摘要:
A method for increasing the porosity and crushability characteristics thereof embodies the firing of a ceramic compact comprising a reactant fugitive filler material and a ceramic material in a controlled atmosphere.
摘要:
A core for investment casting directionally solidified eutectic and superalloy material consists of alumina which has a porous microstructure in which the grain morphology is characteristic of grains which have undergone vapor phase transport action.
摘要:
A method for simultaneously forming an integral barrier layer on selected external surfaces of a fired ceramic article and for increasing the porosity content and crushability characterstics thereof embodies the firing of a ceramic compact comprising a reactant fugitive filler material and a ceramic material in a controlled atmosphere.
摘要:
Optically translucent theoretically dense body of mullite is produced by pressing an amorphous mixed oxide powder composition of from about 72.5 weight % to about 76.5 weight % Al.sub.2 O.sub.3 /balance SiO.sub.2 into a compact of density of at least 1.0 g/cc, sintering the compact in oxygen or a vacuum of 0.05 torr to 1 torr producing a gas-impermeable compact, hot isostatically pressing the gas-impermeable compact to theoretical density, and with respect to compositions ranging from higher than about 74 wt % Al.sub.2 O.sub.3 /balance SiO.sub.2, annealing the theoretically dense body.
摘要翻译:通过将约72.5重量%至约76.5重量%的Al 2 O 3 /平衡SiO 2的无定形混合氧化物粉末组合物压制成至少为1.0g / cc的密度的压块,将氧化物烧结成型,从而产生光学半透明的理论致密的莫来石体 或者为0.05torr至1torr的真空,产生不透气体的压块,将不透气的压块热等静压到理论密度,并且对于高于约74重量%的Al 2 O 3 /平衡SiO 2的组成,退火理论致密 身体。
摘要:
Amorphous mixed oxide powder composed of from about 74 weight % to about 76.5 weight % Al.sub.2 O.sub.3 balance SiO.sub.2 is pressed into a compact with a density of at least 1 g/cc and sintered in oxygen producing an optically translucent theoretically dense body of mullite.
摘要翻译:将由约74重量%至约76.5重量%的Al 2 O 3平衡SiO 2组成的无定形混合氧化物粉末压制成密度为至少1g / cc的压块,并在氧气中烧结,产生光学半透明的理论致密的莫来石体。
摘要:
Amorphous mixed oxide powder composed of from about 74 weight % to about 76.5 weight % Al.sub.2 O.sub.3 balance SiO.sub.2 is pressed into a compact with a density of at least 1 g/cc, fired in oxygen or vacuum of 0.05 to 1 torr producing a gas-impermeable compact, and sintered in air, argon, helium, nitrogen or mixtures thereof producing an optically translucent theoretically dense body of mullite.
摘要翻译:将由约74重量%至约76.5重量%的Al 2 O 3平衡SiO 2组成的无定形混合氧化物粉末压制成密度为至少1g / cc的压块,在氧气或在真空中烧制为0.05至1乇,产生气体不可渗透 在空气,氩气,氦气,氮气或其混合物中烧结,产生光学半透明的理论上致密的莫来石体。
摘要:
A method for simultaneously forming an integral porous outer barrier layer having a density gradient therein on selected external surfaces of a fired ceramic article and for increasing the porosity content and crushability characteristics thereof embodies the firing of a ceramic compact comprising a reactant fugitive filler material and a ceramic material in a controlled atmosphere.
摘要:
A setter is configured to minimize distortion of a core supported during firing. The configuration also provides for adequate gas flow both to envelope the core and to provide an aspiration effort to cause the gas to be drawn downwardly through and about the core structure to the interior of the setter to enhance the removal of reaction products therefrom. A retort, preferably made of molybdenum, is provided to enhance the effects of the setter configuration.
摘要:
A method for simultaneously forming an integral barrier layer on selected external surfaces of a fired alumina-based compound ceramic article and for increasing the porosity and crushability characteristics thereof embodies the sintering of a ceramic compact comprising a reactant fugitive filler material and the alumina-based compound ceramic material in a controlled atmosphere.
摘要:
A fired alumina article having a core of material having from 20 to 65 percent continuous porosity by volume and desired crushability characteristics and an integral outer barrier layer consisting of porous alumina having a density gradient.