摘要:
A semicrystalline propylene polymer composition with good suitability for producing biaxially oriented films and prepared by polymerizing propylene, ethylene and/or C4-C18-1-alkenes, where at least 50 mol % of the monomer units present arise from the polymerization of propylene. Also described is the use of the semicrystalline propylene polymer composition for producing films, fibers or moldings, the films, fibers and moldings made from these compositions, biaxially stretched films made from the semicrystalline propylene polymer compositions, and also a method for characterizing the semicrystalline propylene polymer compositions.
摘要:
Random copolymers of propylene with other 1-alkenes having up to carbon atoms, whose content of comonomers is in the range from 0.7 to 1.4% by weight if the only comonomer present in the propylene copolymers is ethylene, or whose content of comonomers is in the range from 0.7 to 3.0% by weight if at least one C4–C10-1-alkene is present as comonomer, and whose cold-xylene-soluble fraction is from 1.0 to 2.5% by weight if ethylene is present as a comonomer in the propylene copolymers, or whose cold-xylene-soluble fraction is from 0.75 to 2.0% by weight if the only comonomers present are C4–C10-1-alkenes, and a process for preparing the random copolymers of propylene is described, as is their use for producing films, fibers or moldings, and also the films, fibers and moldings themselves and biaxially stretched films made from random propylene copolymers of this type and processes for their production.
摘要:
The present invention relates to a semicrystalline propylene polymer composition prepared by polymerizing propylene, ethylene and/or C4-C18-1-alkenes, where at least 50 mol % of the monomer units present stem from the polymerization of propylene and at least 20% by weight of the propylene polymer composition is the result of a polymerization using metallocene catalysts, with a melting point TM of from 65 to 170° C., where the semicrystalline propylene polymer composition can be broken down into from 65 to 85% by weight of a principal component A, from 10 to 35% by weight of an ancillary component B and from 0 to 25% by weight of an ancillary component C.
摘要:
Random copolymers of propylene with other 1-alkenes having up to carbon atoms, whose content of comonomers is in the range from 0.7 to 1.4% by weight if the only comonomer present in the propylene copolymers is ethylene, or whose content of comonomers is in the range from 0.7 to 3.0% by weight if at least one C4–C10-1-alkene is present as comonomer, and whose cold-xylene-soluble fraction is from 1.0 to 2.5% by weight if ethylene is present as a comonomer in the propylene copolymers, or whose cold-xylene-soluble fraction is from 0.75 to 2.0% by weight if the only comonomers present are C4–C10-1-alkenes, and a process for preparing the random copolymers of propylene is described, as is their use for producing films, fibers or moldings, and also the films, fibers and moldings themselves and biaxially stretched films made from random propylene copolymers of this type and processes for their production.
摘要:
Random copolymers of propylene with other 1-alkenes having up to carbon atoms, whose content of comonomers is in the range from 0.7 to 1.4% by weight if the only comonomer present in the propylene copolymers is ethylene, or whose content of comonomers is in the range from 0.7 to 3.0% by weight if at least one C4-C10-1-alkene is present as comonomer, and whose cold-xylene-soluble fraction is from 1.0 to 2.5% by weight if ethylene is present as a comonomer in the propylene copolymers, or whose cold-xylene-soluble fraction is from 0.75 to 2.0% by weight if the only comonomers present are C4-C10-1-alkenes, and a process for preparing the random copolymers of propylene is described, as is their use for producing films, fibers or moldings, and also the films, fibers and moldings themselves and biaxially stretched films made from random propylene copolymers of this type and processes for their production.
摘要:
Random copolymers of propylene with other 1-alkenes having up to carbon atoms, whose content of comonomers is in the range from 0.7 to 1.4% by weight if the only comonomer present in the propylene copolymers is ethylene, or whose content of comonomers is in the range from 0.7 to 3.0% by weight if at least one C4-C10-1-alkene is present as comonomer, and whose cold-xylene-soluble fraction is from 1.0 to 2.5% by weight if ethylene is present as a comonomer in the propylene copolymers, or whose cold-xylene-soluble fraction is from 0.75 to 2.0% by weight if the only comonomers present are C4-C10-1-alkenes, and a process for preparing the random copolymers of propylene is described, as is their use for producing films, fibers or moldings, and also the films, fibers and moldings themselves and biaxially stretched films made from random propylene copolymers of this type and processes for their production.
摘要:
The present invention relates to a semicrystalline propylene polymer composition prepared by polymerizing propylene, ethylene and/or C4-C18-1-alkenes, where at least 50 mol % of the monomer units present stem from the polymerization of propylene and at least 20% by weight of the propylene polymer composition is the result of a polymerization using metallocene catalysts, with a melting point TM of from 65 to 170° C., where the semicrystalline propylene polymer composition can be broken down into from 65 to 85% by weight of a principal component A, from 10 to 35% by weight of an ancillary component B and from 0 to 25% by weight of an ancillary component C, and where the proportions of components A, B and C are determined by carrying out TREF (temperature rising elution fractionation) in which that fraction of the propylene polymer composition which is soluble in xylene at (TM/2)+7.5° C. is firstly dissolved and separated off and then, as the temperature rises, at all of the higher temperatures 70° C., 75° C., 80° C., 85° C., 90° C., 94° C., 98° C., 102° C., 107° C., 112° C., 117° C., 122° C. and 125° C., the fractions soluble within the temperature range between this elution temperature and the preceding elution temperature are eluted, and the principal component A is formed by all of the fractions which are eluted at above (TM/2)+7.5° C. and have an average molar mass MN [sic] (number average)≧120,000 g/mol, the ancillary component B is formed by the fraction which is eluted at (TM/2)+7.5° C., and the ancillary component C is formed by all of the fractions which are eluted at above (TM/2)+7.5° C. and have an average molar mass Mn (number average)
摘要:
Novel supported, titanized chromium catalysts for the homopolymerization of ethylene and the copolymerization of ethylene with α-olefins, a process for preparing them and to their use for the polymerization of olefins.
摘要:
Novel supported, titanized chromium catalysts can be used for the homopolymerization of ethylene and the copolymerization of ethylene with α-olefins.
摘要:
Novel supported, titanized chromium catalysts for the homopolymerization of ethylene and the copolymerization of ethylene with α-olefins, a process for preparing them and to their use for the polymerization of olefins.