摘要:
Disclosed is a novel, high molecular weight aliphatic polyester having excellent mechanical strengths such as breaking strain and containing a copolymer structure with 3-alkoxy-1,2-propane diol and a method of producing the aliphatic polyester in an industrially advantageous manner. The aliphatic polyester is a biodegradable high molecular weight aliphatic polyester having an ester structure derived from 3-alkoxy-1,2-propane diol.
摘要:
A copolyether composition that can be used to produce a dyeable polyester is provided. The composition can comprise repeat units derived from a first diol such as, for example, 1,3-propanediol and a sulfonated dicarboxylic acid such as, for example, 5-sulfo-isophthalic acid. The dyeable polyester composition can comprise repeat units derived from the copolyether composition, an acid such as, for example, terephthalic acid, and a second diol such as, for example, 1,3-propanediol. Also disclosed is a process that can be used for producing the copolyether composition. The process comprises contacting the first diol with the sulfonated dicarboxylic acid. Further disclosed is a process that can be used for producing the dyeable composition in which the process comprises (1) contacting, in the presence of a catalyst, the copolyether composition with a diol such as, for example, 1,3-propanediol, and a dicarboxylic ester such as, for example, dimethylterephthalate or (2) contacting an acid such as for example, terephthalic acid and a diol such as, for example, 1,3-propanediol to produce an intermediate and thereafter contacting the intermediate with the copolyether.
摘要:
A resin composite characterized in that it includes: a polymer compound which is an alternating copolymer of a saccharic compound and an aliphatic compound and has a three-dimensional network; and a plasticizer contained in the gap in the three-dimensional network of the above polymer compound, the production of the resin composite contributing to making good use of waste vegetable resources, such as used paper and waste molasses, as raw materials, the resin composite having elasticity and flexibility just as does rubber.
摘要:
Polyesters suitable as plasticizers and obtainable by reacting aliphatic dicarboxylic acids, neopentyl glycol, at least one other diol and a nonanol mixture, where the nonanol mixture is mainly composed of 1-nonanol, of monomethyloctanols, of dimethylheptanols and of monoethylheptanols. The nonanol mixture is also described, as is the use of the plasticizers.
摘要:
This invention relates to a water-soluble fiber and a method of manufacturing the fiber. The water-soluble fiber of the invention is composed of a high molecular compound with a weight average molecular weight of not less than 10,000, which high molecular compound is obtainable by reacting a polyalkylene oxide compound, which is obtainable by addition polymerization of an ethylene oxide-containing alkylene oxide and an organic compound containing two active hydrogen atoms, with a polycarboxylic acid, an anhydride thereof, a lower alkyl ester thereof, or a diisocyanate and is manufactured by spinning the same high molecular compound. The water-soluble fiber of the invention is not only high in elongation and tensile strength but is readily soluble in water.
摘要:
The invention relates to a process for making a high molecular weight pre-gel for a cross-linked branched polyester comprising: a) reacting polyester precursor repeat units via condensation polymerization in a continuous or semi-continuous, or batch reactor stage to form a low molecular weight pre-gel; and b) further reacting the low molecular weight pre-gel via condensation polymerization in a continuous thin-film reactive vacuum processing stage to form a high molecular weight pre-gel.
摘要:
The present invention is a method of preparing a high molecular weight copolyester bottle resin that has excellent melt processing characteristics. The method includes the steps of reacting a diacid or diester component and a diol component to form modified polyethylene terephthalate, wherein diol component is present in excess of stoichiometric proportions. Together, the diacid or diester component and the diol component must include at least 7 percent comonomer. The remainder of the diacid component is terephthalic acid or dimethyl terephthalate and the remainder of the diol component is ethylene glycol. The modified polyethylene terephthalate is copolymerized in the melt phase to an intrinsic viscosity of between about 0.25 dl/g and 0.40 dl/g to thereby form a copolyester prepolymer. Thereafter the copolyester prepolymer is polymerized in the solid phase to form a high molecular weight bottle resin that has an intrinsic viscosity of at least about 0.70 dl/g, and a solid phase density of less than 1.413 g/cc.
摘要:
Polyether polyol having the following chemical formula (1): HO—(AO)mZO—(BO)n—H, which is suitable for the manufacture of polyester, polyurethane elastomer and polyurethane paint showing an excellent hydrolysis resistance is disclosed. In this formula, Z is a dimer diol residue; A and B are the same or different alkylene groups having 2-4 carbon atoms; and m and n are the same or different integers of 0 or more where 2≦(m+n)≦40. Also disclosed is a method for the manufacture of mouldable polyester containing the above-mentioned polyether polyol as one of the constituting units.