Abstract:
An ethylene polymer having a density greater than about 0.930 g/ml and a level of long chain branching ranging from about 0.001 LCB/103 carbons to about 1.5 LCB/103 carbons as determined by SEC-MALS. An ethylene polymer having a level of short chain branching ranging from about 0 to about 10 mol. % and a level of long chain branching ranging from about 0.001 LCB/103 carbons to about 1.5 LCB/103 carbons as determined by SEC-MALS. An ethylene polymer having a polydispersity index ranging from about 8 to about 25 and a level of long chain branching ranging from about 0.001 LCB/103 carbons to about 1.5 LCB/103 carbons as determined by SEC-MALS.
Abstract:
Ethylene-based polymers having a density from 0.94 to 0.96 g/cm3, a Mn from 5,000 to 14,000 g/mol, a ratio of Mw/Mn from 18 to 40, and at least one of a PENT value at 2.4 MPa of at least 11,500 hr and/or a W90 from 7.5 to 15 wt. % are disclosed. Additional ethylene polymers can have the same density, Mn, and Mw/Mn values, as well as a relaxation time from 0.5 to 3.5 sec, a CY-a parameter from 0.48 to 0.68, a HLMI from 5 to 11 g/10 min, a viscosity at HLMI from 3,000 to 7,500 Pa-sec, and a higher molecular weight component (HMW) and a lower molecular weight (LMW) component, in which a ratio of the number of SCBs at Mp of the HMW component to the number of SCBs at Mp of the LMW component is from 3.5 to 8.
Abstract:
A bimodal polymer composition comprising a lower molecular weight homopolymer and a higher molecular weight copolymer wherein the bimodal polymer composition has a density of from about 0.930 gram per cubic centimeter (g/cc) to about 0.970 g/cc, a ratio of high load melt index:melt index of from about 10 to about 150 and an Environmental Stress Crack Resistance (ESCR) of from about 25 hours to about 300 hours when measured in accordance with ASTM D1693 or ASTM D2561. A chromium-catalyzed polymer composition comprising (i) a lower molecular weight homopolymer and (ii) a higher molecular weight copolymer, wherein the bimodal polymer composition has an Environmental Stress Crack Resistance (ESCR) of from about 25 hours to about 300 hours when measured in accordance with ASTM D1693 or ASTM D2561.
Abstract:
A polyolefin having a density of greater than about 0.930 g/ml which when extruded at a temperature in the range of from about 590° F. to about 645° F. and then coated onto a substrate at a rate of from about 300 ft/min to about 1000 ft/min has an edge weave of from about 0 in/side to about 2.5 in/side and a neck-in of less than about 3.0 in/side.
Abstract:
A method of preparing a polymer article comprising determining a zero-shear viscosity for a polymer sample; sieving the polymer sample to produce a plurality of sieved polymer samples; determining a molecular weight distribution for each of the plurality of sieved polymer samples; determining a zero-shear viscosity for each of the plurality of sieved polymer samples; determining a compositional diversity of each of the plurality of sieved polymer samples based on a ratio of the zero shear viscosity for each of the plurality of sieved polymer samples to the zero shear viscosity for the polymer sample; identifying a polymer sample having a ratio of the zero shear viscosity to zero shear viscosity for the polymer sample of from about 0.5 to equal to or greater than about 3; and preparing a polymer article from the identified polymer sample.
Abstract:
A catalyst system comprising a half-sandwich chromium complex, an activator support and an optional cocatalyst. A compound of formula Cp′Cr(Cl)2(Ln), where Cp′ is η5-C5H4CH2CH2CH═CH2 and Ln is pyridine, THF or diethylether. A compound of formula Cp″Cr(Cl)2(Ln), where Cp″ is η5-C5H4C(Me)2CH2CH2CH═CH2 and Ln is pyridine, THF or diethylether.
Abstract:
A bimodal polymer composition comprising a lower molecular weight homopolymer and a higher molecular weight copolymer wherein the bimodal polymer composition has a density of from about 0.930 gram per cubic centimeter (g/cc) to about 0.970 g/cc, a ratio of high load melt index:melt index of from about 10 to about 150 and an Environmental Stress Crack Resistance (ESCR) of from about 25 hours to about 300 hours when measured in accordance with ASTM D1693 or ASTM D2561. A chromium-catalyzed polymer composition comprising (i) a lower molecular weight homopolymer and (ii) a higher molecular weight copolymer, wherein the bimodal polymer composition has an Environmental Stress Crack Resistance (ESCR) of from about 25 hours to about 300 hours when measured in accordance with ASTM D1693 or ASTM D2561.
Abstract:
A polymer having a long chain branching content peaking at greater than about 20 long chain branches per million carbon atoms, and a polydispersity index of greater than about 10 wherein the long chain branching decreases to approximately zero at the higher molecular weight portion of the molecular weight distribution. A polymer having a long chain branching content peaking at greater than about 8 long chain branches per million carbon atoms, a polydispersity index of greater than about 20 wherein the long chain branching decreases to approximately zero at the higher molecular weight portion of the molecular weight distribution. A polymer having a long chain branching content peaking at greater than about 1 long chain branches per chain, and a polydispersity index of greater than about 10 wherein the long chain branching decreases to approximately zero at the higher molecular weight portion of the molecular weight distribution.
Abstract:
A radically coupled polymer having a density of from about 0.915 g/ml to about 0.975 g/ml characterized by a crossover modulus that is equal to or less than ymn where ymn=18000e−0.15x and x is the number average molecular weight of the radically coupled polymer. An ethylene polymer having a level of short chain branching ranging from about 0 to about 10 mol. %; a level of long chain branching ranging from about 0.001 LCB/103 carbons to about 1.5 LCB/103 carbons as determined by SEC-MALS; and characterized by a crossover modulus that is equal to or less than ymn where ymn=18000e−0.15x and x is the number average molecular weight of the radically coupled polymer.