摘要:
A friction material composition may include an abrasive, a filler, a binder, and a spherical molybdenum disulfide powder. The spherical molybdenum disulfide powder is made up of molybdenum disulfide sub-particles that are agglomerated together to form individual, substantially spherically-shaped agglomerated particles of at least about 90% by weight molybdenum disulfide.
摘要:
A method of producing a compacted article according to one embodiment may involve the steps of: Providing a copper/molybdenum disulfide composite powder including a substantially homogeneous dispersion of copper and molybdenum disulfide sub-particles that are fused together to form individual particles of the copper/molybdenum disulfide composite powder; and compressing the copper/molybdenum disulfide composite powder under sufficient pressure to cause the copper/molybdenum disulfide composite powder to behave as a nearly solid mass.
摘要:
Molybdenum disulfide powders include substantially spherically-shaped particles of molybdenum disulfide that are formed from agglomerations of generally flake-like sub-particles. The molybdenum disulfide powders are flowable and exhibit uniform densities. Methods for producing a molybdenum disulfide powder may include the steps of: Providing a supply of molybdenum disulfide precursor material; providing a supply of a liquid; providing a supply of a binder; combining the molybdenum disulfide precursor material with the liquid and the binder to form a slurry; feeding the slurry into a stream of hot gas; and recovering the molybdenum disulfide powder, the molybdenum disulfide powder including substantially spherically-shaped particles of molybdenum disulfide formed from agglomerations of generally flake-like sub-particles.
摘要:
A method for producing a metal article according to one embodiment may involve the steps of: Providing a composite metal powder including a substantially homogeneous dispersion of molybdenum and molybdenum disulfide sub-particles that are fused together to form individual particles of the composite metal powder; and compressing the molybdenum/molybdenum disulfide composite metal powder under sufficient pressure to cause the mixture to behave as a nearly solid mass.
摘要:
A friction material composition may include an abrasive, a filler, a binder, and a spherical molybdenum disulfide powder. The spherical molybdenum disulfide powder is made up of molybdenum disulfide sub-particles that are agglomerated together to form individual, substantially spherically-shaped agglomerated particles of at least about 90% by weight molybdenum disulfide.
摘要:
Molybdenum disulfide powders include substantially spherically-shaped particles of molybdenum disulfide that are formed from agglomerations of generally flake-like sub-particles. The molybdenum disulfide powders are flowable and exhibit uniform densities. Methods for producing a molybdenum disulfide powder may include the steps of: Providing a supply of molybdenum disulfide precursor material; providing a supply of a liquid; providing a supply of a binder; combining the molybdenum disulfide precursor material with the liquid and the binder to form a slurry; feeding the slurry into a stream of hot gas; and recovering the molybdenum disulfide powder, the molybdenum disulfide powder including substantially spherically-shaped particles of molybdenum disulfide formed from agglomerations of generally flake-like sub-particles.