公开(公告)号:JP2009521622A
公开(公告)日:2009-06-04
申请号:JP2008547716
申请日:2006-12-19
发明人: アマ,アヒム , メリマン,エドマンド・エイ
CPC分类号: D21H13/20 , F16D69/026 , F16D2200/0095
摘要: The invention concerns a paper comprising (a) 40 to 70 parts by weight of polypyridobisimidazole fiber, polypyridobisimidazole pulp, or mixtures thereof and (b) 30 to 60 parts by weight of friction modifiers, structural resins, wet-strength resins, processing aids, fillers, and mixtures thereof; the parts by weight being based on the total amount of a) and b) in the paper.
-
公开(公告)号:JP3524015B2
公开(公告)日:2004-04-26
申请号:JP13505999
申请日:1999-05-14
申请人: Nskワーナー株式会社
CPC分类号: F16D69/026 , C08L83/08 , D21H13/26 , D21H17/59 , F16D2200/0095 , Y10T428/2962 , Y10T428/31663
-
公开(公告)号:JP2009500511A
公开(公告)日:2009-01-08
申请号:JP2008521430
申请日:2006-07-03
发明人: エリック・アーサー・シューラー , ジェームズ・マーティン・リー , マシュー・ジョセフ・トリッペル
CPC分类号: D21H13/50 , D21H13/18 , D21H17/48 , D21H17/67 , F16D69/026 , F16D2200/0095 , Y10T428/249964 , Y10T442/2115 , Y10T442/2344 , Y10T442/699
摘要: 本発明は摩擦材料に関わり、さらにとりわけ、従来の製紙プロセスを使って製造できる湿式摩擦材料に関する。 湿り気を付与した一様な骨組マトリクスを形成するために長いファイバーが使われ、そのファイバーは、摩擦マトリクス全体およびマトリクスバインダー全体に、特に隣接したファイバーの隙間において粒子状材料を分散させることによって補強され、それにより材料の剪断強度を著しく増やす一方で、材料を通る流量に対するほとんど無視できる影響を持つ。
-
公开(公告)号:JP3535579B2
公开(公告)日:2004-06-07
申请号:JP22993294
申请日:1994-09-26
申请人: ボーグワーナー・インコーポレーテッド
发明人: マーク・エイ・イエスニク
CPC分类号: F16D69/026 , C08L61/06 , C08L83/04 , F16D2200/0095 , C08L83/00 , C08L2666/14
-
5.
公开(公告)号:JP2003292943A
公开(公告)日:2003-10-15
申请号:JP2002096054
申请日:2002-03-29
发明人: AIBA HIROSHI , MORI MASAHIRO
IPC分类号: C08G8/10 , C08K3/14 , C08K3/22 , C08K3/28 , C08K5/00 , C08L61/06 , C09K3/14 , D21H17/48 , D21H17/68 , D21H21/52 , F16D69/02
CPC分类号: F16D69/026 , C08G8/10 , C08K3/14 , C08K3/22 , C08K3/28 , D21H17/48 , D21H17/68 , D21H17/74 , D21H21/52 , F16D2200/0095 , C08L61/06
摘要: PROBLEM TO BE SOLVED: To provide a resin composition for a wet friction material, having a small initial variation of the friction coefficient when used as a wet friction material, improved positive gradient of Δμ-V property and excellent durability and provide a wet friction material having a small initial variation of the friction coefficient, improved positive gradient of Δμ-V property and excellent durability. SOLUTION: The resin composition for the wet friction material is composed mainly of a phenolic resin obtained by reacting a phenol with an aldehyde in the presence of a basic catalyst and contains a granular filler having a specific surface area of 35-410 m 2 /g as an additive. The wet friction material is produced by using the resin composition as a binder. COPYRIGHT: (C)2004,JPO
摘要翻译: 要解决的问题:为了提供一种用作湿摩擦材料的树脂组合物,当用作湿摩擦材料时具有小的摩擦系数的初始变化,提高Δμ-V性能的正梯度和优异的耐久性,并提供一种 湿摩擦材料具有较小的摩擦系数的初始变化,提高Δμ-V性能的正梯度和优异的耐久性。 解决方案:用于湿摩擦材料的树脂组合物主要由在碱性催化剂存在下使酚与醛反应获得的酚醛树脂组成,并含有比表面积为35-410μm的颗粒填料
2 SP> / g作为添加剂。 通过使用树脂组合物作为粘合剂来制造湿摩擦材料。 版权所有(C)2004,JPO -
公开(公告)号:JPS59206436A
公开(公告)日:1984-11-22
申请号:JP8362684
申请日:1984-04-25
申请人: Borg Warner
CPC分类号: F16D69/026 , D21H13/26 , D21H13/40 , F16D2200/0095
-
7.
公开(公告)号:JP5633821B2
公开(公告)日:2014-12-03
申请号:JP2011545923
申请日:2009-12-18
申请人: 国立大学法人北海道大学
IPC分类号: C01B31/02 , C08J5/10 , C08K3/04 , C08L101/00 , C09K3/14 , D01F1/09 , D01F9/22 , H01B1/18 , H01B1/24
CPC分类号: C01B31/0476 , B82Y30/00 , B82Y40/00 , C01B31/043 , C01B32/192 , C01B32/23 , F16D69/026 , F16D2200/006 , F16D2200/0095
-
公开(公告)号:JP2013032794A
公开(公告)日:2013-02-14
申请号:JP2011168059
申请日:2011-08-01
发明人: SUZUKI ATSUSHI , KAWABATA MASATAKA , HATA MAMI , TOIDA SHOJI
CPC分类号: D21H17/67 , D21H21/18 , F16D69/026 , F16D2200/0095 , Y10T428/25 , Y10T428/2982 , Y10T428/31971 , Y10T428/31986 , Y10T428/31989 , Y10T428/31993
摘要: PROBLEM TO BE SOLVED: To provide a wet friction material with an increased coefficient of friction, and a method of manufacturing the material.SOLUTION: The wet friction material includes a pulverized cork heated to 150-200°C, if necessary. The pulverized cork is mixed with paper-making materials of other wet friction material and formed into a paper-made substrate. The paper-made substrate is impregnated with a synthetic resin to be a binder and heated and cured. The cork itself has a high friction coefficient μ. Moreover, powder thereof increases the surface area and an area in contact with a separator plate of a counter member, thereby improving a friction coefficient of a friction surface of the wet friction material. The friction coefficient μ of the cork itself and capacities for absorbing and discharging oil are improved by heating the cork. Thus, there is provided the wet friction material that has a higher friction coefficient μ. An increase in the friction coefficient μ, weight reduction by reducing the number of friction materials, and high efficiency are achieved when used as a wet friction material.
摘要翻译: 要解决的问题:提供具有增加的摩擦系数的湿摩擦材料以及制造该材料的方法。
解决方案:如果需要,湿摩擦材料包括加热至150-200℃的粉碎软木塞。 将粉碎的软木与其它湿摩擦材料的造纸材料混合并形成纸制基材。 用合成树脂浸渍造纸基材作为粘合剂并加热固化。 软木本身具有高摩擦系数μ。 此外,其粉末增加表面积和与对置构件的隔板接触的面积,从而提高湿摩擦材料的摩擦面的摩擦系数。 软木本身的摩擦系数μ以及通过加热软木来提高油的吸收和排出能力。 因此,提供了具有较高摩擦系数μ的湿摩擦材料。 当用作湿摩擦材料时,可以实现摩擦系数μ的增加,减少摩擦材料的重量减少和高效率。 版权所有(C)2013,JPO&INPIT
-
-
公开(公告)号:JP2004346988A
公开(公告)日:2004-12-09
申请号:JP2003142883
申请日:2003-05-21
申请人: Dainatsukusu:Kk , Honda Motor Co Ltd , 本田技研工業株式会社 , 株式会社ダイナックス
发明人: KIMURA MUTSUKO , YAMANE TOMONORI , YOSHIDA JUNPEI
CPC分类号: D21H13/26 , D21H17/33 , D21H17/68 , D21H21/52 , F16D69/026 , F16D2200/0095
摘要: PROBLEM TO BE SOLVED: To provide a wet paper friction material which has both of excellent frictional characteristics and high friction coefficient.
SOLUTION: The wet paper friction material is manufactured by impregnating a paper material with thermosetting resin, and then by hardening the impregnated paper material by heating it, and further by forming it by press working. The paper material contains aramid pulp adjusted so as to have freeness of 200 to 400 ml and aramid pulp adjusted so as to have freeness of 450 to 700 ml respectively by 10 to 50 wt.% of total paper material in addition to cellulose pulp and filler. Further, the surface roughness before and after press-forming by a surface finishing method is adjusted so as to be Rmr(30%)≥55%, where Rmr(C) (C:cutting level %) is a load length factor. As a result, a high friction coefficient, high heat resistance, and high mechanical strength are simultaneously satisfied.
COPYRIGHT: (C)2005,JPO&NCIPI
-
-
-
-
-
-
-
-
-