摘要:
A cubic boron nitride sintered material includes: more than or equal to 20 volume% and less than or equal to 80 volume% of cubic boron nitride grains; and more than or equal to 20 volume% and less than or equal to 80 volume% of a binder phase, wherein the binder phase includes first binder grains and second binder grains, each of the first binder grains and the second binder grains includes one compound composed of titanium, at least one first metal element selected from a group consisting of zirconium, hafnium, a group 5 element, a group 6 element in a periodic table, and aluminum, and one or both of nitrogen and carbon, in each of the first binder grains, a ratio of the number of atoms of the first metal element to a total of the number of atoms of the titanium and the number of atoms of the first metal element is more than or equal to 0.01% and less than 10%, in each of the second binder grains, a ratio of the number of atoms of the first metal element to a total of the number of atoms of the titanium and the number of atoms of the first metal element is more than or equal to 10% and less than or equal to 80%, and an average grain size of the second binder grains is more than or equal to 0.2 µm and less than or equal to 1 µm.
摘要:
A cubic boron nitride sintered material comprises cubic boron nitride particles and a binding phase. The binding phase includes a first region and a second region. The first region accounts for 1.0 vol% or more in the binding phase. The first region includes a plurality of needle crystals. Each of the plurality of needle crystals includes a boride. Each of the plurality of needle crystals has an aspect ratio of 1.5 or more in a cross-section image of the cubic boron nitride sintered material.
摘要:
A cubic boron nitride sintered material comprising cubic boron nitride grains and a binder, in which a content of the cubic boron nitride grains in the cubic boron nitride sintered material is no less than 30% by volume and no more than 80% by volume, the binder includes at least one selected from a second group consisting of a material made of a single element selected from a first group consisting of a group 4 element, a group 5 element and a group 6 element of the periodic table, aluminum, silicon, iron, cobalt and nickel, and an alloy and an intermetallic compound each composed of no less than two elements selected from the first group, or at least one selected from a fourth group consisting of a compound composed of one element selected from the first group and at least one element selected from a third group consisting of nitrogen, carbon, boron and oxygen, and a solid solution of the compound, and a content of a void in the cubic boron nitride sintered material is no less than 0.001% by volume and no more than 0.20% by volume.
摘要:
A cubic boron nitride sintered material includes: more than or equal to 20 volume% and less than or equal to 80 volume% of cubic boron nitride grains; and more than or equal to 20 volume% and less than or equal to 80 volume% of a binder phase, wherein the binder phase includes first binder grains and second binder grains, each of the first binder grains and the second binder grains includes one compound composed of titanium, at least one first metal element selected from a group consisting of zirconium, hafnium, a group 5 element, a group 6 element in a periodic table, and aluminum, and one or both of nitrogen and carbon, in each of the first binder grains, a ratio of the number of atoms of the first metal element to a total of the number of atoms of the titanium and the number of atoms of the first metal element is more than or equal to 0.01% and less than 10%, in each of the second binder grains, this ratio is more than or equal to 10% and less than or equal to 80%, and in an X-ray diffraction spectrum of the cubic boron nitride sintered material, one or both of conditions 1 and 2 are satisfied.
摘要:
A cutting tool comprises a substrate and a coating film disposed on the substrate, wherein the coating film comprises a first layer and a second layer; the first layer has a hardness Hi of 25 GPa or more and 40 GPa or less; the second layer has a hardness H2 satisfying 0.5×H1≤H2≤0.9×H1; and at least one of a ratio I(200)/(I(200)+I(111)+I(220)) of I(200) of (200) plane to a sum of X-ray diffraction intensity I(200) of (200) plane, X-ray diffraction intensity I(111) of (111) plane, and X-ray diffraction intensity I(220) of (220) plane of the coating film, a ratio I(111)/(I(200)+I(111)+I(220)) of I(111) to the sum, and a ratio I(220)/(I(200)+I(111)+I(220)) of I(220) to the sum is 0.45 or more.
摘要:
A cutting tool comprising a substrate and a coating film disposed on the substrate, wherein the coating film comprises a first layer; the first layer has a thickness of 0.2 µm or more and 9 µm or less; the first layer is composed of Ti(1-x-y)AlxMyN, wherein M is at least one element selected from the group consisting of zirconium, hafnium, a group V element in the periodic table, a group VI element, silicon and boron; in the first layer, x and y change along the thickness direction of the first layer; a maximum value of x, xmax, is 0.20 or more and 0.70 or less; a minimum value of x, xmin, is 0 or more and 0.6 or less; xmax and xmin satisfy 0.01 ≤ xmax - xmin ≤ 0.7; a maximum value of y, ymax, is 0.01 or more and 0.20 or less; a minimum value of y, ymin, is 0 or more and 0.19 or less; and ymax and ymin satisfy 0.01 ≤ ymax - ymin ≤ 0.2.
摘要:
A cutting insert has a surface that relates to cutting, the surface comprising cBN sintered material, ceramics, or cermet. The cutting insert comprises: a rake face; a flank face; a chamfer located between the rake face and the flank face; and a cutting edge formed by a ridgeline at which the flank face and the chamfer intersect. The cutting edge comprises a cutting edge portion for push cutting, a cutting edge portion for pull cutting, and a connecting cutting edge portion located between the cutting edge portion for push cutting and the cutting edge portion for pull cutting. In the chamfer located along the cutting edge, the chamfer located along the connecting cutting edge portion has a minimum width.
摘要:
A surface-coated cutting tool including a substrate including a rake face and a flank face and a coating which covers a surface of the substrate is provided. The substrate is made of a cBN sintered material or a ceramic sintered material. The coating includes an alternating layer. The alternating layer is made by alternately stacking a first layer and a second layer different in composition from the first layer. The first layer contains Al, Cr, and N. The second layer contains Ti, Al, and N. A ratio T1/T2 between a thickness T1 of the first layer and a thickness T2 of the second layer is not lower than 0.1 and lower than 1. There are thirty or more interfaces at which the first layer and the second layer are in contact with each other.
摘要:
To provide a sintered material having excellent oxidation resistance, as well as excellent abrasion resistance and chipping resistance. A sintered material containing a first compound formed of Ti, Al, Si, O, and N is provided.
摘要:
A sintered body includes a first hard particle, a second hard particle, and a binder. The first hard particle is an M sialon particle having a coating layer. The M sialon particle is represented by M x Si (6-x-z) Al z O z N (8-z) (in the formula, M is a metal containing at least one selected from the group consisting of calcium, strontium, barium, scandium, yttrium, lanthanoid, manganese, iron, cobalt, nickel, copper, and group IV, group V, and group VI elements of the periodic table, and relationships of 0.01 ≤ x ≤ 2, 0.01 ≤ z ≤ 4.2, and 1.79 ≤ (6 - x - z) ≤ 5.98 are satisfied). The second hard particle is a cubic boron nitride particle.
摘要翻译:烧结体包含第一硬质颗粒,第二硬质颗粒和粘合剂。 第一硬质粒子是具有被覆层的M赛隆粒子。 M硅铝土颗粒由M x Si(6-xz)Al z O z N(8-z)表示(式中,M为含有选自钙,锶,钡,钪,钇,镧系元素, 锰,铁,钴,镍,铜和IV族,V族和VI族元素,并且0.01≤x≤2,0.01≤z≤4.2和1.79≤(6-x-z )≤5.98)。 第二硬质颗粒是立方氮化硼颗粒。