摘要:
A glass substrate for a magnetic disk of the present invention is one in which a laser beam is irradiated on a main surface thereby forming a large number of protrusions thereon to form texture thereon, each of said protrusions being formed by a protruded portion having a convex shape, said glass having a composition in which 0.2 to 3 wt % of an oxide of a transition metal is contained and an absorption coefficient with respect to a wavelength of a light at 266 nm being within a range of 0.03 to 2 .mu.m.sup.-1, and by setting the absorption coefficient of the glass with respect to a wavelength of a light at 266 nm within a range of 0.03 to 2 .mu.m.sup.-1 and irradiating a laser beam having a wavelength in a range of ultraviolet rays selectively on the main surface of a glass substrate at predetermined intervals, texture comprising a large number of protrusions formed by protruded portions each having a small diameter and a convex shape is formed.
摘要:
A glass substrate for an information recording medium has an acid resistance represented by an etching rate of at most 45 nm/min. upon contact with a hydrofluoric acid having a temperature of 50° C. and a concentration of 0.1 weight %. The glass substrate has a recording surface having an average surface roughness Ra smaller than 0.3 nm.
摘要:
A glass substrate for an information recording medium has an acid resistance represented by an etching rate of at most 45 nm/min. upon contact with a hydrofluoric acid having a temperature of 50° C. and a concentration of 0.1 weight %. The glass substrate has a recording surface having an average surface roughness Ra smaller than 0.3 nm.
摘要:
Provided is a glass composition suitable for a glass substrate for a flat panel display such as a liquid crystal display. This glass composition has high thermal stability, and is substantially free of BaO but has a low devitrification temperature. It is suitable for the production of a glass substrate by a downdraw process. This glass composition contains, in terms of mass %; 54 to 62% of SiO2; 4 to 11% of B2O3; 15 to 20% of Al2O3; 2 to 5% of MgO; 0 to 7% of CaO; 0 to 13.5% of SrO; 0 to 1% of K2O; 0 to 1% of SnO2; and 0 to 0.2% of Fe2O3, and is substantially free of BaO. In this glass composition, the total content of alkaline earth metal oxides (MgO+CaO+SrO) is 10 to 18.5 mass %. The devitrification temperature of the glass composition is 1200° C. or lower.
摘要:
The present invention provides a glass article using a glass composition including a base glass composition and colorants. The base glass composition includes, expressed in mass %: 65 to 80% of SiO2; 0 to 5% of Al2O3; 0 to 10% of MgO; 0 to 15% of CaO; 5 to 15% of MgO+CaO; 10 to 18% of Na2O; 0 to 5% of K2O; 10 to 20% of Na2O+K2O; and 0 to 5% of B2O3, and the colorants consist essentially of, expressed in mass %: 0.6% to 1.0% of T-Fe2O3; 0.026 to 0.8% of TiO2; 0 to 2.0% of CeO2; 0.01 to 0.03% of CoO; 0 to 0.0008% of Se; and 0.06 to 0.20% of NiO. The glass article has a grayish color tone, and has a visible light transmittance in a range of 15% to 40%, which is measured with the illuminant A at a thickness of 3.1 mm.
摘要:
A glass composition which is reduced in the amount of residual bubbles and is produced using smaller amounts of an environmentally unfriendly component such as arsenic oxide and antimony oxide. This glass composition comprises, in terms of mass %: 40-70% SiO2; 5-20% B2O3; 10-25% Al2O3; 0-10% MgO; 0-20% CaO; 0-20% SrO; 0-10% BaO; 0.001-0.5% Li2O; 0.01-0.5% Na2O; 0.002-0.5% K2O; and 0-1.0%, excluding 0%, Cl
摘要:
A glass composition of the present invention includes the following components, in terms of mass % and mass ppm: 60 to 79% SiO2; 0 to 13% B2O3 (exclusive of 13%); 0 to 10% Al2O3; 0 to 10% Li2O; more than 0% but not more than 20% Na2O; 0 to 15% K2O; 0 to 10% MgO; 0 to 15% CaO; 0 to 15% SrO; 0 to 15% BaO; 0 to 10% ZnO; 0 to 15% Nb2O5; 0 to 20% Ta2O5; more than 0.02% but not more than 10% TiO2; and 0.5 to 50 ppm T-Fe2O3 (where T-Fe2O3 denotes a total iron oxide obtained by converting all of iron compounds into Fe2O3).
摘要翻译:本发明的玻璃组合物,以质量%和质量ppm为基准,含有60〜79%的SiO 2, 0〜13%B2O3(不含13%); 0〜10%Al2O3; 0〜10%Li2O; 大于0%但不大于20%的Na2O; 0〜15%K2O; 0〜10%MgO; 0〜15%CaO; 0〜15%SrO; 0〜15%BaO; 0〜10%的ZnO; 0〜15%Nb2O5; 0〜20%Ta2O5; 超过0.02%但不超过10%的TiO2; 和0.5〜50ppm的T-Fe 2 O 3(其中T-Fe 2 O 3表示通过将全部铁化合物转化为Fe 2 O 3得到的总氧化铁)。