摘要:
An antiglare film is provided, the antiglare film including: a support; and an antiglare layer including a surface that has asperities, wherein the antiglare layer contains at least first light-transmitting particles and second light-transmitting particles, the first light-transmitting particles have an average particle size that is 0.01 to 2.5 μm greater than an average thickness of the antiglare layer, the second light-transmitting particles have an average particle size that is at least 0.1 μm smaller than the average thickness of the antiglare layer, the first light-transmitting particles are contained in an amount of 0.1 to 2 mass % based on a total solid content in the antiglare layer, the second light-transmitting particles are contained in an amount of 2 to 30 mass % based on the total solid content in the antiglare layer, and the second light-transmitting particles include organic polymer-containing particles each of which has a core particle/shell layer structure.
摘要:
A light-scattering film is provided and includes a transparent support having thereon at least a light-scattering layer. When substantially parallel light is incident on a surface of the film at an incident angle of 5°, the reflectance for an angle θ in the light-receiving part measured in a plane containing the film normal line and the incident direction is R(θ), the value obtained by normalizing R(θ) by the reflectance of regular reflection is Rrel(θ), and the value calculated from the maximum variation |dRrel(θ)/dθ|max for the angle θ is a scattering coefficient A (formula 1), the reflection coefficient B (formula 2) calculated from the scattering coefficient A and the 5° specular reflectance Rs is from 2.0 to 5.0. Scattering coefficient A=1/(10×|dRrel(θ)/dθ|max) (Formula 1) Reflection coefficient B=2.2×log 10(Rs)−7.5×log 10(A)+5.9 (Formula 2)
摘要:
An optical film, is provided, the optical film including: a support; and at least one antiglare layer having a surface that has asperities, wherein the at least one antiglare layer contains at least one kind of light transmitting particles including first light transmitting particles in an amount of 0.01 to 1 mass % based on a total solid content in the antiglare layer, the first light transmitting particles have an average particle size that is 0.1 to 4.0 μm greater than an average thickness of the antiglare layer, and a region θ(0.5) in which slope angles θ of the asperities of the surface of the antiglare layer lie within a range of 0°
摘要:
A light-scattering film is provided and includes a transparent support having thereon at least a light-scattering layer. When substantially parallel light is incident on a surface of the film at an incident angle of 5°, the reflectance for an angle θ in the light-receiving part measured in a plane containing the film normal line and the incident direction is R(θ), the value obtained by normalizing R(θ) by the reflectance of regular reflection is Rrel(θ), and the value calculated from the maximum variation |dRrel(θ)/dθ|max for the angle θ is a scattering coefficient A (formula 1), the reflection coefficient B (formula 2) calculated from the scattering coefficient A and the 5° specular reflectance Rs is from 2.0 to 5.0. Scattering coefficient A=1/(10×|dRrel(θ)/dθ|max) (Formula 1) Reflection coefficient B=2.2×log 10(Rs)−7.5×log 10(A)+5.9 (Formula 2)
摘要:
An optical film, is provided, the optical film including: a support; and at least one antiglare layer having a surface that has asperities, wherein the at least one antiglare layer contains at least one kind of light transmitting particles including first light transmitting particles in an amount of 0.01 to 1 mass % based on a total solid content in the antiglare layer, the first light transmitting particles have an average particle size that is 0.1 to 4.0 μm greater than an average thickness of the antiglare layer, and a region θ(0.5) in which slope angles θ of the asperities of the surface of the antiglare layer lie within a range of 0°
摘要:
An antiglare film is provided and includes: a transparent support; and an antiglare layer containing a binder and a light-transmitting fine particle. The light-transmitting fine particle has an average particle diameter of 3 to 15 μm, the antiglare layer has an average thickness smaller than the average particle diameter of the light-transmitting fine particle by 0.1 to 2.0 μm, the antiglare layer contains the light-transmitting fine particle in an amount of 1.0 to 3.0 weight % based on all solid contents of the antiglare layer. The antiglare layer has a surface having a θ(1) of 60 to 98.5%, wherein the θ(1) is a ratio of a surface region of 0°≦θ≦1° in the surface when θ represents a tilt angle of an irregularity on the surface.
摘要:
An antiglare film is provided, the antiglare film including: a support; and an antiglare layer including a surface that has asperities, wherein the antiglare layer contains at least first light-transmitting particles and second light-transmitting particles, the first light-transmitting particles have an average particle size that is 0.01 to 2.5 μm greater than an average thickness of the antiglare layer, the second light-transmitting particles have an average particle size that is at least 0.1 μm smaller than the average thickness of the antiglare layer, the first light-transmitting particles are contained in an amount of 0.1 to 2 mass % based on a total solid content in the antiglare layer, the second light-transmitting particles are contained in an amount of 2 to 30 mass % based on the total solid content in the antiglare layer, and the second light-transmitting particles include organic polymer-containing particles each of which has a core particle/shell layer structure.
摘要:
Provided is an optical film including a transparent support; and an antiglare layer that comprises a light-transmitting resin and at least two kinds of light-transmitting particles, wherein the antiglare layer has a thickness of from 10 μm to 15 μm, each kind of the at least two kinds of light transmitting particles has an average particle size of from 7 μm to 15 μm, each kind of the at least two kinds of light transmitting particles has a refractive index different from a refractive index of the light-transmitting resin by from 0.001 to 0.050 in absolute value, and a total amount of the at least two kinds of light-transmitting particles are from 15 to 40 mass % based on all solid contents in the antiglare layer.
摘要:
An antiglare film includes a transparent support; and an antiglare layer containing a binder and a fine particle, wherein the antiglare layer has an average thickness smaller than an average particle diameter of the fine particle, and the antiglare layer has a surface roughness skewness (Rsk) of from 0.5 to 1.5.
摘要:
A method for producing an optical film is provided and includes: simultaneously coating at least two coating solutions over a transparent support, the at least two coating solutions each containing a solvent and a solute; and drying the solvent in each of the at least two coating solutions to provide at least two coating layers. When the at least two coating layers are 1, 2, . . . n−1 and n layers in sequence from the outermost surface of the at least two coating layers toward the transparent support, n being an integer of 2 or more, the main component of the solute in the n-th layer is insoluble or sparingly soluble in the main component of the solvent in the (n−1)-th layer.