摘要:
The invention relates to a system (1) comprising at least one extruded or injection moulded part (5) consisting of a moulding mass containing a polymer material, the moulding mass containing at least one filler for reinforcement. The fraction of the reinforcement filler in the moulding mass ranges between 20 and 80 % by weight. The invention also relates to a method for producing a system (1), wherein the moulding mass that contains the reinforcement filler is formed into the part (5) by means of an extrusion method. The invention also relates to the use of said system (1).
摘要:
The present invention relates to a method for producing thermosetting resin moldings, to the thermosetting resin moldings as such, to the use of the thermosetting resin moldings as structural components and to the use of a thermoplastic polymer having a porosity in the range of from 10 to 90% to increase the toughness of a thermosetting resin.
摘要:
The present invention relates to a thermoplastic moulding composition which comprises the following components: A) from 10 to 50% by weight of at least one polyarylene ether having an average of at most 0.5 phenolic end groups per polymer chain and having no carboxy groups, B) from 5 to 44.5% by weight of at least one polyphenylene sulphide, C) from 10 to 65% by weight of at least one fibrous and/or particulate filler, D) from 0.5 to 20% by weight of an elastic graphite, E) from 0 to 20% by weight of at least one polyarylene ether comprising carboxy groups, F) from 0 to 20% by weight of at least one polyarylene ether having an average of at least 1.5 phenolic end groups per polymer chain and having no carboxy groups, and G) from 0 to 40% by weight of at least one additive, where the sum of the proportions by weight of components A) to G) is 100% by weight, based on the moulding composition.
摘要:
The invention relates to the use of a fibre-reinforced plastic material comprising an E-module that is > 8.000 N/mm2, preferably > 10.000 N/mm2, having a softening temperature of > 100°C, preferably > 150°C and an elongation coefficient of