摘要:
A method for manufacturing a glass wafer for augmented reality applications includes the steps of: providing the raw wafer; edge-grinding of the raw wafer; lapping the raw wafer; rough polishing the raw wafer; fine polishing the raw wafer to obtain an intermediate wafer; gluing the intermediate wafer on a flat carrier; performing single-side polishing of a first main side of the intermediate wafer; and performing single-side polishing of a second main side of the intermediate wafer.
摘要:
Provided is an X-ray shielding glass having high shielding capability against X-rays with a tube voltage of 150 kV or less. The X-ray shielding glass has a composition including: 15 mass % to 25 mass % B2O3; 7 mass % to 50 mass % La2O3; 7 mass % to 50 mass % Gd2O3; 10 mass % to 25 mass % WO3; 0 mass % to 7 mass % SiO2; 0 mass % to 10 mass % ZrO2; 0 mass % to 8 mass % Nb2O5; 0 mass % to 10 mass % Ta2O5; 0 mass % to 5 mass % Bi2O3; 0 mass % to 3 mass % CeO2; and 0 mass % to 1 mass % Sb2O3, wherein the glass contains no ZnO, the total content of La2O3 and Gd2O3 is 45 mass % to 65 mass %, and when the thickness of the glass is 3 mm, the transmittance of the glass to an X-ray from an X-ray tube with a tube voltage of 60 kV is 0.0050% or less, and the transmittance of the glass to an X-ray from an X-ray tube with a tube voltage of 100 kV is 0.1500% or less.
摘要:
To provide an optical glass having the optical characteristics of a high refractive index and low dispersion, and moreover, which makes it possible to further reduce devitrification and which can be stably obtained, and a preform and an optical element using the same. The optical glass comprises, expressed in cation % (mol %), 17.0% to 42.0% of P5+, 7.0% to 30.0% of Al3+, more than 0% to 22.0% of Mg2+, more than 0% to 25.0% Ca2+, more than 0% to 30.0% of Sr2+, more than 0% to 35.0% Ba2+, and expressed in anion % (mol %), a content ratio of F− of 37.0 to 64.0%, a content ratio of O2− of 36.0 to 63.0%, a refractive index (nd) of 1.48 to 1.58, and having an Abbe number (vd) of 70 to 88, and a liquidus temperature of 800° C. or less.
摘要:
A high refraction low dispersion optical glass, the components thereof including, by weight percentage: B2O3: 1-30%; SiO2: 0-20%; La2O3: 25-55%; Gd2O3: 5-40%; Y2O3: 0-25%; Yb2O3: 0-10%; Ta2O5: 0-10%; Nb2O5: 1-30%; TiO2: 0-10%; ZrO2: 0.5-20%; WO3: 0-10%; ZnO: 0-15%; R2O: 0-10%; RO: 0-10%; Al2O3: 0-10%; GeO2: 0-10%; Bi2O3: 0-10%. A high refraction low dispersion environmentally friendly optical glass having excellent light transmittance may be obtained by reducing the Ta2O5 content within the glass components and introducing suitable amounts of rare earth oxide components having a high refraction low dispersion effect.
摘要:
A high refraction low dispersion optical glass having a refractive index of 1.86-1.92 and an Abbe number of 36-42. The components of the optical glass comprise, by weight percentage: B2O3: 1-30%; SiO2: 0-20%; La2O3: 25-55%; Gd2O3: 5-40%; Y2O3: 0-25%; Yb2O3: 0-10%; Ta2O5: 0-10%; Nb2O5: 1-30%; TiO2: 0-10%; ZrO2: 0.5-20%; WO3: 0-10%; ZnO: 0-15%; Al2O3: 0-10%; GeO2: 0-10%; Bi2O3: 0-10%. The optical glass does not contain PbO or F. A high refraction low dispersion optical glass having excellent light transmittance may be obtained by introducing suitable amounts of rare earth oxides having a high refraction low dispersion effect and optimizing the proportions of said components.
摘要:
An aspect of the present invention relates to optical glass, which is oxide glass comprising various cationic components in prescribed amounts without Pb, with a refractive index nd of 1.750 to 1.850, an Abbé number νd of 29.0 to 40.0, and a glass transition temperature of less than 630° C.
摘要:
Provided is an optical glass which can satisfy all of the following requirements: (1) it contains no environmentally undesirable components; (2) it can easily achieve a low glass transition point; (3) it has a high refractive index and high dispersion; (4) it can easily provide a glass having a superior visible light transmittance; and (5) it has superior resistance to devitrification during preparation of a preform. The optical glass has a refractive index nd of 2.0 or more, an Abbe's number νd of 20 or less, a glass transition point of 450° C. or below, and a glass composition, in % by mass, of 70 to 90% Bi2O2, 4 to 29.9% B2O2, 0.1 to 10% Li2O+Na2O+K2O, and 0 to 2.5% SiO2+Al2O2 and is substantially free of lead component, arsenic component, F component, TeO2, and GeO2.
摘要翻译:提供可以满足以下所有要求的光学玻璃:(1)不含有环境不良成分; (2)可以轻松实现低玻璃化转变点; (3)折射率高,色散高; (4)可以容易地提供具有优异的可见光透射率的玻璃; 和(5)在制备预成型品时具有优异的抗失透性。 光学玻璃的折射率nd为2.0以上,阿贝数n为20以下,玻璃化转变温度为450℃以下,玻璃组合物的质量%为70〜90 4%〜29.9%的B 2 O 2,0.1〜10%的Li 2 O + Na 2 O + K 2 O,0〜2.5%的SiO 2 + Al 2 O 2,并且基本上不含铅成分,砷成分,F成分,TeO 2和GeO 2。
摘要:
The present invention relates to an optical glass having a refractive index nd of 1.86 or higher and an Abbé number v(nu)d of 28 to 36; a preform for precision press molding and an optical element that are comprised of this glass; and a method for manufacturing the optical element.
摘要:
An optical glass having a refractive index nd of 1.70 or greater and an Abbé number of 50 or greater. Given as mole percentages, it comprises: B2O3 (20 to 80 percent), SiO2 (0 to 30 percent), Li2O (1 to 25 percent), ZnO (0 to 20 percent), La2O3 (4 to 30 percent), Gd2O3 (1 to 25 percent), Y2O3 (0 to 20 percent), ZrO2 (0 to 5 percent), MgO (0 to 25 percent), CaO (0 to 15 percent), and SrO (0 to 10 percent), with the combined quantity of the above components being 97 percent or greater. The molar ratio of {ZnO/(La2O3+Gd2O3+Y2O3)} is 0.8 or less and the molar ratio of {(CaO+SrO+BaO)/(La2O3+Gd2O3+Y2O3)} is 0.8 or less. Ta2O5 may be incorporated as an optional component, with the molar ratio {(ZrO2+Ta2O5)/(La2O3+Gd2O3+Y2O3)} being 0.4 or less.
摘要翻译:折射率nd为1.70以上,Abbé数为50以上的光学玻璃。 以百分比计,B2O3(20-80%),SiO2(0-30%),Li2O(1%至25%),ZnO(0-20%),La2O3(4-30%),Gd2O3 1〜25%),Y2O3(0〜20%),ZrO2(0〜5%),MgO(0〜25%),CaO(0〜15%)和SrO(0〜10% 上述成分的量为97%以上。 {ZnO /(La 2 O 3 + Gd 2 O 3 + Y 2 O 3)}的摩尔比为0.8以下,{(CaO + SrO + BaO)/(La2O3 + Gd2O3 + Y2O3)}的摩尔比为0.8以下。 Ta2O5可以以((ZrO 2 + Ta 2 O 5)/(La 2 O 3 + Gd 2 O 3 + Y 2 O 3)}的摩尔比为0.4以下的任意成分结合。
摘要:
Provided is an optical glass having optical constants, a refractive index (nd) of more than 1.9 and an Abbe number (νd) of not more than 38, having a small partial dispersion ratio and capable of being produced from inexpensive materials. The optical glass has a partial dispersion ratio (θg, F) of at most 0.615, and contains, as indispensable ingredients, B2O3, La2O3, TiO2, Nb2O5 and Ta2O5, wherein the ratio, as % by mass, of TiO2/Nb2O5 is at most 0.26 and GeO2/Nb2O5 is at most 0.38. The optical glass contains, in terms of % by mass, the following ingredients: B2O3 5 to 22%, La2O3 15 to 50%, TiO20.01 to 15%, Nb2O5 5 to 40%, and Ta2O5 0.1 to 25%, and SiO20 to 10% and/or GeO20 to 10% and/or Al2O30 to 10% and/or Gd2O30 to 16% and/or ZrO20 to 15% and/or WO30 to 22% and/or Sb2O30 to 1%.
摘要翻译:提供具有光学常数,大于1.9的折射率(nd)和不大于38的阿贝数(&ngr; d)的光学玻璃,其具有小的分散比并且能够由廉价的材料制成。 光学玻璃具有至多0.615的部分分散比(& g,F),并且含有作为不可缺少的成分的B 2 O 3,La 2 O 3,TiO 2,Nb 2 O 5和Ta 2 O 5,其中以质量%计的TiO 2 / Nb 2 O 5 为0.26以下,GeO 2 / Nb 2 O 5为0.38以下。 光学玻璃以质量%计含有B 2 O 5 5〜22%,La 2 O 3 15〜50%,TiO 2 0.01〜15%,Nb 2 O 5 5〜40%,Ta 2 O 5 0.1〜25%,SiO 2 0 至10%和/或GeO 0至10%和/或Al 2 O 3 0至10%和/或Gd 2 O 3 0至16%和/或ZrO 2 0至15%和/或WO 3 0至22%和/或Sb 2 O 3 0至1 %。