公开(公告)号:JP2007084817A
公开(公告)日:2007-04-05
申请号:JP2006235299
申请日:2006-08-31
Applicant: Rohm & Haas Co , ローム アンド ハース カンパニーRohm And Haas Company
Inventor: FINCH WILLIAM C , TUNG SUNG
IPC: C08L33/02 , C08K3/32 , C08K5/053 , C08L91/00 , C09J11/04 , C09J11/06 , C09J145/00 , C09J161/06 , C09J193/04 , C09J201/08
CPC classification number: C09D193/02 , C08K3/32 , C08K5/13 , C08L33/02 , C08L93/00 , C08L93/04 , C08L2666/02 , C09D133/02 , C09J193/00 , C09J193/04 , C08L2666/26 , C08L2666/04
Abstract: PROBLEM TO BE SOLVED: To provide an aqueous composition exhibiting necessary viscoelastic rhelogical behavior, i.e. viscous flow to enable the formation of adhesive binding and elasticity to attain strength and provide a method for curing the composition.
SOLUTION: The aqueous composition contains a polycarboxy polymer, a reactive tackifier selected from rosin-based resins, rosin esters, terpene-based resins, coumarone-based resins and phenolic tackifiers, and a polyol.
COPYRIGHT: (C)2007,JPO&INPITAbstract translation: 要解决的问题:提供显示出必要的粘弹性流变行为即粘性流动以使得能够形成粘合剂结合和弹性以获得强度并提供固化该组合物的方法的水性组合物。 水溶性组合物含有多羧基聚合物,选自松香类树脂,松香酯,萜烯类树脂,香豆酮类树脂和酚类增粘剂的反应性增粘剂和多元醇。 版权所有(C)2007,JPO&INPIT
-
公开(公告)号:JP2007501882A
公开(公告)日:2007-02-01
申请号:JP2006522932
申请日:2004-07-29
Inventor: アルノ・デュッフェルス , ヴォルフガング・バルテル , ウルフ・アルノ・ティンマン , クリスティアン・ニッチュ , サルヴァトーレ・フィレッチャ , ビルギット・ブルク , マレン・イェケル
IPC: C11D3/37 , C08G18/08 , C08G18/48 , C08L75/04 , C09J11/04 , C09J11/06 , C09J131/04 , C09J133/02 , C09J175/04 , C09J201/08 , C11D3/30 , C11D11/00 , C11D17/00 , C11D17/04 , C11D17/06
CPC classification number: C09J175/04 , C08G18/0804 , C08G18/48 , C08L75/04 , C08L2666/20 , C09J131/04 , C11D3/3726 , C11D3/3761 , C11D17/0073 , C11D17/042
Abstract: エチレン性不飽和モノマーに基づく遊離カルボン酸基を有する少なくとも一つのホモポリマーまたはコポリマー(成分A)40〜70重量%、少なくとも一つの水溶性または水分散性ポリウレタン(成分B)15〜45重量%、少なくとも一つの無機または有機塩基(成分C)10〜45重量%、および0〜20重量%の他の添加剤を含有する水溶性溶融接着剤を含んでなる洗剤または洗浄剤を開示する。 本発明の洗剤または洗浄剤は、高められた貯蔵寿命、改善された崩壊に対する安定性、および有利な溶解挙動を特徴とする。
-
公开(公告)号:JP2006294600A
公开(公告)日:2006-10-26
申请号:JP2006067582
申请日:2006-03-13
Applicant: Matsushita Electric Ind Co Ltd , 松下電器産業株式会社
Inventor: YAMAGUCHI ATSUSHI , MIYAGAWA HIDEKI , HIGUCHI TAKAYUKI , SUGIYAMA KUMIKO , SAKATANI SHIGEAKI
IPC: H01B1/22 , C09C1/62 , C09C3/06 , C09J9/02 , C09J11/04 , C09J201/08 , H01B1/00 , H05K3/12 , H05K3/32
Abstract: PROBLEM TO BE SOLVED: To provide a conductive adhesive materializing stable low resistance bonding when mounting an electronic component. SOLUTION: This conductive adhesive contains a metal filler component containing a low melting point metal component having Sn, Bi and/or In as a basic composition and an Ag filler as well as a resin component. An Ag filler the surface of which is coated with the low melting point metal component can be used as the Ag filler. In addition, it may contain a metal selected from a group of Cu, Ag, and Ni. The resin component contains an epoxy resin as a first component. In addition, it may contains a resin having reducibility as a second resin component. COPYRIGHT: (C)2007,JPO&INPIT
Abstract translation: 要解决的问题:提供一种在安装电子部件时实现稳定的低电阻接合的导电粘合剂。 解决方案:该导电粘合剂包含含有作为碱性组合物的Sn,Bi和/或In的低熔点金属组分的金属填充剂组分和Ag填料以及树脂组分。 可以使用其表面涂有低熔点金属组分的Ag填料作为Ag填料。 此外,它可以含有选自Cu,Ag和Ni中的一种金属。 树脂成分含有环氧树脂作为第一成分。 此外,它可以含有作为第二树脂组分具有还原性的树脂。 版权所有(C)2007,JPO&INPIT
-
84.
公开(公告)号:JP3777734B2
公开(公告)日:2006-05-24
申请号:JP21744697
申请日:1997-08-12
Applicant: 東レ株式会社
IPC: C09J7/00 , H01L21/60 , C09J109/00 , C09J113/00 , C09J161/06 , C09J163/00 , C09J201/00 , C09J201/08 , H01L23/12 , H05K3/38
CPC classification number: H01L24/50 , H01L2924/07802 , H01L2924/14 , H01L2924/351 , H05K3/386 , H01L2924/00
Abstract: PROBLEM TO BE SOLVED: To improve machining property, adhesion force, insulation reliability, and durability by using a thermoplastic resin, a thermosetting resin, and a crosslinking polymer particle as the essential constituents of an adhesive composition for forming an adhesive layer. SOLUTION: A substrate for connecting semiconductor integrated circuit has at least one layer of each of a wiring substrate layer 4 that consists of an insulator layer 3 and a conductor pattern, a layer 7 where no conductor patterns are formed, and an adhesive layer 6. The adhesive layer 6 contains, as essential constituents, at least one type of each of a thermoplastic resin, a thermosetting resin, and a crosslinking polymer particle. A copolymer with butadiene as an essential copolymerization constituent is preferable as the thermoplastic resin. An epoxy resin and a phenol resin are suitable as the thermosetting resin due to the improved insulation property. An example of the crosslinking polymer is the crosslinking polymer particle in core shell structure where polymethacrylate is at an outer layer with crosslinking polybutylacrylate as a center.
-
公开(公告)号:JP2006124640A
公开(公告)日:2006-05-18
申请号:JP2005104675
申请日:2005-03-31
Applicant: Nippon Shokubai Co Ltd , 株式会社日本触媒
Inventor: ISHII TAKAKO , TAZAKI SATOSHI
IPC: C09J133/00 , C09J7/02 , C09J139/04 , C09J201/08
Abstract: PROBLEM TO BE SOLVED: To find a pressure-sensitive adhesive composition without requiring high temperature heating and without causing troubles (acceleration of adhesion, staining of an adherend, interfacial peeling from a substrate and the like) which have to be prevented in removable pressure-sensitive adhesive products.
SOLUTION: The pressure-sensitive adhesive composition comprises 100 pts.mass acrylic tacky polymer (A) containing an oxazoline group and 0.01-10 pts.mass crosslinking polymer (B) containing a carboxy group, and this crosslinking polymer (B) is obtained from a raw material monomer mixture having ≥30 mass% carboxy group-containing monomer.
COPYRIGHT: (C)2006,JPO&NCIPIAbstract translation: 要解决的问题:为了找到压敏粘合剂组合物,不需要高温加热并且不会引起麻烦(加速粘合,被粘物的染色,从基板的界面剥离等),这些必须被防止 可拆卸的压敏胶产品。 解决方案:压敏粘合剂组合物包含含有恶唑啉基的100质量份丙烯酸类粘性聚合物(A)和含有羧基的0.01〜10质量份交联聚合物(B),该交联性聚合物(B) 由具有≥30质量%含羧基单体的原料单体混合物获得。 版权所有(C)2006,JPO&NCIPI
-
公开(公告)号:JP2006028338A
公开(公告)日:2006-02-02
申请号:JP2004209322
申请日:2004-07-16
Applicant: Panac Co Ltd , パナック株式会社
Inventor: KATO JUNICHI , KUSANO KOICHI , KAWAKAMI TAKAHISA , MINAGAWA YOSHITAKA , KANAI MAOMI , MIYAMOTO YUMI , ENAMI HIROSHI , MIZUMURA JUNJI , ANDO MASAMI , SUGIMOTO KIYOSHI , OBARA MASANORI
IPC: C09J201/00 , C09D5/00 , C09D201/08 , C09J11/06 , C09J153/00 , C09J201/08
Abstract: PROBLEM TO BE SOLVED: To provide a fragrant adhesive produceable in simple production steps, having a reworking property, free from residue of paste to the surface to be applied, free from defect of adhesive force by addition of the fragrant agent, releasing adequate fragrance for a long period, preferably further excellent in transparency and suitable for surface protection.
SOLUTION: An adhesive component containing, as a main component, a thermoplastic elastomer and a plasticizer is formulated with a fragrant component substantially having compatibility with the adhesive component to provide the fragrant adhesive. When stronger adhesive force is required, the adhesive is formulated with a carboxylic acid-modified thermoplastic elastomer and a crosslinking agent and/or the adhesive containing these components as main components is primed as an anchor layer.
COPYRIGHT: (C)2006,JPO&NCIPIAbstract translation: 要解决的问题:为了提供在简单的生产步骤中可生产的香料粘合剂,具有返工性能,没有糊剂残留到待施用的表面,通过加入香料没有粘合力的缺陷,释放 足够的香料长时间,优选透明度更好并适合表面保护。 解决方案:以与粘合剂组分基本上相容的芳香组分配制含有作为主要组分的热塑性弹性体和增塑剂的粘合剂组分以提供香料粘合剂。 当需要更强的粘合力时,将粘合剂与羧酸改性的热塑性弹性体一起配制,并将交联剂和/或含有这些组分作为主要组分的粘合剂作为锚定层。 版权所有(C)2006,JPO&NCIPI
-
公开(公告)号:JP3601824B2
公开(公告)日:2004-12-15
申请号:JP51705593
申请日:1993-03-25
Applicant: ヘンケル・コマンディットゲゼルシャフト・アウフ・アクチェン
Inventor: ヴィレケ、ルトガー , クライン、ヨハン , クラウク、ヴォルフガング , ダウテ、ペーター , ルスト、エルンスト−ウルリッヒ
IPC: C04B24/08 , C04B24/28 , C04B26/04 , C08F8/44 , C08G83/00 , C08K3/22 , C08L101/00 , C08L101/08 , C09D5/34 , C09D201/08 , C09J201/00 , C09J201/08
-
公开(公告)号:JP3519298B2
公开(公告)日:2004-04-12
申请号:JP95099
申请日:1999-01-06
Applicant: サンスター技研株式会社
IPC: C08J5/18 , B32B27/00 , B32B27/32 , C08F8/32 , C08K5/17 , C08K5/25 , C08K5/29 , C08K5/3445 , C08L23/26 , C08L53/00 , C08L79/02 , C08L101/08 , C09J7/00 , C09J7/02 , C09J11/06 , C09J123/12 , C09J123/26 , C09J153/02 , C09J201/08
CPC classification number: C08L101/08 , C08F8/32 , C08K5/17 , C08K5/3445 , C08L79/02 , C08L2666/04 , C09J201/08 , Y10T428/249982 , Y10T428/249983 , Y10T428/249985
Abstract: A one-pack type thermally crosslinkable polymer composition comprising a thermoplastic polymer having a carboxylic acid group or an acid anhydride group, and a polyamine compound as a latent curing agent, which is suitably used as an adhesive to adhere a skin material to a substrate of an automobile interior parts.
-
公开(公告)号:JP2004002525A
公开(公告)日:2004-01-08
申请号:JP2002159361
申请日:2002-05-31
Applicant: Dainippon Ink & Chem Inc , 大日本インキ化学工業株式会社
Inventor: TANAKA YOSHIMASA , SHIRAGA JUN , OCHI YASUO , TSUNASHIMA KEIJI
IPC: C08F2/16 , C08F291/00 , C09J109/00 , C09J133/06 , C09J201/08
Abstract: PROBLEM TO BE SOLVED: To provide a high-solids aqueous adhesive composition having excellent water whitening properties and holding power even when used in fields requiring the water whitening resistance and to provide a method for producing the composition and a adhesive product obtained therefrom.
SOLUTION: The aqueous adhesive composition comprises a polymer [A] containing carboxy groups and a polymer [B] derived from monomers consisting essentially of a diene monomer and an acrylate or a methacrylate monomer containing a 4-12C alkyl group and polymer particles [X] having 5-50 mg KOH acid value and dispersed in an aqueous medium. An adhesive film obtained from the aqueous adhesive composition satisfies (1) ≤-25°C actually measured glass transition temperature and (2) 25-80 wt.% of gel fraction (a fraction insoluble in toluene).
COPYRIGHT: (C)2004,JPO-
公开(公告)号:JP2003213244A
公开(公告)日:2003-07-30
申请号:JP2002019993
申请日:2002-01-29
Applicant: DAINIPPON INK & CHEMICALS
Inventor: SHIRAGA JUN , OCHI YASUO , TANAKA YOSHIMASA , TAMAKI YOSHIFUMI
IPC: C09J201/02 , C09J201/08
Abstract: PROBLEM TO BE SOLVED: To obtain an aqueous adhesive composition, excellent in water resistance and whitening resistance and adhesion, and having high solid content. SOLUTION: The aqueous adhesive composition comprises a polymer [A] having carboxy group and a polymer [B] having a crosslinking reactive group, has an acid value of 5-50 and is obtained by dispersing a polymer particle [X] having 300-2,000 nm average particle diameter into an aqueous medium, wherein the composition is characterized in that a film formed from the composition has ≤-25°C glass transition temperature and 25-80 wt.% gel fraction. COPYRIGHT: (C)2003,JPO
-
-
-
-
-
-
-
-
-