摘要:
An object of the present invention is to provide a steel sheet for hot press-forming which makes it possible to produce a hot press-formed part excellent in perforation corrosion resistance and joint corrosion resistance in a severe environment, a hot press-formed part produced using the steel sheet for hot press-forming, and a method for producing a hot press-formed part using the steel sheet for hot press-forming. A steel sheet for hot press-forming of the present invention has a zinc coating layer and a Si-containing compound layer in this order on a base steel sheet, in which the Si-containing compound layer contains a silicone resin having an organic functional group of a carbon number of 4 or more. It is preferable that the zinc coating layer consists of a coating layer I and a coating layer II in this order on the base steel sheet, in which the coating layer I contains 60 mass% or more of Ni and the balance being Zn and inevitable impurities and has a coating weight of 0.01 g/m 2 or more and 5 g/m 2 or less, and the coating layer II contains 10 mass% or more and 25 mass% or less of Ni and the balance being Zn and inevitable impurities and has a coating weight of 10 g/m 2 or more and 90 g/m 2 or less.
摘要:
A surface treated steel plate having excellent corrosion resistance which comprises a steel sheet plated with a zinc-based metal or aluminum-based metal, a composite oxide coating film formed on the metal-plated steel, and an organic coating film formed on the composite oxide coating film, wherein the composite oxide coating film contains oxide particles and phosphoric acid and/or a phosphoric acid derivative, and the organic coating film has a film thickness of 1 to 5 νm.
摘要:
Provided is a method for manufacturing a hot-pressed member excellent in terms of surface appearance with which it is possible to stably manufacture a hot-pressed member having a homogeneous and good surface appearance without causing a significant increase in cost. A method for manufacturing a hot-pressed member includes heating a zinc-based coated steel sheet to a temperature range from the Ac3 transformation temperature to 1000°C, performing hot pressing work, and performing cooling, in which a surface-cleaning treatment is performed on the zinc-based coated steel sheet before the heating is performed. A method for manufacturing a hot-pressed member includes performing cold pressing work on a zinc-based coated steel sheet, heating the zinc-based coated steel sheet to a temperature range from the Ac3 transformation temperature to 1000°C, and cooling the heated steel sheet, in which a surface-cleaning treatment is performed on the zinc-based coated steel sheet before the heating is performed. It is preferable that the zinc-based coated steel sheet be a Zn-Ni-alloy-coated steel sheet having a coating layer on one or both sides of the Zn-Ni-alloy-coated steel sheet, and the coating layer have a chemical composition containing 10 mass% to 25 mass% of Ni and the balance being Zn and inevitable impurities and a coating weight per side of 10 g/m 2 to 90 g/m 2 .
摘要:
There is provided a galvanized steel sheet that has various properties such as corrosion resistance and adhesion and allows for high conductivity at a low contact pressure. A first layer film is formed by applying a surface treatment solution having a pH of 8 to 10 onto the surface of the galvanized steel sheet and drying the surface treatment solution by heating, the surface treatment solution containing a water-soluble zirconium compound, a tetraalkoxysilane, an epoxy group-containing compound, a chelating agent, a silane coupling agent, vanadic acid, and a metal compound in a specific ratio. Subsequently, a second layer film is formed by applying a surface treatment solution containing an organic resin onto the surface of the first layer film and drying the surface treatment solution by heating.
摘要:
The present invention provides a steel sheet for hot press-forming having excellent liquid-metal brittle resistance that ensures no liquid-metal brittle fracture even under hot press-forming conditions including a short transfer time so as to improve productivity. The steel sheet for hot press-forming having; the first coating layer on the surface of the steel sheet, containing 60% or more by mass Ni and a remainder composed of Zn and incidental impurities, a coating mass thereof being more than 5 g/m 2 and 50 g/m 2 or less per side, and the second coating layer on the first coating layer, containing 10% to 25% by mass Ni and a remainder composed of Zn and incidental impurities, a coating mass thereof being 10 to 90 g/m 2 per side.