公开(公告)号:WO2021108207A1
公开(公告)日:2021-06-03
申请号:PCT/US2020/061228
申请日:2020-11-19
Applicant: CORNING INCORPORATED
Inventor: BRONFENBRENNER, David Jack , LEHMAN, Michael James
Abstract: Improved extrusion dies are described herein for manufacturing a honeycomb body structure (330) from honeycomb extrudate (104). An improved extrusion die (102) comprises a swell relief feature in a discharge slot (218) of the extrusion die (102) that is disposed upstream of a discharge surface (214) of the extrusion die (102). The swell relief feature comprises a change in the width (W) of the discharge slot (218).
-
公开(公告)号:WO2017095916A1
公开(公告)日:2017-06-08
申请号:PCT/US2016/064205
申请日:2016-11-30
Applicant: CORNING INCORPORATED
Inventor: BRONFENBRENNER, David Jack , LEHMAN, Michael James , LEWIS, Mark Alan , MURRAY, Pamela Jeanne , SHANLEY, Deborah Lynn
IPC: C04B35/185 , C04B35/195 , C04B35/478 , C04B35/636 , C04B38/00
CPC classification number: C04B35/636 , C04B35/185 , C04B35/195 , C04B35/478 , C04B35/6365 , C04B38/0006 , C04B2111/00793 , C04B2111/0081 , C04B2235/6021 , C04B2235/9607 , C04B2235/9615 , C04B2103/0079 , C04B2103/42
Abstract: Methods for making ceramic articles, and methods for reducing extrusion pressure during processes of making ceramic articles, are disclosed. The methods include mixing a ceramic batch composition comprising amylose and amylopectin in an amylose:amylopectin ratio ranging from about 30:70 to about 95:5, and extruding the ceramic batch composition through an extrusion die to form an extruded green ceramic article.
Abstract translation: 公开了制造陶瓷制品的方法以及在制造陶瓷制品的过程中降低挤压压力的方法。 所述方法包括混合包含直链淀粉:支链淀粉比率为约30:70至约95:5的直链淀粉和支链淀粉的陶瓷批料组合物,并且将陶瓷批料组合物通过挤出模具挤出以形成挤出生坯陶瓷制品。 p>
-
公开(公告)号:WO2015013351A1
公开(公告)日:2015-01-29
申请号:PCT/US2014/047720
申请日:2014-07-23
Applicant: CORNING INCORPORATED
IPC: C04B35/478 , C04B35/626 , C04B38/00
CPC classification number: C04B35/478 , B29D24/005 , C04B35/64 , C04B38/0006 , C04B2111/00793 , C04B2111/0081 , C04B2235/3206 , C04B2235/3217 , C04B2235/3234 , C04B2235/3445 , C04B2235/6562 , C04B2235/6584 , C04B2235/661 , C04B2235/94 , C04B38/068
Abstract: A method for firing a green honeycomb ceramic body including heating the green honeycomb ceramic body from room temperature to a first temperature of less than or equal to about 350°C with at least one heating rate of greater than or equal to about 80°C/hr. The green honeycomb ceramic body may be heated from the first temperature to a second temperature of greater than or equal to about 800°C at a heating rate of greater than or equal to about 90°C/hr. The green honeycomb ceramic body may be heated from the second temperature to a third temperature of greater than or equal to about 1000°C. The green honeycomb ceramic body may include aluminum raw materials for forming an aluminum titanate ceramic body.
Abstract translation: 一种焙烧生坯蜂窝陶瓷体的方法,包括将生坯蜂窝陶瓷体从室温加热至小于或等于约350℃的第一温度,至少一个加热速率大于或等于约80℃/ 小时。 绿色蜂窝陶瓷体可以以大于或等于约90℃/小时的加热速率从第一温度加热至大于或等于约800℃的第二温度。 绿色蜂窝陶瓷体可以从第二温度加热到大于或等于约1000℃的第三温度。 绿色蜂窝陶瓷体可以包括用于形成钛酸铝陶瓷体的铝原料。
-
公开(公告)号:WO2014138015A1
公开(公告)日:2014-09-12
申请号:PCT/US2014/020202
申请日:2014-03-04
Applicant: CORNING INCORPORATED , BEALL, Douglas Munroe , BRONFENBRENNER, David Jack , FABER, Margaret Kathleen , IYER, Sriram Rangarajan , TEPESCH, Patrick David , WING, Douglas Richard
Inventor: BEALL, Douglas Munroe , BRONFENBRENNER, David Jack , FABER, Margaret Kathleen , IYER, Sriram Rangarajan , TEPESCH, Patrick David , WING, Douglas Richard
IPC: C04B35/195 , C04B38/00
CPC classification number: C04B38/0006 , C04B35/195 , C04B38/0038 , C04B2111/343 , C04B2235/6562 , C04B2235/6567 , C04B2235/6584 , C04B2235/6588 , C04B2235/9607 , C04B38/0074 , C04B38/068
Abstract: A method for firing a green honeycomb ceramic body in a kiln may include heating the green honeycomb ceramic body in four stages. The first stage may include heating the green honeycomb ceramic body from room temperature to a first temperature that at a first heating rate that is greater than or equal to about 75 o C/hr. The second stage may include heating the green honeycomb ceramic body from the first temperature to a second temperature at a second heating rate that is less than or equal to the first heating rate. The third stage may include heating the green honeycomb ceramic body from the second temperature to a hold temperature at a third heating rate that is less than or equal to the first heating rate. The fourth stage may include holding the green honeycomb ceramic body at the hold temperature to remove residual carbon.
Abstract translation: 在窑炉中焙烧绿色蜂窝陶瓷体的方法可以包括以四个阶段加热绿色蜂窝陶瓷体。 第一阶段可以包括将生坯蜂窝陶瓷体从室温加热到第一温度,其以大于或等于约75℃/小时的第一加热速率。 第二阶段可以包括以小于或等于第一加热速率的第二加热速率将生坯蜂窝陶瓷体从第一温度加热到第二温度。 第三阶段可以包括以小于或等于第一加热速率的第三加热速率将生坯蜂窝陶瓷体从第二温度加热到保持温度。 第四阶段可以包括将生坯蜂窝陶瓷体保持在保持温度以除去残留的碳。
-
-
-