Abstract:
The present invention relates to positive electrode active substance particles comprising a compound having a spinel type structure comprising at least Li, Ni and Mn, and having an Li content which is controlled such that a molar ratio of Li(Ni+Mn) therein is 0.3 to 0.65, an Ni content of 5 to 25% by weight, an Na content of 0.05 to 1.9% by weight and an S content of 0.0005 to 0.16% by weight, a sum of the Na content and the S content being 0.09 to 1.9005% by weight. The positive electrode active substance particles according to the present invention can be suitably used as positive electrode active substance particles for non-aqueous electrolyte secondary batteries which can exhibit a high discharge voltage and an excellent discharge capacity.
Abstract:
This invention provides lithium manganate which has a high output and is excellent in high-temperature stability. This invention relates to lithium manganate particles which are produced by mixing a lithium compound, a manganese compound, a Y compound and an A compound and then calcining the resulting mixture, and have a composition represented by the following chemical formula 1 and an average secondary particle diameter (D50) of 1 to 15 μm, in which Y is at least one element selected from the group consisting of Al and Mg; A is a sintering aid element having a melting point of not higher than 850° C.; x and y satisfy 0.03≤x≤0.15 and 0≤y≤0.20, respectively; z is in the range of 0 to 2.5 mol % based on Mn, wherein the lithium manganate particles have a sulfur content of not more than 100 ppm. Li1+xMn2-x-yYyO4zA (Chemical Formula 1)
Abstract:
The present invention aims at providing lithium manganate having a high output and an excellent high-temperature stability. The above aim can be achieved by lithium manganate particles having a primary particle diameter of not less than 1 μm and an average particle diameter (D50) of kinetic particles of not less than 1 μm and not more than 10 μm, which are substantially in the form of single crystal particles and have a composition represented by the following chemical formula: Li1+xMn2-x-yYyO4 in which Y is at least one element selected from the group consisting of Al, Mg and Co; x and y satisfy 0.03≦x≦0.15 and 0.05≦y≦0.20, respectively, wherein the Y element is uniformly dispersed within the respective particles, and an intensity ratio of I(400)/I(111) thereof is not less than 33% and an intensity ratio of I(440)/I(111) thereof is not less than 16%.
Abstract:
The present invention provides a precursor of positive electrode active substance particles for non-aqueous electrolyte secondary batteries which have a high discharge voltage and a high discharge capacity, hardly suffer from side reactions with an electrolyte solution, and are excellent in cycle characteristics, positive electrode active substance particles for non-aqueous electrolyte secondary batteries, and processes for producing these particles, and a non-aqueous electrolyte secondary battery. The present invention relates to positive electrode active substance particles for non-aqueous electrolyte secondary batteries having a spinel structure with a composition represented by the following chemical formula (1), in which the positive electrode active substance particles satisfy the following characteristic (A) and/or characteristic (B) when indexed with Fd-3m in X-ray diffraction thereof: (A) when indexed with Fd-3m in X-ray diffraction of the positive electrode active substance particles, a ratio of I(311) to I(111) [I(311)/I(111)] is in the range of 35 to 43%, and/or (B) when indexed with Fd-3m in X-ray diffraction of the positive electrode active substance particles, a gradient of a straight line determined by a least square method in a graph prepared by plotting sin θ in an abscissa thereof and B cos θ in an ordinate thereof wherein B is a full-width at half maximum with respect to each peak position 2θ (10 to 90°) is in the range of 3.0×10−4 to 20.0×10−4; and Li1+xMn2−y−zNiyMzO4 Chemical Formula (1) wherein x, y, z fall within the range of −0.05·x·0.15, 0.4·y·0.6 and 0·z·0.20, respectively; and M is at least one element selected from the group consisting of Mg, Al, Si, Ca, Ti, Co, Zn, Sb, Ba, W and Bi.
Abstract:
The present invention aims at providing lithium manganate having a high output and an excellent high-temperature stability. The above aim can be achieved by lithium manganate particles having a primary particle diameter of not less than 1 μm and an average particle diameter (D50) of kinetic particles of not less than 1 μm and not more than 10 μm, which are substantially in the form of single crystal particles and have a composition represented by the following chemical formula: Li1+xMn2-x-yYyO4 in which Y is at least one element selected from the group consisting of Al, Mg and Co; x and y satisfy 0.03≦x≦0.15 and 0.05≦y≦0.20, respectively, wherein the Y element is uniformly dispersed within the respective particles, and an intensity ratio of I(400)/I(111) thereof is not less than 33% and an intensity ratio of I(440)/I(111) thereof is not less than 16%.
Abstract translation:本发明的目的在于提供具有高输出和优异的高温稳定性的锰酸锂。 上述目的可以通过一次粒径不小于1μm的锰酸锂颗粒和动态颗粒的平均粒径(D50)不小于1μm和不大于10μm来实现,其基本上在 具有由以下化学式表示的组成的Li1 + xMn2-x-yYyO4,其中Y是选自Al,Mg和Co中的至少一种元素; x和y分别满足0.03 @ x @ 0.15和0.05 @ y @ 0.20,其中Y元素均匀分散在各个颗粒内,其I(400)/ I(111)的强度比不小于33 %,I(440)/ I(111)的强度比不小于16%。