1.
公开(公告)号:US09122179B2
公开(公告)日:2015-09-01
申请号:US13972360
申请日:2013-08-21
Applicant: XEROX CORPORATION
Inventor: Jay Lee Schneider , Abdisamed Sheik-Qasim , Randy Pheav Tin , Christopher Michael Wolfe , Richard Philip Nelson Veregin , Mark Elliott , Melanie Davis , Cuong Vong , Shigang Steven Qiu
IPC: G03G9/08
CPC classification number: G03G9/0804 , G03G9/081 , G03G9/0819 , G03G9/0823 , G03G9/09392
Abstract: A method of forming toner particles includes aggregating a mixture of a latex, a wax, and an optional pigment to form pre-toner particles, and coalescing the pre-toner particles at a substantially constant target temperature selected within a range from about the glass transition temperature of the pre-toner particles to about 75° C., thereby creating toner particles having a substantially constant particle size distribution during the coalescing step.
Abstract translation: 形成调色剂颗粒的方法包括将胶乳,蜡和任选颜料的混合物聚集以形成预调色剂颗粒,并将预调色剂颗粒聚集在基本上恒定的目标温度下,所述目标温度在约玻璃化转变 预调色剂颗粒的温度至约75℃,从而在聚结步骤期间产生具有基本恒定的粒度分布的调色剂颗粒。
-
公开(公告)号:US20150099226A1
公开(公告)日:2015-04-09
申请号:US14047426
申请日:2013-10-07
Applicant: XEROX CORPORATION
Inventor: Ke Zhou , Guerino G. Sacripante , Yulin Wang , Abdisamed Sheik-Qasim , Rashid Mahmood , Rosa Duque
IPC: G03G9/08
CPC classification number: G03G9/0804 , G03G9/0819 , G03G9/0827 , G03G9/08755 , G03G9/08795 , G03G9/08797 , G03G9/09392
Abstract: A method for preparing toner particles is disclosed. In embodiments, a suitable method includes aggregating a mixture comprising at least one resin, an optional pigment and an optional wax to form aggregated particles, freezing aggregation of particles by adjusting the pH of the aggregated particles to a freezing aggregation pH; coalescing the aggregated particles to form toner particles at a first pH that is higher than the freezing aggregation pH; and recovering the toner particles.
Abstract translation: 公开了调色剂颗粒的制备方法。 在实施方案中,合适的方法包括聚集包含至少一种树脂,任选颜料和任选的蜡的混合物以形成凝集颗粒,通过将凝集颗粒的pH调节至凝固聚集pH来冻结颗粒的聚集; 聚集凝集的颗粒以在高于冷冻聚集pH的第一pH下形成调色剂颗粒; 并回收调色剂颗粒。
-
公开(公告)号:US09864291B1
公开(公告)日:2018-01-09
申请号:US15187475
申请日:2016-06-20
Applicant: XEROX CORPORATION
Inventor: Richard P. N. Veregin , Valerie M. Farrugia , Frank Ping-Hay Lee , Michael J. D'Amato , Michael S. Hawkins , Edward G. Zwartz , Yulin Wang , Abdisamed Sheik-Qasim , Sandra J. Gardner
CPC classification number: G03G9/09371 , G03G9/0821 , G03G9/09321 , G03G9/09364
Abstract: A hybrid toner includes a core having at least one amorphous polyester resin and at least one crystalline polyester resin, and at least one styrene/acrylate resin, a shell comprising at least one styrene/acrylate resin, at least one wax, and optionally a pigment dispersion, the first modulated differential calorimetry scan of the hybrid toner shows at least two melting point peaks below about 80° C., and the difference between the two melting point peaks is less than or equal to about 15° C.
-
公开(公告)号:US09195155B2
公开(公告)日:2015-11-24
申请号:US14047426
申请日:2013-10-07
Applicant: XEROX CORPORATION
Inventor: Ke Zhou , Guerino G. Sacripante , Yulin Wang , Abdisamed Sheik-Qasim , Rashid Mahmood , Rosa Duque
CPC classification number: G03G9/0804 , G03G9/0819 , G03G9/0827 , G03G9/08755 , G03G9/08795 , G03G9/08797 , G03G9/09392
Abstract: A method for preparing toner particles is disclosed. In embodiments, a suitable method includes aggregating a mixture comprising at least one resin, an optional pigment and an optional wax to form aggregated particles, freezing aggregation of particles by adjusting the pH of the aggregated particles to a freezing aggregation pH; coalescing the aggregated particles to form toner particles at a first pH that is higher than the freezing aggregation pH; and recovering the toner particles.
Abstract translation: 公开了调色剂颗粒的制备方法。 在实施方案中,合适的方法包括聚集包含至少一种树脂,任选颜料和任选的蜡的混合物以形成凝集颗粒,通过将凝集颗粒的pH调节至凝固聚集pH来冻结颗粒的聚集; 聚集凝集的颗粒以在高于冷冻聚集pH的第一pH下形成调色剂颗粒; 并回收调色剂颗粒。
-
公开(公告)号:US20170363984A1
公开(公告)日:2017-12-21
申请号:US15187475
申请日:2016-06-20
Applicant: XEROX CORPORATION
Inventor: Richard P. N. Veregin , Valerie M. Farrugia , Frank Ping-Hay Lee , Michael J. D'Amato , Michael S. Hawkins , Edward G. Zwartz , Yulin Wang , Abdisamed Sheik-Qasim , Sandra J. Gardner
CPC classification number: G03G9/09371 , G03G9/0821 , G03G9/09321 , G03G9/09364
Abstract: A hybrid toner includes a core having at least one amorphous polyester resin and at least one crystalline polyester resin, and at least one styrene/acrylate resin, a shell comprising at least one styrene/acrylate resin, at least one wax, and optionally a pigment dispersion, the first modulated differential calorimetry scan of the hybrid toner shows at least two melting point peaks below about 80° C., and the difference between the two melting point peaks is less than or equal to about 15° C.
-
公开(公告)号:US20150153663A1
公开(公告)日:2015-06-04
申请号:US14093860
申请日:2013-12-02
Applicant: Xerox Corporation
Inventor: Abdisamed Sheik-Qasim , Richard PN Veregin , Mark R Elliott , Melanie L Davis , Shigang Qiu , Jay L Schneider , Randy P Tin , Magid Kamel , Cuong Vong , Edward G Zwartz
IPC: G03G9/08
CPC classification number: G03G9/0804 , G03G9/0819 , G03G9/0821 , G03G9/08782 , G03G9/08795 , G03G9/08797 , G03G9/09392
Abstract: An emulsion aggregation toner process that does not require addition of base to freeze toner particle growth is described.
Abstract translation: 描述了不需要添加碱来冷冻调色剂颗粒生长的乳液聚集调色剂方法。
-
7.
公开(公告)号:US20150056551A1
公开(公告)日:2015-02-26
申请号:US13972360
申请日:2013-08-21
Applicant: XEROX CORPORATION
Inventor: Jay Lee Schneider , Abdisamed Sheik-Qasim , Randy Pheav Tin , Christopher Michael Wolfe , Richard Philip Nelson Veregin , Mark Elliott , Melanie Davis , Cuong Vong , Shigang Steven Qiu
IPC: G03G9/08
CPC classification number: G03G9/0804 , G03G9/081 , G03G9/0819 , G03G9/0823 , G03G9/09392
Abstract: A method of forming toner particles includes aggregating a mixture of a latex, a wax, and an optional pigment to form pre-toner particles, and coalescing the pre-toner particles at a substantially constant target temperature selected within a range from about the glass transition temperature of the pre-toner particles to about 75° C., thereby creating toner particles having a substantially constant particle size distribution during the coalescing step.