1.
公开(公告)号:WO2015179199A1
公开(公告)日:2015-11-26
申请号:PCT/US2015/030722
申请日:2015-05-14
Applicant: GEORGIA-PACIFIC LLC
Inventor: TOPPING, Paul , SEN, Subrata
IPC: C02F11/10
CPC classification number: B01D3/00 , B01J20/02 , B01J20/041 , B01J20/10 , B01J20/103 , B01J20/16 , B01J20/20 , B01J20/3078 , B01J2220/4887 , C02F11/06 , C02F11/121 , C02F2103/28 , C10B53/07 , C10B57/06 , C10G1/10 , D21B1/026 , F23G7/001 , F23G2206/201 , F23G2209/12 , Y02E20/363 , Y02P20/143 , Y02W10/40
Abstract: Methods are provided for reuse of a sludge from a waste fiber supply including an organic fraction and an inorganic fraction. Generally, methods include converting the sludge by burning the sludge to remove a majority of the organic fraction and produce an ash with inorganic materials in an amount of at least about 80% by weight of the ash and adding the ash to a plastic pyrolysis system in an effective amount to remove at least a portion of one or more contaminants from a plastic feed stream of the plastic pyrolysis system. Integrated recycling systems also are provided and include a fiber recovery system; a means for at least partially dewatering a sludge; a burner; and a pyrolyzer.
Abstract translation: 提供了用于重新利用来自包括有机部分和无机部分的废弃纤维供应品的污泥的方法。 通常,方法包括通过燃烧污泥来转移污泥以除去大部分有机部分,并且以灰分的至少约80重量%的量用无机材料产生灰分,并将灰分添加到塑料热解系统中 有效量从塑料热解系统的塑料进料流中除去至少一部分一种或多种污染物。 还提供了综合回收系统,包括纤维回收系统; 用于至少部分地使污泥脱水的方法; 燃烧器 和热解器。
-
公开(公告)号:WO2016149300A1
公开(公告)日:2016-09-22
申请号:PCT/US2016/022539
申请日:2016-03-16
Applicant: GEORGIA-PACIFIC LLC
Inventor: CARROLL, Michael E. , KROON, Johannes A. , PARTON, Rudy F. M. J. , SEN, Subrata , WOESTENBORGHS, Pierre L.
Abstract: Methods and systems are provided for improved liquefaction of a lignocellulosic biomass. The methods include reacting a lignocellulosic biomass slurry at mild conditions for a short period to produce a first reaction mixture having a reduced viscosity as compared to the lignocellulosic biomass slurry and that is substantially free of levulinic acid and hydroxymethylfurfural. The methods further include separating the first reaction mixture into a solid fraction and a liquid fraction, the solid fraction having a majority of lignin from the lignocellulosic biomass slurry and the liquid fraction having a majority of hemicellulose and greater than about 30% by weight of cellulose from the lignocellulosic biomass slurry. The method advantageously prevents or eliminates the formation of tar and/or char.
Abstract translation: 提供了用于改善木质纤维素生物质液化的方法和系统。 所述方法包括使木质纤维素生物质浆料在温和条件下短时间反应以产生与木质纤维素生物质浆料相比具有降低的粘度并且基本上不含乙酰丙酸和羟甲基糠醛的第一反应混合物。 所述方法还包括将第一反应混合物分离成固体部分和液体部分,固体部分具有来自木质纤维素生物质浆料的大部分木质素和具有大多数半纤维素的液体部分和大于约30重量%的纤维素 来自木质纤维素生物质浆料。 该方法有利地防止或消除焦油和/或焦炭的形成。
-