公开(公告)号:US20060289351A1
公开(公告)日:2006-12-28
申请号:US11167067
申请日:2005-06-24
申请人: Zhili Xiao , Yurong Han , Hsien-Hau Wang , Gerold Willing , Ulrich Welp , Wai-Kwong Kwok
发明人: Zhili Xiao , Yurong Han , Hsien-Hau Wang , Gerold Willing , Ulrich Welp , Wai-Kwong Kwok
IPC分类号: B01D71/02
CPC分类号: B01D71/021 , B01D67/0062 , B01D67/0065 , B01D67/0067 , B01D71/022 , B01D2323/24 , B01D2325/10 , B01D2325/26 , B01J23/681 , B01J37/0226 , B82Y30/00 , B82Y40/00 , C01B3/505 , C01B32/162 , C01B2202/08 , C01B2202/34 , C01B2202/36 , C01P2004/13 , G01N33/005 , Y10T428/31678
摘要: This invention provides ways to fabricate nanotubes and nanobead arrays by utilizing nanopores in anodic aluminum oxide (AAO) membranes. Nanotubes of bismuth and other low melting point metals with controlled diameters and lengths can be fabricated by sintering AAO coated with appropriate metals at temperatures above their melting points. Carbon nanotubes may also be readily formed by carbonizing a polymer on the interior walls of the nanopores in AAO membranes. Palladium nanobead arrays which can be used as ultrafast hydrogen sensors are fabricated by coating the flat surface of AAO membranes with controlled pore-wall ratios.
摘要翻译: 本发明提供了通过在阳极氧化铝(AAO)膜中利用纳米孔来制造纳米管和纳米管阵列的方法。 具有受控直径和长度的铋和其他低熔点金属的纳米管可以通过在高于其熔点的温度下烧结用合适的金属涂覆的AAO来制造。 也可以通过在AAO膜中的纳米孔的内壁上碳化聚合物来容易地形成碳纳米管。 可用作超快氢传感器的钯纳米管阵列通过以可控的孔壁比例涂覆AAO膜的平坦表面来制造。