公开(公告)号:US08858909B2
公开(公告)日:2014-10-14
申请号:US13376564
申请日:2010-05-28
申请人: Yoshinori Sato , Kazuyuki Tohji , Masaru Namura
发明人: Yoshinori Sato , Kazuyuki Tohji , Masaru Namura
CPC分类号: C01B31/0233 , B01J19/088 , B01J2219/0809 , B01J2219/0815 , B01J2219/0822 , B01J2219/083 , B01J2219/0839 , B01J2219/0871 , B01J2219/0892 , B82Y30/00 , B82Y40/00 , C01B32/16 , C01B32/162 , C01B32/17 , C01B2202/20 , Y10S977/742 , Y10S977/75 , Y10S977/844
摘要: There is provided a high-purity carbon nanotube, which can be produced with simple purification by causing graphite to be hardly contained in crude soot obtained immediately after being synthesized by arc-discharge, and a method for producing the same. Soot containing carbon nanotubes produced by arc-discharge using an anode which contains amorphous carbon as a main component is heated at a temperature of not lower than 350° C. to be burned and oxidized, immersed in an acid, heated at a temperature, which is not lower than the heating temperature in the previous burning and oxidation and which is not lower than 500° C., to be burned and oxidized, and immersed in an acid again.
摘要翻译: 提供一种高纯度碳纳米管及其制造方法,该碳纳米管可以通过在通过电弧放电合成后立即获得的粗煤烟中几乎不含石墨而简单地进行纯化。 使用含有非晶质碳作为主要成分的阳极通过电弧放电产生的含碳纳米管的碳素纳米管在不低于350℃的温度下加热,被烧成和氧化,浸入酸中,加热温度为 不低于先前燃烧和氧化中的加热温度,不低于500℃,待燃烧和氧化,并再次浸入酸中。
-
公开(公告)号:US20120083408A1
公开(公告)日:2012-04-05
申请号:US13376564
申请日:2010-05-28
申请人: Yoshinori Sato , Kazuyuki Tohji , Masaru Namura
发明人: Yoshinori Sato , Kazuyuki Tohji , Masaru Namura
CPC分类号: C01B31/0233 , B01J19/088 , B01J2219/0809 , B01J2219/0815 , B01J2219/0822 , B01J2219/083 , B01J2219/0839 , B01J2219/0871 , B01J2219/0892 , B82Y30/00 , B82Y40/00 , C01B32/16 , C01B32/162 , C01B32/17 , C01B2202/20 , Y10S977/742 , Y10S977/75 , Y10S977/844
摘要: There is provided a high-purity carbon nanotube, which can be produced with simple purification by causing graphite to be hardly contained in crude soot obtained immediately after being synthesized by arc-discharge, and a method for producing the same. Soot containing carbon nanotubes produced by arc-discharge using an anode which contains amorphous carbon as a main component is heated at a temperature of not lower than 350° C. to be burned and oxidized, immersed in an acid, heated at a temperature, which is not lower than the heating temperature in the previous burning and oxidation and which is not lower than 500° C., to be burned and oxidized, and immersed in an acid again.
摘要翻译: 提供一种高纯度碳纳米管及其制造方法,该碳纳米管可以通过在通过电弧放电合成后立即获得的粗煤烟中几乎不含石墨而简单地进行纯化。 使用含有非晶质碳作为主要成分的阳极通过电弧放电产生的含碳纳米管的碳素纳米管在不低于350℃的温度下加热,被烧成和氧化,浸入酸中,加热温度为 不低于先前燃烧和氧化中的加热温度,不低于500℃,待燃烧和氧化,并再次浸入酸中。
-