摘要:
Composite body comprises nanofibrillar cellulose (NFC) together with abrasive particles (AP). The nanofibrillar cellulose forms a 3-dimensional connecting network for the abrasive particles (AP). The abrasive particles have a hardness above 7 on Mohs scale. The composite body is used for grinding, polishing or cutting.
摘要:
The present invention relates to nanofibrillar polysaccharide hydrogels for use in the prevention and control of scarring and contraction in connection with wound healing or tissue repair.
摘要:
Method for preparing a membrane from fibril cellulose includes supplying fibril cellulose dispersion on a filter layer, draining liquid from a fibril cellulose dispersion by the effect of reduced pressure through the filter layer that is impermeable to fibrils of the fibril cellulose but permeable to the liquid to form a membrane sheet on the filter fabric, applying heat on the opposite side of the membrane sheet to the membrane sheet while continuing draining of the liquid through the filter layer by pressure difference over the filter layer, and removing the membrane sheet from the filter layer as a freestanding membrane.
摘要:
The present invention is related to methods and materials for culturing and transporting stem cells in a three-dimensional culture. The materials comprise cellulose nanofibrils in a form of three-dimensional discontinuous entities in a biocompatible hydrogel.
摘要:
The invention relates to a method for treating nanofibrillar cellulose hydrogel, wherein the method comprises the steps of: providing a nanofibrillar cellulose hydrogel; and subjecting the nanofibrillar cellulose hydrogel to heat treatment, wherein the heat treatment comprises keeping the nanofibrillar cellulose hydrogel at a temperature of at least 130° C. for at least 0.5 seconds, for reducing the number of viable micro-organisms in the nanofibrillar cellulose hydrogel.
摘要:
In a method for preparing nanofibrillar cellulose, fibrous dispersion of ionically charged cellulose is repeatedly passed through a mechanical process of disrupting fibers into fibrils until the viscosity starts to decrease. The number average diameter of the nanofibrillar cellulose after the mechanical process is in the range of 2 – 10 nm, and the zero-shear viscosity is below 10 Pa•s, preferably below 1 Pa•s, when measured in the concentration of 0.5 wt-%. The nanofibrillated cellulose is low aspect ratio nanofibrillated cellulose (NFC-L).