CPC分类号: C08J9/20 , C08J9/00 , C08J9/141 , C08J9/16 , C08J2325/06
摘要: The invention provides a process for preparing expandable styrene polymers which comprises the steps of:(a) adding an aqueous phase comprising a suspension stabilizer and an organic phase comprising styrene and an initiator to a reactor,(b) commencing the addition of a blowing agent at a styrene conversion in the range from 40 to 70% and adding the blowing agent over a period ranging from 30 to 60 minutes,(c) adding a stabilizer to stabilize the bead size distribution of the expandable styrene polymer at a styrene conversion in the range from 65 to 99%.
摘要翻译: 本发明提供了制备可发性苯乙烯聚合物的方法,其包括以下步骤:(a)将包含悬浮稳定剂的水相和包含苯乙烯和引发剂的有机相加入到反应器中,(b)开始加入发泡剂 苯乙烯转化率为40-70%,并在30-60分钟的时间内加入发泡剂,(c)在苯乙烯转化率下加入稳定剂以稳定可发性苯乙烯聚合物的珠粒尺寸分布 范围从65%到99%。
-
公开(公告)号:US08455559B2
公开(公告)日:2013-06-04
申请号:US13046154
申请日:2011-03-11
申请人: Wolfgang Ferstl , Jun Gao , Klaus Hahn , Pascal Hesse , Jan Holoch , Klaus-Dieter Hungenberg , Wolfram Husemann , Renata Jovanovic , Wolfgang Kasten , Olaf Kriha , Eckhard Neufeld , Michel Pepers , Birgit Reinhard , Bernhard Schmied , Rudolf Süttinger , Ping Zhang
发明人: Wolfgang Ferstl , Jun Gao , Klaus Hahn , Pascal Hesse , Jan Holoch , Klaus-Dieter Hungenberg , Wolfram Husemann , Renata Jovanovic , Wolfgang Kasten , Olaf Kriha , Eckhard Neufeld , Michel Pepers , Birgit Reinhard , Bernhard Schmied , Rudolf Süttinger , Ping Zhang
CPC分类号: C08J9/20 , C08J9/00 , C08J9/141 , C08J9/16 , C08J2325/06
摘要: The invention provides a process for preparing expandable styrene polymers which comprises the steps of: (a) adding an aqueous phase comprising a suspension stabilizer and an organic phase comprising styrene and an initiator to a reactor, (b) commencing the addition of a blowing agent at a styrene conversion in the range from 40 to 70% and adding the blowing agent over a period ranging from 30 to 60 minutes, (c) adding a stabilizer to stabilize the bead size distribution of the expandable styrene polymer at a styrene conversion in the range from 65 to 99%.
摘要翻译: 本发明提供了制备可发性苯乙烯聚合物的方法,其包括以下步骤:(a)将包含悬浮稳定剂的水相和包含苯乙烯和引发剂的有机相加入到反应器中,(b)开始加入发泡剂 苯乙烯转化率为40-70%,并在30-60分钟的时间内加入发泡剂,(c)在苯乙烯转化率下加入稳定剂以稳定可发性苯乙烯聚合物的珠粒尺寸分布 范围从65%到99%。
-