HEATING METHOD AND HEATING APPARATUS
    1.
    发明申请
    HEATING METHOD AND HEATING APPARATUS 审中-公开
    加热方法和加热装置

    公开(公告)号:WO1998038344A1

    公开(公告)日:1998-09-03

    申请号:PCT/JP1997004610

    申请日:1997-12-15

    IPC分类号: C21D01/52

    摘要: First regenerators (3A-3C) which are in combustion exhaust gas exhaust passages, second regenerators (4A-4C) which are in suction/recovery passages for sucking and recovering N2, an atmospheric gas, are provided to three or more regenerative heaters (1A-1C), respectively. In one (1C) of the regenerative heaters (1A-1C), the sucked N2 atmospheric gas is passed through the second regenerator (4C) to regenerate its sensible heat. In another one (1A), combustion air is passed through the second regenerator (4A) in which the heat is stored and combustion is carried out by using the heated air. Only the combustion exhaust gas is passed through the first regenerator (3A) for regeneration. In the other one (1B), the N2 atmospheric gas is passed through the first regenerators (3A-3C) in which heat is regenerated to convert the regenerated heat into sensible heat, which is supplied to the atmosphere of an object and heats the object. These processes, i.e. combustion, atmospheric gas heating and atmospheric gas suction, are repeated in this order. Thus, the atmospheric gas is recovered and reused, and the sensible heat of the atmospheric gas is converted into the sensible heat of the combustion air to improve the heat efficiency.

    摘要翻译: 在三个以上的再生加热器(1A)中设置有处于燃烧废气排气通路中的第一再生器(3A-3C),用于吸入和回收N2的吸入/回收通道中的第二再生器(4A-4C) -1C)。 在再生加热器(1A-1C)的一个(1C)中,吸入的N 2大气气体通过第二再生器(4C)以再生其显热。 在另一个(1A)中,燃烧的空气通过第二再生器(4A),其中存储热量并通过使用加热的空气进行燃烧。 只有燃烧废气通过第一再生器(3A)才能再生。 在另一个(1B)中,N2气体通过第一再生器(3A-3C),其中再生热量以将再生热转化成显热,其被供应到物体的气氛并加热物体 。 这些过程,即燃烧,大气气体加热和大气吸入,按此顺序重复。 因此,大气中的气体被回收再利用,大气中的显热转化为燃烧空气的显热,提高了热效率。

    HOT DIP GALVANIZED STEEL SHEET REDUCED IN DEFECTS DERIVED FROM FAILED PLATING AND EXCELLENT IN CONTACT PLATING ADHESION AND PROCESS FOR PRODUCING THE SAME
    2.
    发明申请
    HOT DIP GALVANIZED STEEL SHEET REDUCED IN DEFECTS DERIVED FROM FAILED PLATING AND EXCELLENT IN CONTACT PLATING ADHESION AND PROCESS FOR PRODUCING THE SAME 审中-公开
    热镀锌钢板在由于失败的镀层导致的缺陷中降低,并且接触层压粘合剂和其生产方法

    公开(公告)号:WO1998030729A1

    公开(公告)日:1998-07-16

    申请号:PCT/JP1997000045

    申请日:1997-01-13

    IPC分类号: C23C02/00

    摘要: A hot dip galvanized steel sheet for use as steel sheets for automobiles, an alloyed hot dip galvanized steel sheet, and a process for producing the same. The galvanized steel sheet is reduced in the defects derived from failed plating and excellent in contact plating adhesion, and is characterized by having oxides of elements, more oxidizable than iron just under the plating, the oxides being formed during hot rolling. According to the production process, the temperature of coiling at the time of hot rolling is 600 DEG C or above, the cooling is carried out at a low rate, and the oxides are left intact also in the subsequent steps.

    摘要翻译: 用作汽车用钢板的热浸镀锌钢板,合金化热浸镀锌钢板及其制造方法。 镀锌钢板由于电镀失败而导致的缺陷减少,接触电镀附着性优异,其特征在于,具有比正在电镀下的铁更可氧化的元素氧化物,在热轧时形成氧化物。 根据制造方法,热轧时的卷取温度为600℃以上,冷却以低速进行,氧化物也在后续工序中保持完好。

    PLUG AND MANDREL BAR FOR ROLLING OF SEAMLESS STEEL PIPE AND METHOD OF MANUFACTURING SEAMLESS STEEL PIPE
    3.
    发明申请
    PLUG AND MANDREL BAR FOR ROLLING OF SEAMLESS STEEL PIPE AND METHOD OF MANUFACTURING SEAMLESS STEEL PIPE 审中-公开
    无缝钢管轧制棒和棒材及其制造无缝钢管的方法

    公开(公告)号:WO1998029204A1

    公开(公告)日:1998-07-09

    申请号:PCT/JP1997004741

    申请日:1997-12-22

    IPC分类号: B21B25/00

    CPC分类号: B21B25/00

    摘要: The lives of a plug and mandrel bar for seamless steel pipe rolling which are subjected to severe operation conditions such as a high temperature and a heavy load are significantly improved. At least the surface layers of the plug and the mandrel bar or the surface layers of the tip parts and the work parts of the plug and the mandrel bar are made of ceramic. A method of manufacturing a seamless steel pipe which employs such plug and mandrel bar is also provided.

    摘要翻译: 用于无缝钢管轧制的插头和芯棒的寿命显着改善,其经受诸如高温和重负荷的严苛操作条件。 插头和芯棒的至少表面层或尖端部分的表面层以及插塞和芯棒的工作部分由陶瓷制成。 还提供了一种使用这种插头和芯棒的无缝钢管的制造方法。

    LONG GLASS FIBER-REINFORCED CONDUCTIVE THERMOPLASTIC RESIN MOLDING AND PROCESS FOR PREPARING THE SAME
    4.
    发明申请
    LONG GLASS FIBER-REINFORCED CONDUCTIVE THERMOPLASTIC RESIN MOLDING AND PROCESS FOR PREPARING THE SAME 审中-公开
    长玻璃纤维增​​强导电热塑性树脂模塑及其制备方法

    公开(公告)号:WO1998021281A1

    公开(公告)日:1998-05-22

    申请号:PCT/JP1997004137

    申请日:1997-11-13

    IPC分类号: C08L101/00

    摘要: A thermoplastic resin molding having both electrical conductivity and high strength and comprising 5 to 60 % by weight of glass fibers having a length of not less than 0.4 mm and at least one conductive material in an amount satisfying formula (1), wherein Wk represents the content (wt.%) of the conductive material, Ek represents the volume resistivity ( OMEGA .cm) of each conductive material, and n represents the number of kinds of the conductive material. The process for preparing the above thermoplastic resin molding comprises molding a thermoplastic resin which contains 10 to 90 % by weight of glass fibers having a weight average fiber length of not less than 1 mm and which is substantially impregnated among the glass fibers and at least one conductive material under or after mixing.

    摘要翻译: 具有导电性和高强度的热塑性树脂成型体,其含有5〜60重量%的长度不小于0.4mm的玻璃纤维和至少一种满足式(1)的量的导电材料,其中Wk表示 导电材料的含量(重量%)Ek表示导电材料的体积电阻率(OMEGA·cm),n表示导电材料的种类数。 制备上述热塑性树脂模制品的方法包括将含有10至90重量%的重均纤维长度不小于1mm并且基本上浸渍在玻璃纤维中的玻璃纤维和至少一种 混合之前或之后的导电材料。

    HOT ROLLING ROLL EXCELLENT IN ABRASION RESISTANCE AND REDUCED IN SEGREGATION OF CARBIDE
    5.
    发明申请
    HOT ROLLING ROLL EXCELLENT IN ABRASION RESISTANCE AND REDUCED IN SEGREGATION OF CARBIDE 审中-公开
    耐磨耐磨性好,耐磨性好的热轧辊

    公开(公告)号:WO1997048505A1

    公开(公告)日:1997-12-24

    申请号:PCT/JP1997002062

    申请日:1997-06-16

    IPC分类号: B21B27/00

    CPC分类号: B21B27/00 B32B15/011

    摘要: A high-performance, hot-rolling, high-speed steel roll which possesses excellent abrasion resistance and, at the same time, when produced by an economically advantageous centrifugal casting method, does not cause segregation of any carbide. The hot rolling roll has an outer layer comprising, on a weight basis, C: 2.4 to 2.9 %, Si: not more than 1 %, Mn: not more than 1 %, Cr: 12 to 18 %, Mo: 3 to 9 %, V: 3 to 8 %, and Nb: 0.5 to 4 %, the above constituents simultaneously satisfying requirements represented by the following formulae: (1) 0.27

    摘要翻译: 具有优异的耐磨性,同时通过经济上有利的离心铸造方法制造的高性能,热轧,高速钢辊不会引起任何碳化物的偏析。 该热轧辊的外层的重量为C:2.4〜2.9%,Si:1%以下,Mn:1%以下,Cr:12〜18%,Mo:3〜9 %,V:3〜8%,Nb:0.5〜4%,上述成分同时满足下式所示的要求:(1)0.27

    LONG-FIBERGLASS REINFORCED POLYOLEFIN MOLDINGS IMPROVED IN WEATHERING RESISTANCE AND COMPOSITIONS USEFUL AS THE RAW MATERIAL THEREFOR
    6.
    发明申请
    LONG-FIBERGLASS REINFORCED POLYOLEFIN MOLDINGS IMPROVED IN WEATHERING RESISTANCE AND COMPOSITIONS USEFUL AS THE RAW MATERIAL THEREFOR 审中-公开
    长纤维增强的耐候性和组合物增强的聚烯烃模具作为原材料有用

    公开(公告)号:WO1997024399A1

    公开(公告)日:1997-07-10

    申请号:PCT/JP1996003786

    申请日:1996-12-25

    IPC分类号: C08L23/00

    CPC分类号: C08K5/005 C08K7/14 C08L23/02

    摘要: The long-fiberglass reinforced polyolefin moldings according to the prior art were poor in weathering resistance, though excellent in mechanical strengths. They were also liable to lower in the mechanical characteristics when they contained colorants. The present invention provides long-fiberglass reinforced polyolefin moldings excellent in both weathering resistance and mechanical strengths, compositons useful as the raw material therefor, and further moldings which are not impaired in either of the above properties even when they are colored and compositions useful as the raw material therefor. Specifically, the compositions at least comprise (A) long-fiberglass reinforced polyolefin pellets which are produced by impregnating a glass fiber roving with a polyolefin and cutting the resulting roving in lengths of 2 to 150 mm and have a fiberglass content of 10 to 90 wt.% and wherein the glass fibers contained are arranged in a length substantially equal to that of the pellet, (B) a light stabilizer and (C) a light absorber, and are characterized in that the total amount of the components (B) and (C) is 0.25 to 7.5 parts by weight per 100 parts by weight of the whole polyolefin; and long-fiberglass reinforced polyolefin moldings at least comprising (a) a polyolefin, (b) a fiberglass having a fiber length of 2 to 150 mm, (B) a light stabilizer and (C) a light absorber, characterized in that the total amount of the component (B) and (C) is 0.25 to 7.5 parts by weight per 100 parts by weight of the whole polyolefin and that the fiberglass content is 10 to 90 wt.%. The above moldings can keep both of the above properties at high levels even when colored black with carbon black or gray with carbon black and zinc sulfide, as far as the colorant(s) is added at a specific ratio to the above additives.

    摘要翻译: 根据现有技术的长玻璃纤维增​​强聚烯烃模制品的耐候性差,尽管机械强度优异。 当它们含有着色剂时,它们也容易降低其机械特性。 本发明提供耐候性和机械强度优异的长玻璃纤维增​​强聚烯烃成型品,作为其原料的组合物,以及即使在着色时也不损害上述性能的其它成型品,以及可用作为 原材料。 具体地,组合物至少包含(A)长纤维增强聚烯烃粒料,其通过浸渍用聚烯烃粗纱的玻璃纤维并将所得粗纱切割成2至150mm长度并且玻璃纤维含量为10至90wt %,并且其中所含的玻璃纤维的长度基本上等于颗粒的长度,(B)光稳定剂和(C)光吸收剂,其特征在于组分(B)和 (C)相对于100重量份整个聚烯烃为0.25〜7.5重量份; 和长纤维增强聚烯烃模制品,其至少包含(a)聚烯烃,(b)纤维长度为2至150mm的玻璃纤维,(B)光稳定剂和(C)光吸收剂,其特征在于, 组分(B)和(C)的量相对于全部聚烯烃为100重量份为0.25〜7.5重量份,玻璃纤维含量为10〜90重量%。 上述成型品即使在炭黑或炭黑和硫化锌处于灰色时,也能保持上述性能的高水平,只要以上述添加剂的比例添加着色剂即可。

    IRON POWDER FOR POWDER METALLURGY, PROCESS FOR PRODUCING THE SAME, AND IRON-BASE POWDER MIXTURE FOR POWDER METALLURGY
    7.
    发明申请
    IRON POWDER FOR POWDER METALLURGY, PROCESS FOR PRODUCING THE SAME, AND IRON-BASE POWDER MIXTURE FOR POWDER METALLURGY 审中-公开
    用于粉末冶金的铁粉,其生产方法和用于粉末冶金的铁基粉末混合物

    公开(公告)号:WO1997014523A1

    公开(公告)日:1997-04-24

    申请号:PCT/JP1996003007

    申请日:1996-10-17

    IPC分类号: B22F01/00

    CPC分类号: C22C33/0264

    摘要: Iron powder and iron-base powder mixture for powder metallurgy, which can provide sinters excellent in machinability and wear resistance. The iron powder contains 0.03-0.3 wt.% boron, at most 0.07 wt.% chromium, less than 0.3 wt.% manganese, and the balance consisting of iron and unavoidable impurities, and has an intensity ratio of boron to iron of at least 0.05 in the spectrum of the powder surface as determined by Auger electron spectroscopy. The powder serves to increase the amount of graphite remaining in sinters to thereby improve the machinability and wear resistance thereof. Another iron powder is prepared by adding sulfur, selenium, tellurium, molybdenum or the like to the above powder. These powders are mixed with MoO3 or WO3 powder to develop a so-called iron-base powder mixture. It is produced by water-atomizing the above powders while adjusting the oxygen content of molten steel to 100 ppm or below.

    摘要翻译: 用于粉末冶金的铁粉和铁基粉末混合物,可提供优异的机械加工性和耐磨性的烧结体。 铁粉含有0.03-0.3重量%的硼,至多0.07重量%的铬,小于0.3重量%的锰,余量由铁和不可避免的杂质组成,并且硼与铁的强度比至少为 在通过俄歇电子能谱法测定的粉末表面的光谱中为0.05。 粉末用于增加烧结体中残留的石墨的量,从而提高其机械加工性和耐磨性。 通过向上述粉末中加入硫,硒,碲,钼等制备另一种铁粉。 将这些粉末与MoO 3或WO 3粉末混合以形成所谓的铁基粉末混合物。 通过在将钢水的氧含量调节至100ppm以下的同时对上述粉末进行水雾化而制造。

    NETWORK INTERCONNECTING DEVICE
    8.
    发明申请
    NETWORK INTERCONNECTING DEVICE 审中-公开
    网络互连设备

    公开(公告)号:WO1997013345A1

    公开(公告)日:1997-04-10

    申请号:PCT/JP1996002873

    申请日:1996-10-03

    IPC分类号: H04L12/46

    摘要: A network interconnecting device has two stages, a mask processing section (10) and a transmission control information generating section (30). The mask processing section (10) generates an address mask for extracting various kinds of address components from the destination address (IP) contained in a received message in accordance with the address (IP). Therefore, the extraction of various kinds of address components such as the network address and sub-network address is simplified.

    摘要翻译: 网络互连设备具有两个阶段,即掩模处理部分(10)和传输控制信息产生部分(30)。 掩模处理部(10)根据地址(IP)生成从接收到的消息中包含的目的地地址(IP)中提取各种地址分量的地址掩码。 因此,简化了诸如网络地址和子网地址的各种地址组件的提取。

    METHOD OF ROLLING DEFORMED BAR AND ROLL FOR DEFORMED BAR
    9.
    发明申请
    METHOD OF ROLLING DEFORMED BAR AND ROLL FOR DEFORMED BAR 审中-公开
    轧制变形钢筋和轧辊的方法

    公开(公告)号:WO1997011796A1

    公开(公告)日:1997-04-03

    申请号:PCT/JP1996002783

    申请日:1996-09-26

    IPC分类号: B21B27/02

    CPC分类号: B21B1/163 B21B27/02

    摘要: A deformed bar having knots and four ribs on its surface is produced by performing the final finish rolling by means of a two-roll rolling mill. Rolls R1, R2 of the two-roll rolling mill have a peripheral groove (3), knot grooves (2) and a bottom groove (1). The peripheral groove (3) is substantially semi-circular in cross section, and is provided over the whole peripheral surface of the roll. The knot grooves (2) are made in the groove surfaces of the peripheral groove (3) and have a predetermined width so as to cross the peripheral groove (3). The cross section of the bottom groove (1) is an isosceles trapezoid and the groove (1) is provided along the center line of the peripheral groove (3) over the whole circumference of the peripheral groove.

    摘要翻译: 通过使用双辊轧机进行最终精轧,制造具有节点的变形杆和其表面上的四个肋。 双辊轧机的轧辊R1,R2具有周向槽(3),结槽(2)和底槽(1)。 周边槽(3)的横截面为大致半圆形,设在辊的整个周面上。 结槽(2)形成在周缘槽(3)的沟槽表面中,并且具有预定的宽度以与周边槽(3)交叉。 底槽(1)的横截面为等腰梯形,并且沿着周缘槽的整个周边沿着周向槽(3)的中心线设置槽(1)。

    CLADDING MATERIAL FOR CENTRIFUGAL CASTING ROLL
    10.
    发明申请
    CLADDING MATERIAL FOR CENTRIFUGAL CASTING ROLL 审中-公开
    离心铸造辊用粘合材料

    公开(公告)号:WO1996027688A1

    公开(公告)日:1996-09-12

    申请号:PCT/JP1996000544

    申请日:1996-03-06

    IPC分类号: C22C37/06

    CPC分类号: C22C37/06 B21B27/00

    摘要: A cladding material for centrifugal casting rolls which contains 2.5-4.7 % C, 0.8-3.2 % Si, 0.1-2.0 % Mn, 0.4-1.9 % Cr, 0.6-5 % Mo, 3.0-10.0 % V, and 0.6-7.0 % Nb, these elements satisfying the following relationships (1) to (4): (1) 2.0 + 0.15V + 0.10Nb

    摘要翻译: 一种用于离心铸造辊的包覆材料,其包含2.5-4.7%C,0.8-3.2%Si,0.1-2.0%Mn,0.4-1.9%Cr,0.6-5%Mo,3.0-10.0%V和0.6-7.0% Nb,这些元素满足以下关系式(1)〜(4):(1)2.0 + 0.15V + 0.10Nb