公开(公告)号:US4399089A
公开(公告)日:1983-08-16
申请号:US337745
申请日:1982-01-07
申请人: Yoshio Mohri , Tsutomu Ikeda , Takashi Hiroishi , Kinzi Sano , Yasuhiro Yamamoto , Yuji Yamamoto , Ryoji Nakashima
发明人: Yoshio Mohri , Tsutomu Ikeda , Takashi Hiroishi , Kinzi Sano , Yasuhiro Yamamoto , Yuji Yamamoto , Ryoji Nakashima
IPC分类号: D05B71/00 , B32B18/00 , B41J2/335 , C03C3/091 , C03C8/02 , C04B41/50 , C04B41/86 , H05K1/03 , H05K3/02 , F27B21/00
CPC分类号: C04B41/009 , C04B41/5022 , C04B41/86 , H05K1/0306 , H05K3/022
摘要: A method of producing a glazed ceramic substrate, which is useful for a hybrid integrated circuit or a thermal head of a thermal printer for instance, by applying a glass onto a major surface of a ceramic substrate, firing the substrate to form a molten glass layer on the substrate surface and cooling the fired substrate. To obtain the glazed ceramic substrate with high flatness despite the tendency of the substrate to warp due to difference in thermal expansion coefficient between the ceramic and the glass, a refractory base which supports the substrate during the firing and cooling steps is so shaped as to allow the substrate to deform during the firing step reversely to the expected warp at the cooling step, so that the warp at the cooling step is offset by the preceding deformation. For example, the upper surface of the base is shaped into a continuous and concave surface. As a modification, suitably shaped rib-like or pillar-like spacers are arranged on the top face of a flat base plate with intervals therebetween.
摘要翻译: 一种制造玻璃陶瓷基板的方法,其可用于混合集成电路或热敏打印机的热敏头,例如通过在陶瓷基板的主表面上施加玻璃,烧制基板以形成熔融玻璃层 在基板表面上并冷却烧制的基板。 为了获得陶瓷和玻璃之间的热膨胀系数的差异,由于陶瓷和玻璃之间的热膨胀系数的差异,由于基板的翘曲倾向,所以能够获得具有高平坦度的玻璃陶瓷基板,在烧成和冷却工序中支承基板的耐火基材的形状为允许 基板在烧制步骤期间与在冷却步骤期间的预期翘曲相反地变形,使得冷却步骤的翘曲被前面的变形抵消。 例如,基部的上表面被成形为连续且凹入的表面。 作为修改,在平坦基板的顶面上布置适当形状的肋状或柱状间隔件,间隔。
-
公开(公告)号:US4396682A
公开(公告)日:1983-08-02
申请号:US333402
申请日:1981-12-22
申请人: Yoshio Mohri , Tsutomu Ikeda , Takashi Hiroishi , Kinzi Sano , Yasuhiro Yamamoto , Yuji Yamamoto , Ryoji Nakashima
发明人: Yoshio Mohri , Tsutomu Ikeda , Takashi Hiroishi , Kinzi Sano , Yasuhiro Yamamoto , Yuji Yamamoto , Ryoji Nakashima
IPC分类号: H05K1/03 , B41J2/335 , C03C3/087 , C03C8/02 , C03C8/08 , C03C8/12 , C04B41/86 , H01L23/15 , B32B9/00
CPC分类号: C03C8/12 , C03C3/087 , C03C8/02 , C03C8/08 , H05K1/0306
摘要: A glazed ceramic substrate for use in electric or electronic devices, obtained by forming a glass coating layer directly on a major surface of a ceramic substrate such as an alumina substrate. The glass as the material of the coating layer contains 50-60 Wt % of SiO.sub.2, 10-30 Wt % of Al.sub.2 O.sub.3, 15-30 Wt % of CaO and MgO, and 2-6 Wt % of ZrO.sub.2 as essential components, optionally with the addition of small amount(s) of at least one of TiO.sub.2, BaO, ZnO, PbO, P.sub.2 O.sub.5, B.sub.2 O.sub.3, Na.sub.2 O and K.sub.2 O. The coating layer formed of this glass is excellent in its high-temperature stability, so that the glazed ceramic substrate is particularly suitable for use in thermal heads of thermal printing devices.
摘要翻译: 一种用于电气或电子设备的玻璃陶瓷基板,其通过在诸如氧化铝基板的陶瓷基板的主表面上直接形成玻璃涂层而获得。 作为涂层材料的玻璃含有50-60重量%的SiO 2,10-30重量%的Al 2 O 3,15-30重量%的CaO和MgO,以及2-6重量%的ZrO 2作为必需成分, 添加少量的TiO 2,BaO,ZnO,PbO,P 2 O 5,B 2 O 3,Na 2 O和K 2 O中的至少一种。 由该玻璃形成的涂层的高温稳定性优异,因此特别适用于热敏打印装置的热敏头。
-