Process for producing compact silicon nitride ceramics
    1.
    发明授权
    Process for producing compact silicon nitride ceramics 失效
    生产紧凑型氮化硅陶瓷的方法

    公开(公告)号:US4205033A

    公开(公告)日:1980-05-27

    申请号:US935416

    申请日:1978-08-22

    摘要: A process for producing a compact silicon nitride ceramic product which comprises molding a powder mixture of Si.sub.3 N.sub.4, Ta.sub.2 O.sub.5 and Al.sub.2 O.sub.3 in proportions defined by the region A, B, C, D in the FIGURE within the ranges of 65.0 to 96.0% by volume Si.sub.3 N.sub.4, 1.0 to 32.0% by volume Ta.sub.2 O.sub.5 and 3.0 to 20.0% by volume Al.sub.2 O.sub.3, and then firing the powder mixture in a non-oxidizing atmosphere containing a carbon compound; or hot-pressing the powder mixture; in a graphite mold.

    摘要翻译: 一种制造紧凑型氮化硅陶瓷产品的方法,其包括在图中的区域A,B,C,D定义的范围内,以65.0至96.0体积%Si 3 N 4的范围模制Si 3 N 4,Ta 2 O 5和Al 2 O 3的粉末混合物, 1.0〜32.0体积%的Ta 2 O 5和3.0〜20.0体积%的Al 2 O 3,然后在含有碳化合物的非氧化性气氛中烧成粉末混合物; 或热压粉末混合物; 在石墨模具中。

    Ceramics spike pin
    2.
    发明授权
    Ceramics spike pin 失效
    陶瓷钉针

    公开(公告)号:US4993174A

    公开(公告)日:1991-02-19

    申请号:US511429

    申请日:1990-04-23

    IPC分类号: A43B13/26 A43C15/00 A43C15/02

    CPC分类号: A43C15/005

    摘要: A ceramics spike pin is provided with a pin body having a horizontal cross section of a substantially circular shape, which pin body is provided with a rounded free end portion having a predetermined radius of curvature and a connecting base portion having a predetermined radius of curvature, and a horizontally expanded base connected to the connecting base portion, wherein a diameter (d) of the connecting base portion in horizontal cross section, the radius of curvature(r) of the connecting base portion, and a maximum diagonal length (D) of the horizontally expanded base satisfy the relationship of 0

    摘要翻译: 陶瓷尖钉设置有具有大致圆形形状的水平截面的销体,该销体设置有具有预定曲率半径的圆形自由端部和具有预定曲率半径的连接基部, 以及与所述连接基部连接的水平膨胀基部,其中,所述连接基部的水平截面的直径(d),所述连接基部的曲率半径(r)和所述连接基部的最大对角线长度(D) 水平扩展的基座满足0 / = 1.36之间的关系。 因此,可以大大减轻应力集中,提高耐冲击性,从而提高耐久性。

    Process for the production of silicon nitride sintered bodies
    3.
    发明授权
    Process for the production of silicon nitride sintered bodies 失效
    制造氮化硅烧结体的方法

    公开(公告)号:US4521358A

    公开(公告)日:1985-06-04

    申请号:US521283

    申请日:1983-08-08

    摘要: Processes for the production of a silicon nitride sintered body are disclosed. One process comprises molding a mixed powder of 100 parts by weight of metallic silicon with a maximum particle size of 20 .mu.m or less and 0.2 to 2 parts by weight (calculated as chromium oxide) of a chromium component and, thereafter, reaction sintering the mold in a nitrogen gas or in a non-oxidizing atmosphere containing nitrogen gas at a temperature of 1,300.degree. to 1,500.degree. C. This invention provides further process which comprises molding a mixed powder of 100 parts by weight of metallic silicon with a maximum particle size of 20 .mu.m or less, 0.2 to 1 part by weight (calculated as chromium oxide) of a chromium component, and further 10 to 20 parts by weight of an oxide component of one or more of the oxides of yttrium, lanthanum, cerium, gadolinium, and erbium, reaction sintering the above-prepared mold, and thereafter, hot pressing the reaction sintered body. This silicon nitride hot pressed body is superior in oxidation resistance, and moreover is of high density and has high mechanical strength. Thus it is suitable for use as, e.g., gas turbine parts of diesel engine parts.

    摘要翻译: 公开了制造氮化硅烧结体的方法。 一种方法包括:将100重量份最大粒度为20μm或更小的金属硅和0.2至2重量份(以铬氧化物计)的铬组分的混合粉末模塑,然后将 在氮气中或在含有氮气的非氧化性气氛中在1300〜1500℃的温度下成型。本发明提供了进一步的方法,其包括将最大粒径为100重量份的金属硅的混合粉末 20μm以下,0.2〜1重量份(以氧化铬计算)的铬成分,还含有10〜20重量份的氧化物成分,一种或多种钇,镧,铈, 钆和铒,对上述制备的模具进行反应烧结,然后热压该反应烧结体。 该氮化硅热压体的耐氧化性优异,而且密度高,机械强度高。 因此,它适用于例如柴油发动机部件的燃气轮机部件。

    Ceramic bearing and metal shaft assembly
    4.
    发明授权
    Ceramic bearing and metal shaft assembly 失效
    陶瓷轴承和金属轴组件

    公开(公告)号:US4997296A

    公开(公告)日:1991-03-05

    申请号:US513859

    申请日:1990-04-24

    摘要: A bearing includes an inner ring made of ceramics. A shaft is made of metal and fitted in the inner ring. The ceramics has a tensile strength equal to or larger than 50 Kg/mm.sup.2, and the ceramics and the metal are determined so as to satisfy the relation of .beta..sub.2 -.beta..sub.1 .ltoreq.6.times.10.sup.-6 /.degree.C. where .beta..sub.1 is a coefficient of linear expansion of the ceramics and .beta..sub.2 is a coefficient of linear expansion of the metal.

    摘要翻译: 轴承包括由陶瓷制成的内圈。 轴由金属制成并安装在内圈中。 陶瓷具有等于或大于50Kg / mm2的拉伸强度,并且确定陶瓷和金属以满足β2-β1≤6×10 -6 /℃的关系,其中β1是 陶瓷的线膨胀系数和β2是金属的线性膨胀系数。

    Composition for animals
    8.
    发明授权
    Composition for animals 失效
    动物组成

    公开(公告)号:US4743591A

    公开(公告)日:1988-05-10

    申请号:US946664

    申请日:1986-12-24

    CPC分类号: A61K31/495 A61K31/65

    摘要: Disclosed is a composition for treatment or prevention of diseases of animals or for addition to feeds for acceleration of growth which contains a mycinamicin antibiotic and at least one compound selected from the group consisting of a quinoxaline-di-N-oxide and a tetracycline antibiotic as effective ingredients. Administration of this composition affords excellent synergistic effects in antibacterial action and good body weight gaining effect and growth accelerating effect.

    摘要翻译: 公开了用于治疗或预防动物疾病或加入含有霉菌素抗生素和至少一种选自喹喔啉二-N-氧化物和四环素抗生素的化合物的生长加料的组合物, 有效成分。 该组合物的施用在抗菌作用和良好的体重增加效果和生长促进作用方面具有优异的协同作用。

    Process for producing silicon nitride sintered products having high
toughness
    9.
    发明授权
    Process for producing silicon nitride sintered products having high toughness 失效
    具有高韧性的氮化硅烧结体的制造方法

    公开(公告)号:US4440707A

    公开(公告)日:1984-04-03

    申请号:US428507

    申请日:1982-09-29

    CPC分类号: C04B35/593 C04B35/584

    摘要: A process for producing a silicon nitride sintered product having high toughness is described, comprising blending from 97 to 57% by weight of metallic silicon powder having a maximum particle size of 25 .mu.m or less with from 1 to 15% by weight, calculated as TiN, of a TiN powder having a maximum particle size of 20 .mu.m or less or a powder of titanium component capable of changing into TiN during reaction sintering, and from 2 to 28% by weight of one or more components selected from the group consisting of AlN, Al.sub.2 O.sub.3, SiO.sub.2 and oxides of rare earth elements, molding the resulting mixture, carrying out reaction sintering in a nonoxidizing atmosphere of a nitrogen gas or a nitrogen-containing mixed gas, and thereafter resintering in the same atmosphere at a temperature of from 1,600.degree. C. to 2,200.degree. C.

    摘要翻译: 描述了一种制造具有高韧性的氮化硅烧结产品的方法,其包括将97至57重量%的最大粒度为25μm或更小的金属硅粉末与1至15重量%混合,计算为 TiN,其具有最大粒度为20μm以下的TiN粉末或能够在反应烧结时变为TiN的钛成分的粉末,以及2〜28重量%的选自以下的组分中的一种或多种: 的AlN,Al2O3,SiO2和稀土元素的氧化物,将所得混合物成型,在氮气或含氮混合气体的非氧化气氛中进行反应烧结,然后在相同的气氛中在 1600〜2200℃