摘要:
A method of cementing a wellbore comprising preparing a wellbore cementing composition comprising a cementitious materials and a modified biopolymer additive wherein the modified biopolymer additive is the reaction product of a process comprising contacting a biopolymer and an organic carbonate to form a reaction mixture and subjecting the reaction mixture to a temperature of from about 100° F. to about 250° F. and placing the wellbore cementing fluid in the wellbore. A method of cementing a wellbore comprising contacting a modified biopolymer additive with a cementitious slurry to produce a wellbore cementing composition having an initial viscosity, v0; placing the wellbore cementing composition to a desired depth in a subterranean formation wherein the wellbore cementing composition has a transitional viscosity, vt, during placement in the subterranean formation and a final viscosity, vf, at the desired depth wherein vf≧vt>v0; and allowing the wellbore cementing composition to set.
摘要:
A method of cementing a wellbore comprising preparing a wellbore cementing composition comprising a cementitious materials and a modified biopolymer additive wherein the modified biopolymer additive is the reaction product of a process comprising contacting a biopolymer and an organic carbonate to form a reaction mixture and subjecting the reaction mixture to a temperature of from about 100° F. to about 250° F. and placing the wellbore cementing fluid in the wellbore. A method of cementing a wellbore comprising contacting a modified biopolymer additive with a cementitious slurry to produce a wellbore cementing composition having an initial viscosity, v0; placing the wellbore cementing composition to a desired depth in a subterranean formation wherein the wellbore cementing composition has a transitional viscosity, vt, during placement in the subterranean formation and a final viscosity, vf, at the desired depth wherein vf≧vt>v0; and allowing the wellbore cementing composition to set.
摘要翻译:一种固井井筒的方法,包括制备包含胶凝材料和改性生物聚合物添加剂的井筒胶结组合物,其中所述改性生物聚合物添加剂是包括使生物聚合物和有机碳酸盐接触以形成反应混合物并使反应 混合物加热至约100°F(38℃)至约250°F(121℃)的温度,并将井筒固井液置于井眼中。 一种固井的方法,包括使改性生物聚合物添加剂与水泥浆接触以产生具有初始粘度的井筒水泥组合物,v 0:将井筒水泥组合物置于地下地层中的期望深度,其中井筒水泥组合物具有 在放置在地下地层中的过渡粘度vt和在所需深度处的最终粘度V f,其中V f≥Vt> v 0; 并允许井筒固井组合物固化。
摘要:
The present invention relates to cement compositions and their use in cementing operations. The cements comprise an aluminosilicate; a sodium aluminate, a calcium aluminate, a potassium aluminate, or a combination thereof; and water. In some cases the cement does not include Portland cement. The cement may be used in a subterranean formation having corrosive components therein, wherein the set cement sheath is resistant to degradation from the corrosive components within the subterranean formation.
摘要:
According to an embodiment, a composition is provided that can be used in a cementing. The composition includes at least: (i) a hydraulic cement; and (ii) a copolymer comprising at least the monomeric units (a) through (d) of formula (A); (a) A = H, B = H, CH 3 (or) A = COOH, B = H, CH 2 , (b) D = -NH-C(CH 3 ) 2 -CH 2 -SO 3 M, Where M = Na, K, (c) E = H, CH 3 , F = -(CH 2 ) 2 -OH, -CH 2 -CH(CH 3 )-OH, wherein the monomeric units (a) through (d) can be any sequence and any proportion in the copolymer. With water, the composition of the hydraulic cement and such a copolymer becomes a cement composition. According to the method, the cement composition is introduced into a well and allowed to set in the well.
摘要:
A method of cementing in a subterranean formation comprising the steps of: (A) introducing a cement composition into the subterranean formation, the cement composition comprising: (i) cement; (ii) water; and (iii) a high-density additive selected from the group consisting of silicon carbide, sintered bauxite, and any combination thereof, wherein the cement composition has a density of at least 16 pounds per gallon; and (B) allowing the cement composition to set. According to an embodiment, the high-density additive is in a concentration of at least 30% by weight of the cement. A cement composition for use in an oil or gas well comprises: (A) cement; (B) water; and (C) a high-density additive selected from the group consisting of silicon carbide, sintered bauxite, and a combination thereof, wherein the high-density additive is in a concentration of at least 30% by weight of the cement, and wherein the cement composition has a density of at least 16 pounds per gallon.
摘要:
Methods and compositions for treating a subterranean formation with salt-tolerant cement slurries including treating a salt-containing subterranean formation having sodium salts, potassium salts, magnesium salts, calcium salts, or any combination thereof comprising: providing a salt-tolerant cement slurry comprising: a base fluid, a cementitious material, a pozzolanic material, a salt-tolerant fluid loss additive, a salt additive, and optionally, an elastomer, a weight additive, a fluid loss intensifier, a strengthening agent, a dispersant, or any combination thereof; introducing the salt-tolerant cement slurry into the subterranean formation; and allowing the salt-tolerant cement slurry to set.
摘要:
Methods and compositions are provided that relate to cement compositions and methods comprising sub-micron calcium carbonate and latex. An embodiment includes a method of cementing in a subterranean formation. The method may comprise introducing a cement composition into the subterranean formation, wherein the cement composition comprises cement, water, sub-micron calcium carbonate, and latex. The method further may comprise allowing the cement composition to set in the subterranean formation. Another embodiment includes a cement composition that may comprise cement, water, a sub-micron calcium carbonate, and latex.
摘要:
Methods and compositions are provided that may comprise cement, a nano-particle, latex, and water. An embodiment of the present invention includes a method of cementing in a subterranean formation. The method may include introducing a cement composition into the subterranean formation, wherein the cement composition comprises cement, a nano-particle, latex, and water. The method further may include allowing the cement composition to set in the subterranean formation. Another embodiment of the present invention include a cement composition. The cement composition may comprise cement, a nano-particle, latex, and water.