An article in the form of one of a plate, a sheet, a cylinder, and a portion of a cylinder, which is adapted for use as at least a portion of a wear resistant working surface of a roll is disclosed. The article includes a metal matrix composite comprising a plurality of inorganic particles dispersed in a matrix material. The matrix material includes at least one of a metal and a metal alloy, wherein the melting temperature of the inorganic particles is greater than the melting temperature of the matrix material. A plurality of hard elements are embedded in the metal matrix composite. The wear resistance of the metal matrix composite is less than the wear resistance of the hard elements, and the metal matrix composite preferentially wears away when the article is in use, thereby providing or preserving gaps between each of the plurality of hard elements at a working surface of the article.
Abstract:
An article includes a working portion including cemented carbide, and a heat sink portion in thermal communication with the working portion. The heat sink portion includes a heat sink material having a thermal conductivity greater than a thermal conductivity of the cemented carbide. Also disclosed are methods of making an article including a working portion comprising cemented carbide, and a heat sink portion in thermal communication with the working portion and including a heat sink material having a thermal conductivity that is greater than a thermal conductivity of the cemented carbide. The heat sink portion conducts heat from the working portion.
Abstract:
Embodiments of the present invention include methods of producing a composite article. A method comprises introducing a first powdered metal grade from a feed shoe into a first portion of a cavity in a die and a second powdered metal grade from the feed shoe into a second portion of the cavity, wherein the first powder metal grade differs from the second powdered metal grade in chemical composition or particle size. Further methods are also provided. Embodiments of the present invention also comprise composite inserts for material removal operations. The composite inserts may comprise a first region and a second region, wherein the first region comprises a first composite material and the second region comprises a second composite material.
Abstract:
The present invention relates to compositions and methods for forming a bit body for an earth-boring bit. The bit body may comprise hard particles, wherein the hard particles comprise at least one carbide, nitride, boride, and oxide and solid solutions thereof, and a binder binding together the hard particles. The binder may comprise at least one metal selected from cobalt, nickel, and iron, and, optionally, at least one melting point reducing constituent selected from a transition metal carbide in the range of (30) to (60) weight percent, boron up to (10) weight percent, silicon up to (20) weight percent, chromium up to (20) weight percent, and manganese up to (25) weight percent, wherein the weight percentages are based on the total weight of the binder. In addition, the hard particles may comprise at least one of (i) cast carbide (WC + W2C) particles, (ii) transition metal carbide particles selected from the carbides of titanium, chromium, vanadium, zirconium, hafnium, tantalum, molybdenum, niobium, and tungsten, and (iii) sintered cemented carbide particles.
Abstract:
Methods for forming a wear resistant layer metallurgically bonded to at least a portion of a surface of a metallic substrate may generally comprise positioning hard particles adjacent the surface of the metallic substrate, and infiltrating the hard particles with a metallic binder material to form a wear resistant layer metallurgically bonded to the surface. In certain embodiments of the method, the infiltration temperature may be 50C to 100C greater than a liquidus temperature of the metallic binder material. The wear resistant layer may be formed on, for example, an exterior surface and/or an interior surface of the metallic substrate. Related wear resistant layers and articles of manufacture are also described.
Abstract:
An article in the form of one of a plate, a sheet, a cylinder, and a portion of a cylinder, which is adapted for use as at least a portion of a wear resistant working surface of a roll is disclosed. The article includes a metal matrix composite comprising a plurality of inorganic particles dispersed in a matrix material. The matrix material includes at least one of a metal and a metal alloy, wherein the melting temperature of the inorganic particles is greater than the melting temperature of the matrix material. A plurality of hard elements are embedded in the metal matrix composite. The wear resistance of the metal matrix composite is less than the wear resistance of the hard elements, and the metal matrix composite preferentially wears away when the article is in use, thereby providing or preserving gaps between each of the plurality of hard elements at a working surface of the article.
Abstract:
A thread rolling die (10) includes a thread rolling region (12) comprising a working surface (14) including a thread form (16). The thread rolling region (12) of the thread rolling die (10) comprises a sintered cemented carbide material having a hardness in the range of 78 HRA to 89 HRA. In certain embodiments, the thread rolling die (10) may further include at least one non-cemented carbide piece (18) metallurgically bonded to the thread rolling region (12) in an area of the thread rolling region that does not prevent a workpiece from contacting the working surface, and wherein the non-cemented carbide piece (18) comprises at least one of a metallic region and a metal matrix composite region.
Abstract:
An article of manufacture includes a cemented carbide piece7 and a joining phase that binds the cemented carbide piece into the article. The joining phase includes inorganic particles and a matrix material. The matrix material is a metal and a metallic alloy. The melting temperature of the inorganic particles is higher than the melting temperature of the matrix material. A method includes infiltrating the space between the inorganic particles and the cemented carbide piece with a molten metal or metal alloy followed by solidification of the metal or metal alloy to form an article of manufacture.
Abstract:
A macroscopic composite sintered powder metal article including a first region including cemented hard particles, for example, cemented carbide. The article includes a second region including one of a metal and a metallic alloy selected from the group consisting of a steel, nickel, a nickel alloy, titanium, a titanium alloy, molybdenum, a molybdenum alloy, cobalt, a cobalt alloy, tungsten, and a tungsten alloy. The first region is metallurgically bonded to the second region, and the second region has a thickness of greater than 100 microns. A method of making a macroscopic composite sintered powder metal article is also disclosed, herein. The method includes co-press and sintering a first metal powder including hard particles and a powder binder and a second metal powder including the metal or metal alloy.
Abstract:
Embodiments of the present invention include composite articles comprising at least a first region and a second region and methods of making such articles. The first region may comprise a first composite material, wherein the first region comprises less than 5 wt. % cubic carbides by weight, and the second region may comprise a second composite material, wherein the second composite material differs from the first composite material in at least one characteristic. The composite article may additionally comprise at least one coolant channel. In certain embodiments, the first and second composite material may individually comprise hard particles in a binder, wherein the hard particles independently comprise at least one of a carbide, a nitride, aboride, a silicide, an oxide, and solid solutions thereof and the binder comprises at least one metal selected from cobalt, nickel, iron and alloys thereof. In specific embodiments, the first composite material and the second composite material may individually comprise metal carbides in a binder, such as a cemented carbide.