GLASS-BASED ARTICLES WITH ENGINEERED STRESS PROFILES AND METHODS OF MANUFACTURE
    2.
    发明申请
    GLASS-BASED ARTICLES WITH ENGINEERED STRESS PROFILES AND METHODS OF MANUFACTURE 审中-公开
    具有工程应力特征的玻璃基制品和制造方法

    公开(公告)号:WO2018063966A1

    公开(公告)日:2018-04-05

    申请号:PCT/US2017/053198

    申请日:2017-09-25

    IPC分类号: C03C17/23 C03C21/00 C03C17/22

    摘要: Strengthened glass-based substrates having a first outer region compressive stress and a first side having first coating thereon are disclosed. The first coating comprising a material selected to have a first coating Young's modulus value, a first coating thickness, and a first coating stress that is either neutral or compressive, such that the absolute value of first outer region compressive stress is greater than the absolute value of the first coating stress. Methods of making glass-based articles are provided, and glass-based articles having coatings that provide different strength values and/or reliability on different sides of the glass-based articles are also disclosed.

    摘要翻译: 公开了具有第一外部区域压缩应力和其上具有第一涂层的第一面的增强的玻璃基衬底。 所述第一涂层包含被选择为具有第一涂层杨氏模量值,第一涂层厚度和第一涂层应力的材料,所述第一涂层厚度和第一涂层应力为中性或压缩,使得第一外区压应力的绝对值大于绝对值 的第一涂层应力。 提供了制造基于玻璃的制品的方法,并且还公开了具有在玻璃基制品的不同侧上提供不同强度值和/或可靠性的涂层的基于玻璃的制品。

    COATED GLAZING
    4.
    发明申请
    COATED GLAZING 审中-公开
    涂层玻璃

    公开(公告)号:WO2016166527A1

    公开(公告)日:2016-10-20

    申请号:PCT/GB2016/051028

    申请日:2016-04-13

    IPC分类号: C03C17/25 B60J1/00 C03C17/34

    摘要: The invention relates to a coated glazing, a method of manufacturing said glazing and the use of a layer based on silica and/or an organo silica deposited on a glazing to achieve a coefficient of kinetic friction between an exterior surface of the layer based on silica and/or an organo silica and a contact surface wiping means that does not substantially change between a dry state and a wet state of said surfaces. Also disclosed is a glazing suitable for combination with a wiping means, the combination of said glazing with a wiping means and the use of said glazing to facilitate a reciprocating motion of a part of a wiping means and/or to facilitate a tilting and/or flipping of a part of a wiping means.

    摘要翻译: 本发明涉及一种涂覆玻璃,一种制造所述玻璃的方法,以及使用沉积在玻璃上的二氧化硅和/或有机二氧化硅层,以获得基于二氧化硅的层的外表面之间的动摩擦系数 和/或有机二氧化硅和接触表面擦拭装置,其在所述表面的干燥状态和湿态之间基本上不变化。 还公开了一种适于与擦拭装置组合的玻璃窗,所述玻璃窗与擦拭装置的组合以及所述玻璃窗的使用以促进擦拭装置的一部分的往复运动和/或促进倾斜和/或 翻转一部分擦拭装置。

    低反射コーティング、低反射コーティング付き基板および光電変換装置
    5.
    发明申请
    低反射コーティング、低反射コーティング付き基板および光電変換装置 审中-公开
    低反射涂层,具有低反射涂层的基板和光电转换装置

    公开(公告)号:WO2016002215A1

    公开(公告)日:2016-01-07

    申请号:PCT/JP2015/003300

    申请日:2015-06-30

    摘要:  本発明の低反射コーティングは、中実な球状で平均粒径が80~150nmであるシリカ微粒子が、シリカを主成分とするバインダによって固定されてなる多孔質膜である。バインダは、アルミニウム化合物をさらに含む。低反射コーティングにおける成分の含有率は、質量%表示で、シリカ微粒子55~70%、バインダにおけるシリカ25~40%、アルミニウム化合物をAl 2 O 3 に換算して2~7%、である。低反射コーティングの膜厚は80~800nmである。低反射コーティングを基板に施すことにより得られる透過率ゲインは2.5%以上である。ここで、透過率ゲインは、波長域380~850nmにおける平均透過率に関し、前記低反射コーティングを施す前の基板の平均透過率に対する、前記低反射コーティングを施した前記基板の平均透過率の増分、である。

    摘要翻译: 该低反射涂层是通过具有二氧化硅作为其主要成分的粘合剂固定平均粒径为80-150nm的固体球形二氧化硅微粒的多孔膜。 粘合剂还包括铝化合物。 表示为质量%的低反射涂层中的成分的含量比例为二氧化硅微粒的55-70%,粘合剂中的二氧化硅为25-40%,铝化合物为Al 2 O 3为2-7%。 低反射涂层的膜厚为80-800nm。 通过将低反射涂层施加到基板而获得的透射率增加为2.5%以上。 这里,透射率增益与380-850nm的波长区域的平均透射率有关,并且是低反射涂层所施加的基板的平均透射率相对于低于基板的平均透射率之前的增加 应用反射涂层。

    アンチグレア膜付ガラス曲板の製造方法
    7.
    发明申请
    アンチグレア膜付ガラス曲板の製造方法 审中-公开
    制造具有防透膜的弯曲玻璃板的方法

    公开(公告)号:WO2015133346A1

    公开(公告)日:2015-09-11

    申请号:PCT/JP2015/055407

    申请日:2015-02-25

    发明人: 池上 耕司

    摘要:  高い防眩性を有するアンチグレア膜付ガラス曲板を好適に製造し得る方法を提供する。 ガラス平板10の一主面10bの上に、ガラス平板10よりもガラス転移温度(Tg)が高いアンチグレア膜11を成膜し、アンチグレア膜付ガラス平板12を作製する成膜工程を行う。アンチグレア膜付ガラス平板12を加熱しながら変形させ、アンチグレア膜付ガラス曲板14を作製する変形工程を行う。

    摘要翻译: 提供一种可以适当地制造设置有具有高抗眩光性的防眩光膜的弯曲玻璃板的方法。 本发明中,在平板玻璃板的主面(10b)上形成玻璃化转变温度(Tg)高于平板玻璃板(10)的防眩光膜(11)的成膜工序, (10),并制造设置有防眩光膜的平板玻璃板(12)。 在本发明中,为了使设置有防眩光膜的平板玻璃板(12)变形而进行变形,进行加热,制造设有防眩光膜的弯曲玻璃板(14)。

    METHODS TO BOND SILICA PARTS, A CRUCIBLE, A SYSTEM FOR GROWING A SINGLE CRYSTAL INGOT AND A METHOD FOR GROWING A SINGLE CRYSTAL INGOT
    8.
    发明申请
    METHODS TO BOND SILICA PARTS, A CRUCIBLE, A SYSTEM FOR GROWING A SINGLE CRYSTAL INGOT AND A METHOD FOR GROWING A SINGLE CRYSTAL INGOT 审中-公开
    粘结二氧化硅部件的方法,可溶性,用于生长单晶体的系统和用于生长单晶的方法

    公开(公告)号:WO2014100487A3

    公开(公告)日:2015-03-05

    申请号:PCT/US2013076708

    申请日:2013-12-19

    申请人: SUNEDISON INC

    IPC分类号: C03C27/06

    摘要: A method of bonding a first silica part to a second silica part includes coating contacting surfaces of the first and second silica parts with a solution having one of silica and silica precursors. The coated surfaces of the first silica part are placed adjacent to the coated surfaces of the second silica part to form an assembly, and the assembly is heated, a crucible for use in directional solidification of multicrystalline ingots comprising a base, a sidewall and a weir, a system for growing a single crystal ingot comprising a crucible having a base, a sidewall, a weir, a heater and a feed tube, and a method for growing a single crystal ingot from a crucible havng a base and a sidewall and a weir comprising placing a feedstock material into the crucible, melting the feedstock material, lowering a seed cyrstal into the melt and pulling the seed crystal from the melt to pull an ingot.

    摘要翻译: 将第一二氧化硅部分结合到第二二氧化硅部分的方法包括第一和第二二氧化硅部分的涂层接触表面与具有二氧化硅和二氧化硅前体之一的溶液。 第一二氧化硅部分的涂覆表面被放置成与第二二氧化硅部分的涂覆表面相邻以形成组件,并且组件被加热,坩埚用于多晶锭的定向凝固,所述多晶锭包括基体,侧壁和堰 ,用于生长单晶锭的系统,其包括具有基底,侧壁,堰,加热器和进料管的坩埚,以及用于从具有基部和侧壁的坩埚和堰的生长单晶锭的方法 包括将原料材料放入坩埚中,熔化原料,将晶体降低成熔体并将晶种从熔体中拉出以拉出晶锭。

    GLASS OUTPUT COATED WITH A SOLUTION
    9.
    发明申请
    GLASS OUTPUT COATED WITH A SOLUTION 审中-公开
    玻璃输出涂有溶液

    公开(公告)号:WO2015012772A2

    公开(公告)日:2015-01-29

    申请号:PCT/TR2014/000073

    申请日:2014-03-12

    IPC分类号: C03C17/25

    摘要: The present invention relates to a coating solution applied to glass surfaces for increasing transmittances of cover glasses used in photovoltaic modules and in thermal collectors, the production method of said coating solution, the application thereof onto the glass, and relates to coated glass.

    摘要翻译: 本发明涉及一种涂覆在玻璃表面上的涂覆溶液,用于提高光伏模块和集热器中使用的覆盖玻璃的透射率,所述涂覆溶液的生产方法,其在玻璃上的应用, 并涉及镀膜玻璃。

    太陽電池劣化抑制用の塗工液及びその薄膜、並びに太陽電池劣化抑制方法
    10.
    发明申请
    太陽電池劣化抑制用の塗工液及びその薄膜、並びに太陽電池劣化抑制方法 审中-公开
    用于抑制太阳能电池的测定,薄膜的薄膜的涂覆液体和用于抑制太阳能电池的测定的方法

    公开(公告)号:WO2014199798A1

    公开(公告)日:2014-12-18

    申请号:PCT/JP2014/063644

    申请日:2014-05-23

    摘要:  太陽電池の部材そのものを変更することなく、太陽電池の発電能力の低下を防ぐ手段を提供する。 ケイ素、アルミニウム、ジルコニウム、スズ及び亜鉛から選ばれる少なくとも1種の金属の、水溶性化合物の水溶液又は該金属の酸化物の微粒子分散液からなり、金属酸化物換算で固形分濃度が0.01~10質量%であり、該微粒子分散液は平均一次粒径が50nm以下の微粒子が、分散粒径(D50)100nm未満で分散している、太陽電池劣化抑制用塗工液、該塗工液から形成された厚さ10~700nmの太陽電池劣化抑制用薄膜、該塗工液を太陽電池のカバーガラス面上に塗布し、常温~200℃の温度で乾燥硬化させて厚さ10~700nmの薄膜を形成する太陽電池劣化抑制方法、及び該塗工液の薄膜を太陽電池のカバーガラス面上に形成した、劣化抑制された太陽電池。

    摘要翻译: 提供了防止太阳能电池的发电能力下降而不改变太阳能电池的部件本身的装置。 一种用于抑制太阳能电池劣化的涂布液,其由选自硅,铝,锆,锡和锌中的至少一种金属的水溶性化合物的水溶液组成,或者由 金属氧化物的细颗粒的分散液,其中固体成分浓度为金属氧化物换算为0.01〜10质量%,或平均一次粒径为50nm以下的微粒分散在 分散粒径(D50)小于100nm的分散液; 用于抑制由涂布液形成并具有10-700nm厚度的太阳能电池的劣化的薄膜; 一种用于抑制太阳能电池劣化的方法,其中将涂布液涂覆在太阳能电池盖玻璃的表面上,并在常温至200℃的温度下干燥固化,从而形成具有 厚度10-700nm; 以及太阳能电池的太阳能电池,其中在太阳能电池的盖玻璃的表面上形成涂布液的薄膜,并且其被抑制劣化。