Method for joining parts of ceramic high-temperature superconductor
material
    2.
    发明授权
    Method for joining parts of ceramic high-temperature superconductor material 失效
    陶瓷高温超导体材料接合方法

    公开(公告)号:US5244876A

    公开(公告)日:1993-09-14

    申请号:US966589

    申请日:1992-10-26

    IPC分类号: C04B35/45 C04B37/00 H01L39/02

    摘要: Method for joining parts of ceramic high-temperature superconductor material of the composition Bi.sub.(2+a-b) (Sr.sub.1-c) Ca.sub.c) .sub.(3-a) Pb.sub.b Cu.sub.(2+d) O.sub.x, where a is 0 to 0.3, b is 0 to 0.5, c is 0.1 to 0.9 and d is 0 to 2 and x has a value depending on the state of oxidation of the metals present, the end faces of the parts located at a gap spacing apart from one another are heated by means of a fuel gas/oxygen flame to temperatures from 750.degree. to 875.degree. C. Simultaneously, a rod of the same material above the spacing gap is heated until the melt thereof drips off into the gap between the end faces of the two parts, completely filling the gap. At least the joint region between the two parts is then heat-treated for 7 to 100 hours at temperatures between 780.degree. and 850.degree. C.

    摘要翻译: 组合物Bi(2 + ab)(Sr1-c)Cac)(3-a)PbbCu(2 + d)Ox的陶瓷高温超导体材料部分的方法,其中a为0至0.3,b为0 至0.5,c为0.1至0.9,d为0至2,x具有取决于存在的金属的氧化状态的值,位于间隔间隔的部分的端面通过 燃料气体/氧气火焰至750℃至875℃的温度。同时,将间隔间隔上方的相同材料的棒加热直到其熔体滴落到两部分的端面之间的间隙中,完全填充 差距。 至少两部分之间的接合区域在780〜850℃的温度下进行7〜100小时的热处理。