摘要:
A suction puncture device includes a puncture needle having an outer tube that has an opening edge of a first front end formed in the shape of a blade, and a stopper member that has a second front end disposed within the outer tube at a position separated from the first front end of the outer tube by a predetermined distance. A sample containing portion is formed between the second front end of the stopper member and the first front end of the outer tube. A ventilation passage is formed around the stopper member within the outer tube, a suction unit is connected to a first base end side of the outer tube, and the suction unit is communicated with and connected to the sample containing portion via the ventilation passage.
摘要:
A finish for acrylic fiber to be processed into carbon fiber includes an ester compound having at least three ester groups in its molecule and a silicone compound, wherein the silicone compound constitutes 10 to 50 weight percent of the whole of the nonvolatile matter of the finish. A method of manufacturing carbon fiber includes the processes of applying the finish for acrylic fiber to be processed into carbon fiber to acrylic fiber to be processed into carbon fiber; oxidative-stabilizing the finish-applied acrylic fiber in an oxidizing atmosphere at 200 to 300 deg. C. to convert the fiber into oxidized fiber; and carbonizing the oxidized fiber in an inert atmosphere at 200 to 3000 deg. C.
摘要:
A finish for acrylic fiber to be processed into carbon fiber includes an ester compound having at least three ester groups in its molecule and a silicone compound, wherein the silicone compound constitutes 10 to 50 weight percent of the whole of the nonvolatile matter of the finish. A method of manufacturing carbon fiber includes the processes of applying the finish for acrylic fiber to be processed into carbon fiber to acrylic fiber to be processed into carbon fiber; oxidative-stabilizing the finish-applied acrylic fiber in an oxidizing atmosphere at 200 to 300 deg. C. to convert the fiber into oxidized fiber; and carbonizing the oxidized fiber in an inert atmosphere at 200 to 3000 deg. C.