Invention Grant
- Patent Title: Adhesive sheet and method for producing same
-
Application No.: US15300141Application Date: 2015-04-02
-
Publication No.: US10221339B2Publication Date: 2019-03-05
- Inventor: Satoshi Kawada , Kiichiro Kato , Kazue Uemura , Yumiko Amino , Shigeru Saito , Koji Tsuchibuchi , Takamasa Kase
- Applicant: LINTEC CORPORATION
- Applicant Address: JP Itabashi-ku
- Assignee: LINTEC CORPORATION
- Current Assignee: LINTEC CORPORATION
- Current Assignee Address: JP Itabashi-ku
- Agency: Oblon, McClelland, Maier & Neustadt, L.L.P.
- Priority: JP2014-076577 20140402; JP2014-076579 20140402; JP2014-076580 20140402
- International Application: PCT/JP2015/060423 WO 20150402
- International Announcement: WO2015/152357 WO 20151008
- Main IPC: C09J7/02
- IPC: C09J7/02 ; C08K3/34 ; C09J133/08 ; C09J5/00 ; C09J7/38 ; C09J201/00 ; B05D1/36 ; B05D3/10 ; B05D5/00 ; C09J11/04 ; C09J7/22 ; C09J7/20 ; C09J7/25 ; C09J7/10 ; C09J121/00 ; C09J167/00 ; C09J175/04 ; C08K3/013 ; C08K3/36 ; C08K7/00

Abstract:
A pressure sensitive adhesive sheet including, on a substrate or a release material, a resin layer including a resin part (X) containing a resin as a main component, and a particle part (Y) consisting of fine particles and having a surface (α) having pressure sensitive adhesiveness and one or more concave portions. When the surface (α) of the resin layer is adhered to a smooth surface of a light transmissive adherend to give a laminate, the areal ratio (S1) of the attached area adhered to the smooth surface to the surface (α) is 10 to 95% at 23° C. and 50% RH, and the area increase rate {[(S2−S1)/S1]×100} is −10 to 20% after heating of the smooth surface by statically leaving the laminate at 80° C. for 30 minutes.