Abstract:
An object of the present invention is to provide a positive electrode mixture capable of conducting stable charging and discharging with a less amount of gasses generated which has an operating voltage or an initial crystal phase transition voltage of not less than 4.5 V on the basis of lithium. The present invention relates to a positive electrode mixture comprising carbon black having a bulk density of not more than 0.1 g/cm3, a crystallite size of 10 to 40 Å, an iodine adsorption of 1 to 150 mg/g, a volatile content of not more than 0.1% and a metal impurity content of not more than 20 ppm, and a positive electrode active substance having an operating voltage or an initial crystal phase transition voltage of not less than 4.5 V on the basis of lithium.
Abstract:
Provided herein are processes for producing positive electrode active substance particles for non-aqueous electrolyte secondary batteries which is excellent in life characteristics of a battery with respect to a repeated charging and discharging performance thereof, as well as a non-aqueous electrolyte secondary battery. In particular, provided herein are processes for producing a positive electrode active substance for non-aqueous electrolyte secondary batteries comprising lithium transition metal layered oxide having a composition represented by the formula: Lia(NixCoyMn1-x-y)O2 wherein a is 1.0≤a≤1.15; x is 0
Abstract:
The present invention relates to lithium composite oxide particles which can be produced by mixing nickel-cobalt-manganese-based compound particles, a zirconium raw material and a lithium raw material with each other and then calcining the resulting mixture, and comprise a Zr compound that is allowed to be present on a surface thereof, in which the Zr compound is represented by the chemical formula: Lix(Zr1-yAy)Oz wherein x, y and z are 2.0≤x≤8.0; 0≤y≤1.0; and 2.0≤z≤6.0, respectively, and a content of Zr in the lithium composite oxide particles is 0.05 to 1.0% by weight. By using the lithium composite oxide particles as a positive electrode active substance, it is possible to produce a lithium ion secondary battery that has a low electric resistance at a high temperature, and is excellent in cycle characteristic at a high temperature as well as high-temperature rate characteristic.
Abstract:
The present invention relates to positive electrode active substance particles for non-aqueous electrolyte secondary batteries, comprising an oxide having a spinel structure and comprising at least Li and Mn as main components and an oxide comprising at least Li and Zr, in which the oxide comprising at least Li and Zr forms a mixed phase comprising two or more phases, and a content of the oxide comprising at least Li and Zr in the positive electrode active substance particles is 0.1 to 4% by weight. The present invention provides positive electrode active substance particles for non-aqueous electrolyte secondary batteries which are excellent in high-temperature characteristics and a process for producing the positive electrode active substance particles, and a non-aqueous electrolyte secondary battery.
Abstract:
The present invention relates to lithium composite oxide particles which can be produced by mixing nickel-cobalt-manganese-based compound particles, a zirconium raw material and a lithium raw material with each other and then calcining the resulting mixture, and comprise a Zr compound that is allowed to be present on a surface thereof, in which the Zr compound is represented by the chemical formula: Lix(Zr1-yAy)Oz wherein x, y and z are 2.0≦x≦8.0; 0≦y≦1.0; and 2.0≦z≦6.0, respectively, and a content of Zr in the lithium composite oxide particles is 0.05 to 1.0% by weight. By using the lithium composite oxide particles as a positive electrode active substance, it is possible to produce a lithium ion secondary battery that has a low electric resistance at a high temperature, and is excellent in cycle characteristic at a high temperature as well as high-temperature rate characteristic.
Abstract:
The present invention relates to positive electrode active substance particles for non-aqueous electrolyte secondary batteries, comprising an oxide having a spinel structure and comprising at least Li and Mn as main components and an oxide comprising at least Li and Zr, in which the oxide comprising at least Li and Zr forms a mixed phase comprising two or more phases, and a content of the oxide comprising at least Li and Zr in the positive electrode active substance particles is 0.1 to 4% by weight. The present invention provides positive electrode active substance particles for non-aqueous electrolyte secondary batteries which are excellent in high-temperature characteristics and a process for producing the positive electrode active substance particles, and a non-aqueous electrolyte secondary battery.