ELECTROCHEMICAL CELLS EXPOSED TO HYDROSTATIC PRESSURE
    33.
    发明公开
    ELECTROCHEMICAL CELLS EXPOSED TO HYDROSTATIC PRESSURE 审中-公开
    ELEKTROCHEMISCHE ZELLEN MIT HYDROSTATISCHEM DRUCK

    公开(公告)号:EP3132485A1

    公开(公告)日:2017-02-22

    申请号:EP15717112.5

    申请日:2015-04-02

    申请人: BASF SE

    IPC分类号: H01M10/052

    摘要: The present invention relates to a battery comprising as a first component (A) a pressure vessel (A) and as a second component (B), which is inside of the pressure vessel (A), at least one electrochemical cell (B) comprising at least one cathode comprising at least one electroactive sulfur-containing material, wherein the pressure vessel (A) can be filled or is filled with a pressure medium (C) in order to generate a pressure in the range from 2 bar to 200 bar inside of said pressure vessel. The present invention further relates to a process for operating an electrochemical cell (B), wherein the electrochemical cell (B) is exposed to a hydrostatic pressure in the range from 2 bar to 200 bar.

    摘要翻译: 本发明涉及一种电池,其包括作为压力容器(A)的第一组分(A)和作为压力容器(A)内部的第二组分(B))的至少一个电化学电池(B),其包含 至少一个阴极,其包括至少一种电活性含硫材料,其中压力容器(A)可以填充或填充有压力介质(C),以产生在2巴至200巴范围内的压力 的压力容器。 本发明还涉及一种用于操作电化学电池(B)的方法,其中电化学电池(B)暴露于2巴至200巴的静水压力。

    KOMPOSITMATERIALIEN, IHRE HERSTELLUNG UND VERWENDUNG IN ELEKTROCHEMISCHEN ZELLEN
    36.
    发明公开
    KOMPOSITMATERIALIEN, IHRE HERSTELLUNG UND VERWENDUNG IN ELEKTROCHEMISCHEN ZELLEN 审中-公开
    复合材料,生产和使用电化学电池

    公开(公告)号:EP2826085A1

    公开(公告)日:2015-01-21

    申请号:EP13761297.4

    申请日:2013-03-05

    申请人: BASF SE

    IPC分类号: H01M4/38 H01M4/62

    摘要: The present invention relates to new composite materials, in the production of which at least (A) at least one polymer containing fluorine, (B) carbon in a modification that comprises at least 60% sp
    2 -hybridized C atoms, and C) at least one component containing sulfur are used as starting components, comprising a mixture that is thermally treated in a method step, which mixture contains starting components (A) and (B) or starting components (A) and (C) or starting components (A), (B), and (C), wherein the fraction of the sum of the weight fractions of starting components (A) and (B), (A) and (C), or (A), (B), and (C) in the particular mixture before the thermal treatment with respect to the total weight of the mixture before the thermal treatment is 90 to 100%, and wherein the thermal treatment of the mixture containing starting components (A) and (B), (A) and (C), or (A), (B), and (C) is performed at a temperature of at least 115 °C. The present invention further relates to a method for producing composite materials according to the invention, cathode materials for electrochemical cells containing composite materials according to the invention, corresponding electrochemical cells, and special thermally treated mixtures containing at least starting components (A) and (C).