    摘要: A continuous vapor-phase fluidized-bed process for the preparation of ethylene homopolymers and copolymers having a density of from 0.87 to 0.97 g/cm3 in which ethylene or mixtures of ethylene and C3-C8 a-monoolefins are (co)polymerized in the presence of a supported chromium catalyst in the polymerization zone of a vapor-phase fluidized-bed reactor under pressures ranging from 1 to 100 bar and at temperatures ranging from 30° to 125° C. in the vapor phase in an agitated bed of bulk material comprising particulate polymer, the resultant heat of polymerization is removed by cooling the recirculated reactor gas and the resulting (co)polymer is removed from the vapor-phase fluidized-bed reactor, wherein, for the preparation of a (co)polymer of a specific density d, the (co)polymerization is carried out at a temperature which is in a range restricted by an upper envelope defined by equation I T H = 171 + 6 ⁢ d ′ 0.84 - d ′ ( I ) and a lower envelope defined by equation II T L = 173 + 7.3 ⁢ d ′ 0.837 - d ′ , ( II ) in which the variables have the following meanings: TH is the highest reaction temperature in ° C.; TL is the lowest reaction temperature in ° C.; d′ is the numerical value of the density d of the (co)polymer to be synthesized.

    摘要翻译: 用于制备密度为0.87至0.97g / cm 3的乙烯均聚物和共聚物的连续气相流化床方法,其中乙烯或乙烯和C 3 -C 8α-单烯烃的混合物(共)聚合 在负载的铬催化剂的存在下,在气相流化床反应器的聚合区域的存在下,在压力范围为1至100巴,温度范围为30至125℃,气相在搅拌床 包含颗粒聚合物的散装材料,通过冷却再循环的反应器气体除去所得到的聚合热,并将所得(共)聚合物从气相流化床反应器中除去,其中,为制备(共)聚合物 特定密度d,(共)聚合在由等式I定义的上包络限制的范围内进行,并且由等式IIin定义的下包络,其中变量具有以下含义:T H是最高的反应温度,单位°C; TL是最低反应温度(℃); d'是待合成的(共)聚合物的密度d的数值。

    Vapor-phase fluidized-bed process and ethylene homopolymers and copolymers produced thereby
    6.
    发明授权
    Vapor-phase fluidized-bed process and ethylene homopolymers and copolymers produced thereby 失效
    气相流化床方法和由此制备的乙烯均聚物和共聚物

    公开(公告)号:US06849699B2

    公开(公告)日:2005-02-01

    申请号:US10658916

    申请日:2003-09-11

    CPC分类号: C08F10/02 C08F4/24 C08F2/34

    摘要: A continuous vapor-phase fluidized-bed process for the preparation of ethylene homopolymers and copolymers having a density of from 0.87 to 0.97 g/cm3 in which ethylene or mixtures of ethylene and C3-C8 a-monoolefins are (co)polymerized in the presence of a supported chromium catalyst in the polymerization zone of a vapor-phase fluidized-bed reactor under pressures ranging from 1 to 100 bar and at temperatures ranging from 30° to 125° C. in the vapor phase in an agitated bed of bulk material comprising particulate polymer, the resultant heat of polymerization is removed by cooling the recirculated reactor gas and the resulting (co)polymer is removed from the vapor-phase fluidized-bed reactor, wherein, for the preparation of a (co)polymer of a specific density d, the (co)polymerization is carried out at a temperature which is in a range restricted by an upper envelope defined by equation I T H = 171 + 6 ⁢   ⁢ d ′ 0.84 - d ′ ( I ) and a lower envelope defined by equation II T L = 173 + 7.3 ⁢   ⁢ d ′ 0.837 - d ′ , ( II ) in which the variables have the following meanings: TH is the highest reaction temperature in ° C.; TL is the lowest reaction temperature in ° C.; d′ is the numerical value of the density d of the (co)polymer to be synthesized.

    摘要翻译: 用于制备密度为0.87至0.97g / cm 3的乙烯均聚物和共聚物的连续气相流化床方法,其中乙烯或乙烯和C 3 -C 8α-单烯烃的混合物(共)聚合 在负载的铬催化剂的存在下,在气相流化床反应器的聚合区域的存在下,在压力范围为1至100巴,温度范围为30至125℃,气相在搅拌床 包含颗粒聚合物的散装材料,通过冷却再循环的反应器气体除去所得到的聚合热,并将所得(共)聚合物从气相流化床反应器中除去,其中,为制备(共)聚合物 特定密度d,(共)聚合在由等式I定义的上包络限制的范围内进行,并且由等式IIin定义的下包络,其中变量具有以下含义:T H是最高的反应温度,单位°C; TL是最低反应温度(℃); d'是待合成的(共)聚合物的密度d的数值。

    Gaseous phase fluidized-bed reactor
    10.
    发明授权
    Gaseous phase fluidized-bed reactor 失效
    气相流化床反应器

    公开(公告)号:US07601303B1

    公开(公告)日:2009-10-13

    申请号:US09700367

    申请日:1999-05-04

    IPC分类号: B01J8/18

    摘要: Gas-phase fluidized-bed reactor for polymerizing ethylenically unsaturated monomers, comprising a reactor chamber (1) in the form of a vertical tube, if desired a calming zone (2) following the upper section of the reactor chamber, a circulation gas line (3), a circulation gas compressor (4) and a cooling device (5), where, in the region of transition of the reaction gas from the circulation gas line into the reactor chamber and in the lower section of the reactor chamber itself, there is either no gas distributor plate at all or only a gas distributor plate the total surface area of whose gas orifices is more than 20% of the total surface area of said gas distributor plate.

    摘要翻译: 用于聚合烯键式不饱和单体的气相流化床反应器,包括垂直管形式的反应器室(1),如果需要,在反应器室的上部之后的平静区域(2),循环气体管线 3),循环气体压缩机(4)和冷却装置(5),其中在反应气体从循环气体管线进入反应器室和反应器室本身的下部的过渡区域 完全不是气体分配器板,或者只有气体分配器板,其气体孔的总表面积大于所述气体分布板的总表面积的20%。