公开(公告)号:US09452377B2
公开(公告)日:2016-09-27
申请号:US14079662
申请日:2013-11-14
发明人: Jingshen Wu , Dong Lv , Zheming Zhang , Dan Li
IPC分类号: C04B35/64 , B01D39/20 , C04B35/622 , C04B38/00 , C04B111/00
CPC分类号: B01D39/2068 , C04B35/62245 , C04B35/64 , C04B38/00 , C04B2111/00801 , C04B2235/5228 , C04B2235/5284 , C04B38/0074 , C04B38/067
摘要: A nanoporous ceramic membrane and preparation method thereof is provided. The nanoporous ceramic membrane is prepared by halloysite nanotubes (HNTs), and its porosity is between 35% to 85%. This method comprises steps as following: HNTs and polymers with a certain ratio are dispersed in organic solvent, and HNTs/polymer composite fibers are prepared through electrospinning method; after the HNTs/polymers composite fibers are laminated, they are sintered at high temperature in a certain or vacuum atmosphere, and a nanoporous ceramic membrane is obtained. Ceramic membrane prepared by this method is corrosion resistant, thermal resistant, and have large specific surface area, it may widely applied in the field of filtration, catalyst carrier and purification of high-temperature gas, etc.
摘要翻译: 提供了纳米多孔陶瓷膜及其制备方法。 纳米多孔陶瓷膜由多水高岭土纳米管(HNTs)制备,孔隙率在35%〜85%之间。 该方法包括以下步骤:将具有一定比例的HNTs和聚合物分散在有机溶剂中,通过静电纺丝法制备HNTs /聚合物复合纤维; 在层合有HNTs /聚合物复合纤维之后,在某些或真空气氛中在高温下烧结,得到纳米多孔陶瓷膜。 通过该方法制备的陶瓷膜耐腐蚀,耐热,比表面积大,可广泛应用于过滤领域,催化剂载体和高温气体净化等领域。