摘要:
A copolymer having monomer units derived from ethylene and monomer units derived from an α-olefin of 3 to 20 carbon atoms, a density of 906 to 970 kg/m3 and an activation energy of flow of 50 kJ/mol or more, and satisfying specific relations among a melt complex viscosity, a melt flow rate and a characteristic relaxation time.
摘要翻译:具有衍生自乙烯的单体单元和衍生自3至20个碳原子的α-烯烃的单体单元,密度为906至970kg / m 3的共聚物和50kJ的流动活化能 / mol以上,并且满足熔体复数粘度,熔体流动速率和特征弛豫时间之间的特定关系。
摘要:
An ethylene-α-olefin copolymer having monomer units derived from ethylene and monomer units derived from an α-olefin of 3 to 20 carbon atoms, a density of 906 to 970 kg/m3, an activation energy of flow of 50 kJ/mol or more and a heat quantity of fusion of a cold xylene soluble part of 30 J/g or more, and satisfying specific relations among a rate of the cold xylene soluble part in the copolymer, the density, a melt flow rate and a characteristic relaxation time.
摘要翻译:具有衍生自乙烯的单体单元和衍生自3-20个碳原子的α-烯烃的单体单元,密度为906至970kg / m 3的乙烯-α-烯烃共聚物,活化能 的流动为50kJ / mol以上,冷二甲苯可溶部分的熔融热量为30J / g以上,满足共聚物中冷二甲苯可溶部分的比例,密度,a 熔体流动速率和特征弛豫时间。
摘要:
An ethylene-α-olefin copolymer having monomer units derived from ethylene and monomer units derived from an α-olefin of 3 to 20 carbon atoms, a density of 906 to 970 kg/m3, an activation energy of flow of 50 kJ/mol or more and a heat quantity of fusion of a cold xylene soluble part of 30 J/g or more, and satisfying specific relations among a rate of the cold xylene soluble part in the copolymer, the density, a melt flow rate and a characteristic relaxation time.
摘要翻译:具有衍生自乙烯的单体单元和衍生自3-20个碳原子的α-烯烃的单体单元,密度为906至970kg / m 3的乙烯-α-烯烃共聚物,活化能 的流动为50kJ / mol以上,冷二甲苯可溶部分的熔融热量为30J / g以上,满足共聚物中冷二甲苯可溶部分的比例,密度,a 熔体流动速率和特征弛豫时间。
摘要:
A copolymer having monomer units derived from ethylene and monomer units derived from an α-olefin of 3 to 20 carbon atoms, a density of 906 to 970 kg/m3 and an activation energy of flow of 50 kJ/mol or more, and satisfying specific relations among a melt complex viscosity, a melt flow rate and a characteristic relaxation time.
摘要翻译:具有衍生自乙烯的单体单元和衍生自3至20个碳原子的α-烯烃的单体单元,密度为906至970kg / m 3的共聚物和50kJ的流动活化能 / mol以上,并且满足熔体复数粘度,熔体流动速率和特征弛豫时间之间的特定关系。
摘要:
A resin composition wherein the content of the following component (i) is 99 to 30 wt % and the content of the following component (ii) is 1 to 70 wt %, a pressurized foaming molded body of the resin composition, and a laminate obtained by laminating a layer composed of the pressure-foamed molding and a layer composed of another material: (i) an ethylene-a-olefin-based copolymer comprising an ethylene monomer unit and an a-olefin monomer unit having 3 to 20 carbon atoms wherein the melt flow rate is 0.01 to 5 g/10 minutes and the activation energy for flow is 30 kJ/mol or more, (ii) an ethylene-unsaturated ester-based copolymer comprising an unsaturated ester monomer unit and an ethylene monomer unit.
摘要:
A resin composition for pressure-foam molding, which comprises an ethylene-based copolymer and a foaming agent, wherein the ethylene-based copolymer has monomer units derived from ethylene and monomer units derived from an a-olefin having 3 to 20 carbon atoms, has a melt flow rate of 0.01 to 0.7 g/10 minutes, a molecular weight distribution of 5 or more determined by a gel permeation chromatography, an activation energy of flow of 40 kJ/mol or more, and inflection points of 3 or less on a melting curve within temperature range from 25° C. to the end point of melting obtained by a differential scanning calorimetry; a foam obtained by press foaming; and a process for producing the foam.
摘要:
A resin composition for pressure-foam molding, which comprises an ethylene-based copolymer and a foaming agent, wherein the ethylene-based copolymer has monomer units derived from ethylene and monomer units derived from an a-olefin having 3 to 20 carbon atoms, has a melt flow rate of 0.01 to 0.7 g/10 minutes, a molecular weight distribution of 5 or more determined by a gel permeation chromatography, an activation energy of flow of 40 kJ/mol or more, and inflection points of 3 or less on a melting curve within temperature range from 25° C. to the end point of melting obtained by a differential scanning calorimetry; a foam obtained by press foaming; and a process for producing the foam.
摘要:
An ethylene-α-olefin copolymer having monomer units derived from ethylene and monomer units derived from an α-olefin of 3 to 20 carbon atoms, a melt flow rate (MFR) of 0.01 to 4 g/10 minutes, a density of 890 to 970 kg/m3, an activation energy of flow of 50 kJ/mol or more and a molecular weight distribution measured by gel permeation chromatography of 3 or more, wherein a characteristic relaxation time (τ) determined by a melt viscoelasticity measurement or an external haze ratio (EHR) satisfies a relationship of the following formula (1) or (2), respectively: 3×MFR−0.75+1.1>τ>1.3×MFR−0.5+1.4 (1) EHR≦−15×log MFR+0.145×d−47 (2)
摘要:
An ethylene-α-olefin copolymer containing monomer units derived from ethylene and monomer units derived from an α-olefin having 4 to 20 carbon atoms, and having a density of 890 to 970 kg/m3, an activation energy of flow of 50 kJ/mol or more, a molecular weight distribution of 3 or more determined by a gel permeation chromatography, and the number of inflection points of 3 or less on a melting curve obtained by a differential scanning calorimetry within a temperatures ranges of from 25°C. to an end point of melting.
摘要翻译:含有源自乙烯的单体单元和衍生自碳原子数4〜20的α-烯烃,密度为890〜970kg / m 3的乙烯-α-烯烃共聚物,流动的活化能为50kJ / mol以上,通过凝胶渗透色谱法测定的分子量分布为3以上,通过差示扫描量热法在25℃的温度范围内获得的熔解曲线上的拐点数为3以下。 到熔化的终点。
摘要:
An ethylene-α-olefin copolymer containing monomer units derived from ethylene and monomer units derived from an α-olefin having 4 to 20 carbon atoms, and having a density of 890 to 970 kg/m3, an activation energy of flow of 50 kJ/mol or more, a molecular weight distribution of 3 or more determined by a gel permeation chromatography, and the number of inflection points of 3 or less on a melting curve obtained by a differential scanning calorimetry within a temperatures range of from 25° C. to an end point of melting.
摘要翻译:包含衍生自乙烯的单体单元和衍生自碳原子数4〜20的α-烯烃,密度为890〜970kg / m 3的单体单元的乙烯-α-烯烃共聚物, 通过凝胶渗透色谱法测定的流动活化能为50kJ / mol以上,分子量分布为3以上,通过差示扫描量热法在温度下得到的熔解曲线上的拐点数为3以下 范围为25°C至熔点终点。