the mixture, such that the flow promoter is volatilized and a melt-blown fiber is formed, in which the melt-blown fiber has a fiber body and the water repellent disposed on the fiber body with a particle size (D90) between 350 nm and 450 nm.
-
-