    Heat storing material, composition thereof and their use 审中-公开
    储热材料及其用途及其用途

    公开(公告)号:US20050106392A1

    公开(公告)日:2005-05-19

    申请号:US10506051

    申请日:2003-03-07

    摘要: A heat-accumulative material composed of a polymer or oligomer having a melting point of −10 to 100° C. and latent heat of 30 J/g or more for use around a body, and heat-accumulative composition comprising the same heat-accumulative material. The heat-accumulative material tends to be kept at a constant temperature more effectively by absorbing heat as ambient temperature increases to melt, and releasing heat as ambient temperature decreases to solidify, to moderate the effect of changed ambient temperature, and thereby to exhibit the function as a heat-accumulative material. They have a sufficiently high viscosity, preventing the heat-accumulative material from flowing out even when it is molten. Each of the heat-accumulative material and composition can be made into a heat-accumulative film or sheet, laminate, molded article, composite fiber and cloth which can be suitably used around a body.

    摘要翻译: 由熔点为-10〜100℃的聚合物或低聚物构成的蓄热材料和在身体周围使用的潜热为30J / g以上的蓄热材料,以及包含相同的蓄热性的蓄热组合物 材料。 当周围环境温度升高时,热​​积累材料通过吸收热量更有效地保持在恒定温度下进行融化,并且随着环境温度的降低固化而释放热量,以缓解环境温度变化的影响,从而发挥功能 作为蓄热材料。 它们具有足够高的粘度,即使在熔融时也能防止蓄热材料流出。 每个蓄热材料和组合物可以制成可适用于身体周围的热积聚膜或片,层压体,模制品,复合纤维和布。

    Formaldehyde scavenger and wood material using same
    3.
    发明授权
    Formaldehyde scavenger and wood material using same 有权
    甲醛清除剂和木材使用相同

    公开(公告)号:US08389125B2

    公开(公告)日:2013-03-05

    申请号:US13000982

    申请日:2009-06-26

    IPC分类号: B32B21/04

    摘要: Provided are a formaldehyde scavenger capable of providing excellent formaldehyde scavenging performance without discoloring a wood material and not reemitting formaldehyde, and a wood material using the same.The formaldehyde scavenger contains urea, ammonium phosphate monobasic and ammonium phosphate dibasic. The formaldehyde scavenger contains urea, ammonium phosphate monobasic and ammonium phosphate dibasic preferably in a weight ratio of urea/ammonium phosphate monobasic/ammonium phosphate dibasic in the range of 5 to 45/0.5 to 15/1 to 20, and further preferably in a weight ratio of urea/ammonium phosphate monobasic/ammonium phosphate dibasic in the range of 10 to 35/1 to 10/2 to 15. The wood material is prepared by applying the formaldehyde scavenger thereto. The formaldehyde scavenger is preferably applied in the range of 1 to 50 g/m2 by dry weight.

    摘要翻译: 提供能够提供卓越的甲醛清除性能而不使木材变色而不再次发生甲醛的甲醛清除剂,以及使用其的木材。 甲醛清除剂含有尿素,磷酸二氢铵和磷酸氢二铵。 甲醛清除剂含有尿素,磷酸二氢铵和磷酸氢二铵,优选以尿素/磷酸二氢铵/磷酸氢二铵的重量比为5〜45 / 0.5〜15/1〜20,进一步优选为重量 尿素/磷酸二氢铵/磷酸氢二铵的比例在10〜35/1〜10/2〜15的范围内。通过向其中施加甲醛清除剂制备木材。 甲醛清除剂的干燥重量优选为1〜50g / m 2。

    FORMALDEHYDE SCAVENGER AND WOOD MATERIAL USING SAME
    4.
    发明申请
    FORMALDEHYDE SCAVENGER AND WOOD MATERIAL USING SAME 有权
    甲醛防腐剂和使用它的木材

    公开(公告)号:US20110171482A1

    公开(公告)日:2011-07-14

    申请号:US13000982

    申请日:2009-06-26

    IPC分类号: B32B21/04 C09K3/00

    摘要: Provided are a formaldehyde scavenger capable of providing excellent formaldehyde scavenging performance without discoloring a wood material and not reemitting formaldehyde, and a wood material using the same.The formaldehyde scavenger contains urea, ammonium phosphate monobasic and ammonium phosphate dibasic. The formaldehyde scavenger contains urea, ammonium phosphate monobasic and ammonium phosphate dibasic preferably in a weight ratio of urea/ammonium phosphate monobasic/ammonium phosphate dibasic in the range of 5 to 45/0.5 to 15/1 to 20, and further preferably in a weight ratio of urea/ammonium phosphate monobasic/ammonium phosphate dibasic in the range of 10 to 35/1 to 10/2 to 15. The wood material is prepared by applying the formaldehyde scavenger thereto. The formaldehyde scavenger is preferably applied in the range of 1 to 50 g/m2 by dry weight.

    摘要翻译: 提供能够提供卓越的甲醛清除性能而不使木材变色而不再次发生甲醛的甲醛清除剂,以及使用其的木材。 甲醛清除剂含有尿素,磷酸二氢铵和磷酸氢二铵。 甲醛清除剂含有尿素,磷酸二氢铵和磷酸氢二铵,优选以尿素/磷酸二氢铵/磷酸氢二铵的重量比为5〜45 / 0.5〜15/1〜20,进一步优选为重量 尿素/磷酸二氢铵/磷酸氢二铵的比例在10〜35/1〜10/2〜15的范围内。通过向其中施加甲醛清除剂制备木材。 甲醛清除剂的干燥重量优选为1〜50g / m 2。