摘要:
The present invention is directed to a primer composition comprising 2,5,7,10-tetraoxaundecane (TOU). The invention also provides a method of surface-treating a substrate to improve adhesive bonding thereto. Moreover, the present invention is further directed to an article comprising a substrate surface-treated with the primer composition according to the invention.
摘要:
The present invention is directed to a water based primer composition comprising an organic solvent selected from 2,5,7,10-teiraoxaundecane (TOU), propylene carbonate (PC), dimethyl-2-methylglutarate (IRIS) and dimethyl sulfoxide (DMSO). The invention also provides a method of surface-treating a substrate to improve adhesive bonding thereto. Moreover, the present invention is further directed to an article comprising a substrate surface-treated with the water based primer composition according to the invention.
摘要:
The present invention relates to a hot melt adhesive composition, comprising based on the total weight of the hot melt adhesive composition: (a) from about 10 to about 50 weight percent of at least one block copolymer; (b) from about 15 to about 50 weight percent of at least one plasticizer; (c) from about 15 to about 50 weight percent of at least one resins; (d) optionally up to 25 weight percent of at least one semicrystalline polyolefin; and (e) optionally up to 10 weight percent of at least one wax. The hot melt adhesive composition of the invention can be used for bonding bundles of metal containers such as cans into packs.
摘要:
An adhesive composition that includes: one or more polyester polyether copolymers of formula I: wherein Nu is a predominately cyclic nucleus and R1 is randomly selected from either a C2-6 alkylene or an amorphous, long-chain polyether subunit including a polyoxyalkylene group; one or more polyisocyanate prepolymers that includes the reaction product of: one or more polyols; and a polyfunctional isocyanate having a functionality of more than about 2; polymeric MDI; and a first aromatic or aromatic-aliphatic polymer tackifying resin having a softening point of equal to or greater than about 100° C.
摘要:
This invention claims hot melt adhesive compositions that can be used to form elastic composites that are useful in disposable absorbent articles. The compositions have good elastic recovery and high peel adhesion at a viscosity of less than about 15,000 cps at 177° C. (350° F.). The low viscosity makes it possible to apply the hot melt adhesive at a high line speed and target application to only those areas requiring elastic performance.
摘要:
The present invention relates to a packaged hot-melt pressure sensitive adhesive comprising a hot-melt pressure sensitive adhesive composition and a coextrusion coating consisting of neat low density polyethylene, neat polypropylene, or neat ethylene vinyl acetate. The present invention further relates to the use of the packaged adhesive formed as individual forms in an adhesive application process, and the use of the packaged adhesive in the production of laminated articles, including nonwoven hygiene articles, disposable medical drapes, and also laminate constructions such as tapes and labels.
摘要:
A fluid adhesive composition is disclosed that includes a liquid carrier and a solid particle including a ethylene copolymer where the ethylene copolymer has a Melt Index as tested by ASTM D 1238 (190° C./2.16 kg) of less than 2.
摘要:
A curable aqueous composition that includes a first polymer that includes carboxyl groups, and a second component that includes a second water insoluble polymer and a stabilizer. The second component includes functional groups that react with the carboxyl groups of the first polymer during cure, is free from carboxylic acid groups, or a combination thereof. The composition, when dry, exhibits a first Tg of at least 10°C and a second Tg of at least 50°C.
摘要:
A hot melt adhesive composition that includes a first copolymer that includes the reaction product of a functionalized polyethylene, a propylene-alpha-olefin polymer that includes at least 50 mole % propylene and has a viscosity of no greater than 10,000 centipoise at 190° C., a ratio of z average molecular weight (Mz) to number average molecular weight (Mn) (Mz/Mn) of greater than 20, and a ratio of Mz to weight average molecular weight (Mw) (Mz/Mw) of greater than 3.0, and a free radical initiator.