摘要:
A dielectric porcelain composition of the present invention includes a first component and second component. If the first component is represented by the general formula of xBaO-yNd 2 O 3 -zTiO 2 -wBi 2 O 3 (provided that x+y+z+w= 100), x, y, z, and w satisfy 12 ≤ x ≤ 16,12 ≤ y ≤ 16, 65 ≤ z ≤ 69, and 2 ≤ w ≤ 5, respectively. The second component includes 30 to 37 wt% of BaO, 33 to 46 wt% of SiO 2 , 8 to 12 wt% of La 2 O 3 , 3 to 7 wt% of Al 2 O 3 , 0 to 1 wt% of SrO, 0 to 10 wt% of Li 2 O, 0 to 20 wt% of ZnO, and 7 wt% or less of B 2 O 3 . The compounding ratio of the second component is between 10 wt% and 30 wt% when the sum of the first and second components is 100. In addition, 0.1 to 1 parts by weight of Li 2 O and 3 to 10 parts by weight of ZnO, relative to 100 parts by weight of the sum of the first and second components, is also contained as a third component. An average particle diameter of the dielectric mixed powder forming dielectric porcelain composition before firing is 0.9 µm or less.
摘要翻译:本发明的电介质瓷组合物包括第一组分和第二组分。 如果第一组分由通式xBaO-yNd 2 O 3 -zTiO 2 -wBi 2 O 3表示(假定x + y + z + w = 100),x,y,z和w满足12‰ x‰16,12‰y‰16,65‰z‰69,‰‰5。 第二组分包括30至37重量%的BaO,33至46重量%的SiO 2,8至12重量%的La 2 O 3,3至7重量%的Al 2 O 3,0至1重量%的SrO ,0〜10重量%的Li 2 O,0〜20重量%的ZnO和7重量%以下的B 2 O 3。 当第一和第二组分的总和为100时,第二组分的配混比为10重量%至30重量%。此外,将0.1至1重量份的Li 2 O和3至10重量份的ZnO 相对于100重量份的第一和第二组分的总和,也被包含为第三组分。 焙烧前的介电混合粉末形成介电瓷组合物的平均粒径为0.9μm以下。
摘要:
It is an object of the present invention to provide a ceramic component with high reliability and accuracy in dimension in which electrical characteristics thereof are not largely deteriorated and defects such as cracks around the inner electrodes in the substrate after firing are inhibited, in a firing technique with high accuracy in dimension for sandwiching a glass ceramic laminate with heat-shrinkage inhibiting sheets and firing them. In order to achieve this object, the method of manufacturing the ceramic component of the present invention includes: a conductor printing step of applying, to a glass ceramic green sheet, conductor paste that has substantially the same sintering speed as the glass ceramic green sheet; a lamination step of laminating a plurality of the glass ceramic green sheets to form a laminate; a composite lamination step of further laminating, on at least one side of the laminate, a heat-shrinkage inhibiting green sheet based on inorganic material to form a composite laminate; a debindering step of burning out organic material from the composite laminate; a firing step of sintering the composite laminate after the removal of the organic material so that the sintering behaviors of the glass ceramic green sheets and the conductor paste match with each other; and a step of removing the inorganic material in the heat-shrinkage inhibiting green sheet.
摘要:
A high-reliability, high-dimension-accuracy ceramic component having electric characteristics thereof not significantly deteriorated and defects such as cracks restricted in the vicinity of an internal electrode in a substrate after firing when subjected to a high-dimension-accuracy firing method in which a glass ceramic laminate is fired while being held between heat shrinkage restricting sheets. A method of producing a ceramic component comprising the conductor printing step of printing on a glass ceramic green sheet a conductor paste having a sintering speed equivalent to that of the glass ceramic green sheet, the laminating step of laminating a plurality of the glass ceramic green sheets to form a laminate, a composite laminating step of further laminating on the one or both surfaces of the laminate heat shrinkage restricting green sheets mainly containing inorganic matters, a binder removing step of removing by burning organic matters from the composite laminate, the firing step of sintering the organic matter-removed composite laminate with sintering behaviors of the glass ceramic green sheets and the conductor paste matched, and the step of removing inorganic matters in the heat shrinkage green sheets.
摘要:
There is provided a static electricity countermeasure component including a varistor layer having a plurality of inner electrodes of a planer shape, embedded therein a board including alumina laminated with the varistor layer, and a terminal connected to the inner electrode of the varistor layer and formed at a side face of the varistor layer, in which the varistor layer and the board are sintered to thereby diffuse bismuth oxide of the varistor layer in the board and provide a bismuth oxide diffusing layer at the board. In this way, the static electricity countermeasure component achieving thin-sized formation while maintaining a varistor characteristic against a small surge voltage can be realized.
摘要:
A laminated filter includes : a first dielectric layer 2101a having a first shield electrode on one principal plane; a second dielectric layer 2101b having resonator electrodes on one principal plane; a third dielectric layer 2101c having a coupling electrode provided facing part of the above-described resonator electrodes; a fourth dielectric layer 2101d having a second shield electrode on one principal plane; a fifth dielectric layer 2101d whose at least one principal plane is exposed outside; and a grounding electrode 2108 provided on the other principal plane of the above-described dielectric layer and/or the above-described one principal plane of the above-described fifth dielectric layer, and the above-described first grounding electrode and the above-described first shield electrode are electrically connected through a via hole 2109 provided in the above-described first dielectric layer.