Abstract:
Polymer composition comprising a) an oligo- or polyurethane U of the formula (I) wherein k and n independently are numbers from 1 to 100, m is from the range 1-100, (X) is a block of formula (II) and (Y) is a block of the formula (III), (A) is a residue of an aliphatic or aromatic diisocyanate linker, (B) is a residue of a linear oligo- or polysiloxane containing alkanol end groups, and optionally further containing one or more aliphatic ether moieties, and (C) is an aromatic oligo- or polyarylene ether block that is at least partly etherified at its terminal positions with one alkylene glycol unit; or a mixture of such oligo- or polyurethanes; and b) one or more further organic polymers P selected from the group consisting of polyvinyl pyrrolidone, polyvinyl acetates, cellulose acetates, polyacrylonitriles, polyamides, polyole- fines, polyesters, polyarylene ethers, polysulfones, polyethersulfones, polyphenylenesulfones, polycarbonates, polyether ketones, sulfonated polyether ketones, polyamide sul- fones, polyvinylidene fluorides, polyvinylchlorides, polystyrenes and polytetrafluorethylenes, copolymers thereof, and mixtures thereof; preferably selected from the group consisting of polysulfones, polyphenylenes, polyethersulfones, polyvinylidene fluorides, polyamides, cellulose acetate and mixtures thereof.
Abstract:
The present invention relates to a method for producing thermosetting resin moldings, to the thermosetting resin moldings as such, to the use of the thermosetting resin moldings as structural components and to the use of a thermoplastic polymer having a porosity in the range of from 10 to 90% to increase the toughness of a thermosetting resin.
Abstract:
Process for making a membrane M comprising the following steps: a) preparing a copolymer C, wherein said copolymer C comprises blocks of at least one polyarylene ether A and blocks of polyalkylene oxide PAO, wherein the content of polyethyleneoxide in copolymer C is 30 to 90% by weight and wherein copolymer C is prepared in a solvent L to yield solution S; b) providing a dope solution D comprising at least one polymer P; c) mixing solution S and dope solution D; d) preparing a membrane by bringing the mixture of solution S and dope solution D into contact with at least one coagulating agent.
Abstract:
The invention relates to a method for producing a polyarylene ether sulfone polymer by reacting a reaction mixture (R G ) containing a dihalogen component (A1), a dihydroxy component (B1) and potassium carbonate (C1) having an average volumetric particle size of