公开(公告)号:US06869916B2
公开(公告)日:2005-03-22
申请号:US10327905
申请日:2002-12-26
申请人: Stephan Gauss , Joachim Bock , Johannes Holzem , Guenter Brommer , Markus Grom , Werner Horst
发明人: Stephan Gauss , Joachim Bock , Johannes Holzem , Guenter Brommer , Markus Grom , Werner Horst
IPC分类号: H01F6/00 , H01B12/04 , H01B13/00 , H01L39/14 , H01L39/16 , H01L39/24 , B29C53/00 , C04B35/653
CPC分类号: H01L39/143 , H01L39/16 , Y10S505/703 , Y10S505/739 , Y10S505/741
摘要: The invention relates to a high-temperature superconductor component with a particular cross-sectional area, which has a current-carrying section, the current-carrying section being in contact with a safety conductor in such a way that the critical current flowing on transition of the superconductor to normal conduction can be taken up without damage by the safety conductor in at least 1 second and rerouted, as well as a process for its production.
摘要翻译: 本发明涉及具有特定横截面积的高温超导体部件,其具有通电部分,载流部分与安全导体接触,使得临时电流流过 超导体至正常导通可以在至少1秒钟内被安全导体承受,而不会损坏,并重新布线,以及其生产工艺。
-
2.
公开(公告)号:US5244876A
公开(公告)日:1993-09-14
申请号:US966589
申请日:1992-10-26
申请人: Eberhard Preisler , Joachim Bock , Johannes Holzem , Werner Horst
发明人: Eberhard Preisler , Joachim Bock , Johannes Holzem , Werner Horst
CPC分类号: C04B35/4525 , C04B37/005 , H01L39/02 , C04B2237/06 , C04B2237/34 , C04B2237/78 , C04B2237/80 , Y10S505/739 , Y10S505/782
摘要: Method for joining parts of ceramic high-temperature superconductor material of the composition Bi.sub.(2+a-b) (Sr.sub.1-c) Ca.sub.c) .sub.(3-a) Pb.sub.b Cu.sub.(2+d) O.sub.x, where a is 0 to 0.3, b is 0 to 0.5, c is 0.1 to 0.9 and d is 0 to 2 and x has a value depending on the state of oxidation of the metals present, the end faces of the parts located at a gap spacing apart from one another are heated by means of a fuel gas/oxygen flame to temperatures from 750.degree. to 875.degree. C. Simultaneously, a rod of the same material above the spacing gap is heated until the melt thereof drips off into the gap between the end faces of the two parts, completely filling the gap. At least the joint region between the two parts is then heat-treated for 7 to 100 hours at temperatures between 780.degree. and 850.degree. C.
摘要翻译: 组合物Bi(2 + ab)(Sr1-c)Cac)(3-a)PbbCu(2 + d)Ox的陶瓷高温超导体材料部分的方法,其中a为0至0.3,b为0 至0.5,c为0.1至0.9,d为0至2,x具有取决于存在的金属的氧化状态的值,位于间隔间隔的部分的端面通过 燃料气体/氧气火焰至750℃至875℃的温度。同时,将间隔间隔上方的相同材料的棒加热直到其熔体滴落到两部分的端面之间的间隙中,完全填充 差距。 至少两部分之间的接合区域在780〜850℃的温度下进行7〜100小时的热处理。
-
公开(公告)号:US12112729B2
公开(公告)日:2024-10-08
申请号:US17782879
申请日:2019-12-07
申请人: Nicole Liesel Mumberg , Arnd Mumberg , Alina Ilona Mumberg , Regina Engelhardt , Arne Werner Horst Siebling
发明人: Nicole Liesel Mumberg , Arnd Mumberg , Alina Ilona Mumberg , Regina Engelhardt , Arne Werner Horst Siebling
摘要: A headpiece is provided for a transverse flute having a first leg and a second leg, which is connectable to a tube of the transverse flute. The two legs are arranged at an acute angle to one another.
-
公开(公告)号:US20230008370A1
公开(公告)日:2023-01-12
申请号:US17782879
申请日:2019-12-07
申请人: Arnd MUMBERG , Nicole Liesel MUMBERG , Alina Ilona MUMBERG , Regina ENGELHARDT , Arne Werner Horst SIEBLING
发明人: Nicole Liesel Mumberg , Arnd Mumberg , Alina Ilona Mumberg , Regina Engelhardt , Arne Werner Horst Siebling
摘要: A headpiece is provided for a transverse flute having a first leg and a second leg, which is connectable to a tube of the transverse flute. The two legs are arranged at an acute angle to one another.
-
公开(公告)号:US06584333B1
公开(公告)日:2003-06-24
申请号:US09762240
申请日:2001-05-09
申请人: Stephan Gauss , Joachim Bock , Johannes Holzem , Guenter Brommer , Markus Grom , Werner Horst
发明人: Stephan Gauss , Joachim Bock , Johannes Holzem , Guenter Brommer , Markus Grom , Werner Horst
IPC分类号: H01B1200
CPC分类号: H01L39/143 , H01L39/16 , Y10S505/703 , Y10S505/739 , Y10S505/741
摘要: The invention relates to a high-temperature superconductor component with a particular cross-sectional area, which has a current-carrying section, the current-carrying section being in contact with a safety conductor in such a way that the critical current flowing on transition of the superconductor to normal conduction can be taken up without damage by the safety conductor in at least 1 second and rerouted, as well as a process for its production.
摘要翻译: 本发明涉及具有特定横截面积的高温超导体部件,其具有通电部分,载流部分与安全导体接触,使得临时电流流过 超导体至正常导通可以在至少1秒钟内被安全导体承受,而不会损坏,并重新布线,以及其生产工艺。
-
-
-
-