Method of soldering honeycomb body
    4.
    再颁专利
    Method of soldering honeycomb body 失效
    蜂窝体焊接方法

    公开(公告)号:USRE35063E

    公开(公告)日:1995-10-17

    申请号:US188448

    申请日:1994-01-21

    IPC分类号: B23K1/00 B23P13/00

    CPC分类号: B23K1/0014

    摘要: When soldering a honeycomb body formed by alternately piling flat foils (plates) and corrugated foils (plates), a binder liquid is sucked up from the end face of tile honeycomb body to form a binder streak in a space defined by contacting portions of the flat foil (plate) and corrugated foil (plate), a solder is scattered and applied onto the binder streak, and the honeycomb body is then dried and heated to effect a soldering of the honeycomb body. According to this method, soldering can be accomplished only in the vicinity of the contacting portions of the flat foil (plate) and corrugated foil (plate), with a desired soldering structure.

    摘要翻译: 当焊接通过交替打桩扁平箔(板)和波纹箔(板)形成的蜂窝体时,粘合剂液体从瓷砖蜂窝体的端面被吸起,以在平坦部分接触限定的空间中形成粘合剂条纹 箔(板)和波纹箔(板),焊料被散射并施加到粘合剂条纹上,然后将蜂窝体干燥并加热以实现蜂窝体的焊接。 根据该方法,只能在平板(板)和波纹箔(板)的接触部分附近具有期望的焊接结构。

    Method of straightening wire rods of titanium and titanium alloy
    5.
    发明授权
    Method of straightening wire rods of titanium and titanium alloy 失效
    矫直钛和钛合金线材的方法

    公开(公告)号:US6077369A

    公开(公告)日:2000-06-20

    申请号:US817804

    申请日:1997-03-19

    CPC分类号: B21D3/12 B23P15/002

    摘要: A method of straightening a wire rod of titanium or titanium alloy wherein the rod is hot-straightened to a straight rod at the straightening temperature T and elongation .epsilon. satisfying the expression (1) or (2). The method includes hot rolling a titanium billet of .beta. titanium alloy, (.alpha.+.beta.) titanium alloy or a near .alpha. titanium alloy into a wire rod, winding the hot rolled wire rod into a coil, cold drawing the wire rod, cutting the wire rod to obtain a bent wire rod, heating the bent wire rod to a straightening temperature T while both end portions of the bent wire rod are fixed, applying a predetermined elongation .epsilon. to the wire rod, maintaining a straightening temperature T, hot-straightening the wire in accordance with the expression (2).epsilon.(T-400).gtoreq.400 (1).epsilon.(T-500).gtoreq.200 (2)and cooling the wire rod while applying tension. The method is suitable for preparing a straight rod for use in an engine valve.

    摘要翻译: PCT No.PCT / JP95 / 01897 Sec。 371日期1997年3月19日 102(e)日期1997年3月19日PCT 1995年9月20日提交了一种矫直钛或钛合金线材的方法,其中将杆在矫直温度T下热矫直至直杆,伸长率ε满足表达式 (1)或(2)。 该方法包括将钛钛合金(α+β)钛合金或近α钛合金热轧成线材,将热轧线材卷绕成线圈,冷拔线材,切割线材 杆,以获得弯曲的线材,将弯曲的线材加热至矫直温度T,同时弯曲线材的两个端部都固定,向线材施加预定的伸长率ε,保持矫直温度T,热矫直 根据表达式(2)ε(T-400)> / = 400(1)ε(T-500)> / = 200(2),并施加张力来冷却线材。 该方法适用于制备用于发动机气门的直杆。

    Method of soldering honeycomb body
    6.
    发明授权
    Method of soldering honeycomb body 失效
    蜂窝体焊接方法

    公开(公告)号:US5082167A

    公开(公告)日:1992-01-21

    申请号:US583331

    申请日:1990-09-17

    IPC分类号: B23K1/00

    CPC分类号: B23K1/0014

    摘要: When soldering a honeycomb body formed by alternately piling flat foils (plates) and corrugated foils (plates), a binder liquid is sucked up from the end face of the honeycomb body to form a binder streak in a space defined by contacting portions of the flat foil (plate) and corrugated foil (plate), a solder is scattered and applied onto the binder streak, and the honeycomb body is then dried and heated to effect a soldering of the honeycomb body. According to this method, soldering can be accomplished only in the vicinity of the contacting portions of the flat foil (plate) and corrugated foil (plate), with a desired soldering structure.

    摘要翻译: 当焊接通过交替打桩扁平箔(板)和波纹箔(板)形成的蜂窝体时,粘合剂液体从蜂窝体的端面被吸出,以在由平坦部分接触的部分限定的空间中形成粘合剂条纹 箔(板)和波纹箔(板),焊料被散射并施加到粘合剂条纹上,然后将蜂窝体干燥并加热以实现蜂窝体的焊接。 根据该方法,只能在平板(板)和波纹箔(板)的接触部分附近具有期望的焊接结构。