Abstract:
According to the present invention, even when a high recovery ratio operation is performed, the influence of concentration of ingredients to be separated in the feed fluid can be reduced, the concentration polarization can be prevented by increasing the turbulence effect on the membrane surface, and the fluid permeation performance and the separation performance of the separation membrane element can be maintained.
Abstract:
The present invention provides a separation membrane and a separation membrane element which are capable of exhibiting good water production performance and excellent in handleability and process passage. A separation membrane of the present invention is a separation membrane including: a separation membrane main body having a feed-side face and a permeate-side face; and a permeate-side channel member adhered to the permeate-side face of the separation membrane main body, in which the permeate-side channel member includes a composition containing at least a high-crystalline polypropylene (A) and satisfies the following requirements (a) and (b): (a) a content of the high-crystalline polypropylene (A) in the composition is from 40 to 95% by weight; and (b) the permeate-side channel member has a melting endothermic energy amount (ΔH) of from 20 to 70 J/g.
Abstract:
The present invention relates to a flat-sheet separation membrane element having formed therein a separation membrane pair in which separation membranes are disposed such that permeation-side faces thereof face each other and in which a channel material is provided, wherein the area of a high-elasticity region satisfying a bending modulus of 100-1000 MPa and a maximum bending stress of 1-15 MPa at least in one direction is not less than 10% of the area of a filtration region of the pair of separation membranes.
Abstract:
The present invention provides a separation membrane and a separation membrane element capable of exhibiting a good water production performance even at a high temperature and also excellent handleability and quality. The separation membrane of the present invention includes a separation membrane main body having a feed-side face and a permeate-side face; and a permeate-side channel member fixed onto the permeate-side face of the separation membrane main body, and the permeate-side channel member includes polypropylene as a main component and satisfies the following requirements (a) to (c): (a) a softening point temperature is 60° C. or higher; (b) a tensile elongation in a standard state is 10% or more; and (c) a yield point stress under a wet condition at 50° C. is 2 MPa or more.
Abstract:
The present invention relates to a separation membrane element for use in separation of ingredients contained in fluids such as liquid and gas. An object of the present invention is to provide a separation membrane element which, even when used in a high-recovery ratio operation, has high fresh-water production performance and high removal performance and is less apt to suffer scaling.
Abstract:
The purpose of the present invention is to provide a composite semipermeable membrane having achieved both strength and water-permeable properties. This composite semipermeable membrane is provided with a substrate, a porous support body disposed on the substrate, and a separation function layer provided on the porous support body. The substrate has a structure provided with a crimped portion and a non-crimped portion. The porous support body is impregnated inside a crimped portion and inside a non-crimped portion of the substrate.
Abstract:
In order to provide a composite semipermeable membrane which combines strength and water permeability, the present invention provides a composite semipermeable membrane including: a supporting membrane including a substrate and a porous support; and a separation functional layer disposed on the porous support, in which the substrate has a weight A per unit area, a portion of the porous support which is located within the substrate has a weight B per unit area, and a sum of the weight A and the weight B, (A+B), is 30 to 100 g/m2, and a ratio between the weight A and the weight B, B/A, is 0.10 to 0.60.